Low Temperature Copper-Copper Thermocompression Bonding
Authors:
- 1 December 2008
- conference paper
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- Vol. 75, 399-404
Abstract
Successful direct copper thermocompression bonding was demonstrated at room temperature under ambient environment, yielding shear strength of 21 MPa. Studies on the effect of bonding temperature on the copper joint shear strength revealed a unique phenomenon at the low temperature regime (~80degC -140degC) whereby bond integrity degrades with increasing temperature. Beyond 140degC, direct relationship between temperature and joint shear strength was observed. A hypothesis on the bonding mechanism between copper surfaces is proposed to explain the anomalous bonding behaviour with temperature.Keywords
This publication has 15 references indexed in Scilit:
- Critical temperatures in thermocompression gold stud bondingJournal of Applied Physics, 2007
- Pressure dependence in peripheral bonding in gold-gold thermocompression2006
- Temperature and pressure dependence in thermocompression gold stud bondingThin Solid Films, 2005
- The low-temperature thermal oxidation of copper, Cu3O2, and its influence on past and future studiesVacuum, 2005
- Morphology and Bond Strength of Copper Wafer BondingElectrochemical and Solid-State Letters, 2004
- Temperature and duration effects on microstructure evolution during copper wafer bondingJournal of Electronic Materials, 2003
- Optical characterization of thin thermal oxide films on copper by ellipsometryApplied Physics A, 2002
- 3-D ICs: a novel chip design for improving deep-submicrometer interconnect performance and systems-on-chip integrationProceedings of the IEEE, 2001
- Effect of working temperature on young's modulus of electrolytic copperCzechoslovak Journal of Physics, 1979
- Optical Properties of Copper Oxide FilmsJournal of Applied Physics, 1966