Effects of Cooling Rate During Solid Solution Treatment on Precipitation Behavior and Hardness in Ni–38Cr–3.8Al Alloys
Open Access
- 25 April 2025
- journal article
- research article
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 56 (7) , 2320-2328
Abstract
The effects of the cooling rate during solid solution (SS) treatment on the hardness and microstructure of Ni–38Cr–3.8Al alloy were studied using a modified Jominy test. Hardness decreased with increasing cooling rate after SS treatment but exceeded 50 HRC after precipitation aging under all conditions. Faster cooling led to lower initial hardness but higher hardness after aging. Microscopic analysis revealed precipitation was more widespread at lower cooling rates after SS treatment but became uniform after aging. Rietveld analysis of X-ray diffraction indicated that after SS treatment, the weight fraction of Ni3Al (γ′) increased as the cooling rate decreased, and its final fraction remained nearly constant regardless of cooling rate, although γ′ increased further during aging. Despite this, hardness did not exhibit a direct correlation with the γ′ weight fraction after aging, suggesting that lamellar spacing and other microstructural factors also influence hardness. A simple hardness model incorporating phase volume fractions and lamellar spacing was developed to predict hardness trends. The model exhibits good agreement with experimental data, confirming that lamellar spacing and microstructural factors significantly affect hardness. These findings provide insights into optimizing heat treatment to achieve desired mechanical properties—particularly for applications requiring high hardness and low magnetic permeability.Keywords
Funding Information
- Tokyo City University
This publication has 13 references indexed in Scilit:
- Structure restoration and coarsening of nanocrystalline cementite in cold drawn pearlitic wire induced by low temperature annealingScripta Materialia, 2022
- A modified pearlite microstructure to overcome the strength-plasticity trade-off of heavily drawn pearlitic wireScripta Materialia, 2022
- Creep behavior of Ni–38Cr-3.8Al alloy with lamellar structure formed by discontinuous precipitationMaterials Science and Engineering: A, 2019
- Primary α phase and its effect on the impact ductility of a high Cr content cast Ni-base superalloyJournal of Alloys and Compounds, 2012
- Seal for rolling bearingsSealing Technology, 2009
- Thermodynamic properties of the Ni–Al–Cr systemIntermetallics, 1999
- Effect of interlamellar spacing on the delamination of pearlitic steel wiresScripta Materialia, 1996
- Effect of refractory elements on the evolution of the NiAl intermetallic phase in NiCrAl alloysMaterials Science and Engineering: A, 1990
- The application of nonmagnetic alloys in high pressure cell designHigh Pressure Research, 1990
- Effects of Al and Ti on Age-Hardenability of 40Cr-Ni AlloyJournal of the Japan Institute of Metals and Materials, 1972