Synthesis of proton‐conducting membranes by the utilization of preirradiation grafting and atom transfer radical polymerization techniques
- 4 January 2002
- journal article
- research article
- Published by Wiley in Journal of Polymer Science Part A: Polymer Chemistry
- Vol. 40 (4) , 591-600
Abstract
The atom transfer radical polymerization (ATRP) of styrene onto poly(vinylidene fluoride)‐graft‐poly(vinylbenzyl chloride) (PVDF‐g‐PVBC) membranes was investigated. Novel membranes were designed for fuel‐cell applications. The benzyl chloride groups in the PVDF‐g‐PVBC membranes functioned as initiators, and a Cu‐based catalytic system with the general formula Cu(n)Xn/ligand [where X is Cl or Br and the ligand is 2,2′‐bipyridyl (bpy)] was employed for the ATRP. In addition, 10 vol % dimethylformamide was added for increased solubility of the catalyst complex in styrene. The system was homogeneous, except for the membrane, when the initiator/copper halide/ligand/monomer molar ratio was 1/1/3/500. As anticipated, the fastest polymerization rate of styrene was observed with the copper bromide/bpy‐based catalyst system. The reaction rate was strongly temperature‐dependent within the studied temperature interval of 100–130 °C. The degree of grafting increased linearly with time, thereby indicating first‐order kinetics, regardless of the polymerization temperature. Furthermore, 120 °C was the maximum polymerization temperature that could be used in practice because the membrane structure was destroyed at higher temperatures. The degree of styrene grafting reached 400% after 3 h at 120 °C. Such a high degree of grafting could not be reached with conventional uncontrolled radiation‐induced grafting methods because of termination reactions. On the basis of an Arrhenius plot, the activation energy for the homogeneous ATRP of styrene was 217 kJ/mol. The prepared membranes became proton‐conducting after sulfonation of the polystyrene grafts. The highest conductivity measured for the prepared membranes was 70 mS/cm, which is comparable to the values normally measured for commercial Nafion membranes. The scanning electron microscopy/energy‐dispersive X‐ray results showed that the membranes had to be grafted through the matrix with both PVBC and polystyrene to become proton‐conducting after sulfonation. In addition, PVDF‐g‐[PVBC‐g‐(styrene‐block‐tert‐butyl acrylate)] membranes were also synthesized by ATRP. © 2002 John Wiley & Sons, Inc. J Polym Sci Part A: Polym Chem 40: 591–600, 2002; DOI 10.1002/pola.10146Keywords
Funding Information
- Academy of Finland (through the EMMA program)
This publication has 41 references indexed in Scilit:
- Versatile Initiators for Macromonomer Syntheses of Acrylates, Methacrylates, and Styrene by Atom Transfer Radical PolymerizationMacromolecules, 2000
- Effect of Solvent on the Activation Rate Parameters for Polystyrene and Poly(butyl acrylate) Macroinitiators in Atom Transfer Radical PolymerizationMacromolecules, 2000
- Homogeneous Reverse Atom Transfer Radical Polymerization of Styrene Initiated by PeroxidesMacromolecules, 1999
- Synthesis of fluorine-containing block copolymers via ATRP 1. Synthesis and characterization of PSt-PVDF-PSt triblock copolymersPolymer, 1999
- Copper Triflate as a Catalyst in Atom Transfer Radical Polymerization of Styrene and Methyl AcrylateMacromolecules, 1998
- Nafion®-based composite polymer electrolyte membranesElectrochimica Acta, 1998
- Synthesis and properties of sulfonated and crosslinked poly[(vinylidene fluoride)-graft-styrene] membranesPolymers for Advanced Technologies, 1998
- Investigation of radiation-grafted PVDF-g-polystyrene-sulfonic-acid ion exchange membranes for use in hydrogen oxygen fuel cellsSolid State Ionics, 1997
- Proton Transport Through Polyethylene‐Tetrafluoroethylene‐Copolymer‐Based Membrane Containing Sulfonic Acid Group Prepared by RIGPJournal of the Electrochemical Society, 1996
- Effect of oxygen on the polymerization of vinyl chloride. I. Kinetic featuresJournal of Polymer Science: Polymer Chemistry Edition, 1973