REFRACTORIES SERVICE CONDITIONS IN THE BLAST FURNACE*
Author:
- 1 July 1942
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 25 (11) , 311-320
Abstract
A bstract: An analysis of “how a blast‐furnace lining wears out” is presented. The conclusions drawn are the result of critical studies on three furnaces as their linings were being removed for relining. Scab and scab‐refractory interface samples were taken at 3‐ft. intervals. These were analyzed and studied petrographically. Alkali attack and carbon disintegration are concluded to be the most serious causes of lining wear and deterioration in the stack, whereas insufficient refractoriness and high porosity are concluded to be the sources of trouble in the hearth.Keywords
This publication has 9 references indexed in Scilit:
- Effect upon Furnace Refractories of Protective Gases for High-Carbon SteelsIndustrial & Engineering Chemistry, 1941
- Chemical Equilibrium and the Control of Furnace AtmospheresIndustrial & Engineering Chemistry, 1941
- KINETICS OF SOME REACTIONS OF INTEREST TO CERAMISTS* The Disintegration of Blast‐Furnace Linings Due to Carbon Deposition†Journal of the American Ceramic Society, 1936
- The Rate of Reduction of Iron Ores with Carbon Monoxide Effect of Particle Size, Gas Velocity, and Gas CompositionIndustrial & Engineering Chemistry, 1934
- A PROGRESS REPORT ON THE DEVELOPMENT OF AN ABRASION TEST FOR REFRACTORIES AT HIGH TEMPERATURES 1Journal of the American Ceramic Society, 1930
- DISCUSSION 1 ON “PREVENTION OF DISINTEGRATION OF BLAST‐FURNACE LININGS” 2Journal of the American Ceramic Society, 1929
- THE PREVENTION OF DISINTEGRATION OF BLAST FURNACE LININGS 1Journal of the American Ceramic Society, 1928
- DISCUSSION ON THE DISINTEGRATION OF CLAY REFRACTORIES IN IRON BLAST FURNACESJournal of the American Ceramic Society, 1924
- THE DISINTEGRATION OF REFRACTORY BRICK BY CARBON MONOXIDE 1Journal of the American Ceramic Society, 1923