Abstract
Oxide films on 316L stainless steel govern its corrosion resistance but are also prone to structural/chemical modifications under applied potential as well as upon immersion into electrolyte. Here, relationships between the pristine characteristics of oxide films and restructuring over time upon immersion in 0.5 M K 2 SO 4 solution (pH 3) are depicted in details with a combination of physical-chemical and electrochemical characterization techniques. Differences in the rate of the oxide film restructuring can be measured for samples from different suppliers and after the application of a moderate heat treatment. A thickening of the inner Cr oxide layer takes place even without the external application of potential, even faster than the partial dissolution of the outer Fe oxide layer. This dissolution of the Fe oxide layer is slower than the increase of its electronic defects. Electronic defects control the open circuit potential and its change over time of immersion in electrolyte. Such detailed picturing of the initial behavior of the pristine oxide film without preliminary polishing step highlights the influence of the history of the steel samples. Therefore, such history is of utmost relevance for applications in which a high degree of accuracy in surface properties is required.

This publication has 40 references indexed in Scilit: