Mn-Bi Magnetic Powders With High Coercivity and Magnetization at Room Temperature
Authors:
- 18 October 2012
- journal article
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 48 (11) , 3641-3643
Abstract
Mn55Bi45+x at.% Mn ( x=0, 7 and 11) magnetic powders were prepared by low energy ball milling technique. The x-ray diffraction pattern showed that the samples mainly contain over 90% of the low temperature Mn-Bi phase for x = 0 and 7 with a very small amount of Bi phase. Microstructural analysis showed that the amount of sub-micron particles increases with milling time. The milling time dependent magnetic properties were studied for all the compositions. An intrinsic coercivity (Hci) of 12.2 kOe, remanent magnetization (4 πMr) of 7.1 kG, and energy product (BH)max of 11 MGOe have been obtained for the 8 hours milled Mn55Bi45+7 at.% Mn sample. These Mn-Bi powders have potential use as precursor for rare earth free permanent magnets.Keywords
This publication has 9 references indexed in Scilit:
- Anisotropic nanocrystalline MnBi with high coercivity at high temperatureApplied Physics Letters, 2011
- Structural and magnetic properties of bulk MnBi permanent magnetsJournal of Applied Physics, 2011
- Crystal structure, magnetic properties and electronic structure of the MnBi intermetallic compoundJournal of Physics: Condensed Matter, 2002
- Magnetic properties of the MnBi intermetallic compoundApplied Physics Letters, 2001
- Temperature dependence of coercivity in MnBiJournal of Applied Physics, 1993
- Formation of MnBi ferromagnetic phases through crystallization of the amorphous phaseJournal of Applied Physics, 1991
- Effect of Grinding on the Coercivity of MnBi ParticlesJapanese Journal of Applied Physics, 1977
- Anisotropy Field and Coercivity for Aligned MnBi ParticlesJapanese Journal of Applied Physics, 1976
- A New Permanent Magnet from Powdered Manganese BismuthideReviews of Modern Physics, 1953