Properties of Gold Deposited at Liquid Air Temperature
Authors:
- 1 December 1949
- journal article
- research article
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 20 (12) , 1168-1171
Abstract
Gold deposited in vacuum at liquid air temperature contained defects and strain. The number of defects and their characteristic decay energy increased rapidly with increasing rate of deposit in the range from 1 to 5 micrograms/cm2/min. The defects decayed with rising temperature but the relief of strain did not occur until after most of the defects had disappeared. Electron micrographs showed that the gold film was made up of aggregations of discreet particles rather than a smooth continuous film.Keywords
This publication has 4 references indexed in Scilit:
- A Geiger Counter Spectrometer for X-Ray Fluorescence AnalysisReview of Scientific Instruments, 1948
- A method for determining small amounts of gold, and its use in ascertaining the thickness of electrodeposited gold coatingsJournal of Research of the National Bureau of Standards, 1946
- A theory of the irreversible electrical resistance changes of metallic films evaporated in vacuumProceedings of the Physical Society (1926-1948), 1943
- Discussion of the papers by Finch, Appleyard and Lennard-JonesProceedings of the Physical Society (1926-1948), 1937