Abstract
In this work, carbon-added tungsten ( W1−xCxW1−xCx , x⩽0.19x⩽0.19 ) and thin carbon layer-inserted tungsten ( Wtop∕C∕WbottomWtop∕C∕Wbottom , the thickness of WbottomWbottom is set to be 2nm2nm and 10nm10nm ) gate stacks are deposited on SiO2∕SiSiO2∕Si to fabricate metal-oxide-semiconductor capacitors. Grazing incident angle X-ray diffraction reveals that the W1−xCxW1−xCx films become amorphous when the concentration of added C is lower than 16 atom %. However, when the C concentration is as high as 19 atom %, a trace of γ phase of tungsten carbide phase appears in the W0.81C0.19W0.81C0.19 film. No interdiffusion between C-added W and SiO2SiO2 is observed by Auger electron spectroscopy depth profiling. The resistivity of W, W0.88C0.12W0.88C0.12 , W0.84C0.16W0.84C0.16 , and W0.81C0.19W0.81C0.19 are 132, 151, 163, and 337μΩcm337μΩcm , respectively. The work function of W0.81C0.19W0.81C0.19 , W0.84C0.16W0.84C0.16 , W0.88C0.12W0.88C0.12 , W, W∕C∕WW∕C∕W (10nm)(10nm) , and W∕C∕WW∕C∕W (2nm)(2nm) on SiO2SiO2 are 4.82, 4.75, 4.73, 4.66, 4.52, and 4.32eV4.32eV , respectively. The C-related dipole shows apparent influence on the work function. The leakage current densities of C-added W films are smaller than 2×10−5A∕cm22×10−5A∕cm2 in the range from 0to5×107V∕cm0to5×107V∕cm . No significant influence of these gate electrodes on the fixed oxide charge and the leakage behavior of SiO2SiO2 are observed.

This publication has 23 references indexed in Scilit: