Abstract
The SCC characteristics of a transformable type 301 stainless steel have been examined under a series of different deformation conditions. The open circuit potential in every case shifted from the same initial potential to the same rest potential ( −380 mV), regardless of the nature of the deformation and the absence or presence of martensite. Deformations that produced martensite accelerated the time to attain the rest potential, but had no influence on failure time at the rest potential. The general profile of behavior was independent of the yield strength, the amount of deformation, the temperature of deformation, and the presence and amount of alpha or alpha plus epsilon martensite. The critical cracking potential (−380 mV) was the same for all conditions with or without deformation and with or without martensite. For all conditions, the potential after film formation was closely related if not identical to the critical cracking potential. The SCC characteristics and related electrochemical parameters were independent of a broad range of varying bulk properties and completely under the control of the surface.Keywords
This publication has 9 references indexed in Scilit:
- Stress Corrosion Cracking of Austenitic Stainless Steel in an Acidified Chloride SolutionCorrosion, 1980
- Influence of Chloride Concentration on Stress Corrosion Cracking of Austenitic Stainless Steel in LiCl SolutionsCorrosion, 1980
- Role of Hydrogen in Stress Corrosion Cracking of Austenitic Stainless SteelsCorrosion, 1975
- Effects of Surface Preparation on Stress Corrosion Cracking of Type 310 Stainless Steel in Boiling 42% Magnesium ChlorideCorrosion, 1968
- Effect of Potential and Stress on Time to Failure of Austenitic Stainless Steels in Magnesium Chloride SolutionsCorrosion, 1967
- Effect of Cold Work on Stress Corrosion of Type 309 Austenitic Stainless SteelCorrosion, 1966
- Threshold Stress and Incubation Period in Stress Corrosion of Types 302 and 316 Wire in Boiling Magnesium ChlorideCorrosion, 1965
- Hydrogen Embrittlement of Austenitic Stainless SteelCorrosion, 1965
- Film-rupture mechanism of stress corrosionJournal of Research of the National Bureau of Standards, 1952