Argon and induction stirred copper melts were deoxidized at different temperatures by short‐circuiting a solid electrolyte cell. The solid electrolyte cell consisted of an yttria‐stabilized zirconia tube closed at one end. The tube interior was flushed with a reducing gas and the tube was immersed in the copper melt. A layer of porous Ni‐ZrO 2 cermet deposited on the inner wall of the tube served as the anode while the copper melt was the cathode. The deoxidation experiments were modeled as a function of mass transfer in the melt, temperature, electronic and ionic conductivity of the electrolyte, short‐circuit resistance, and flow rate of the reducing gas. The deoxidation model was used to discuss process optimization and scaleup.