Experimental Study of Effects of Water-Cement Ratio on the Mechanical Property of High-Performance Cement-Based Iron-Tailings Grouting Material
Authors:
- 1 November 2012
- journal article
- Published by Trans Tech Publications, Ltd. in Advanced Materials Research
- Vol. 600, 186-189
Abstract
This thesis aims to research the influence factors of the mechanical property of high performance cement-based iron-tailings grouting material (ICGM). By changing the parameter of water-cement ratio, the experiment is performed to contrast ordinary cement-based grouting material (OCGM) with ICGM. Their compression strength and anti-breaking strength are studied. Through the experimental results and the contrast of them, the influence of water-cement ratio on the mechanical property of the cement-based iron-tailings grouting material is evaluated and the reasonable water-cement ratio parameter is obtained. The experimental results show that the mechanical properties of ICGM reduce with the increase of water-cement ratio. Moreover, when the water-cement ratio reaches 0.31, there is an obvious reduction of early age strength. Thus, it is advisable to adopt 0.30 as the reasonable water-cement ratio.Keywords
This publication has 4 references indexed in Scilit:
- Investigation of Drying Shrinkage of Concrete Prepared with Iron Mine TailingsKey Engineering Materials, 2011
- Approaches to control the quality of cementitious PFA grouts for nuclear waste encapsulationPowder Technology, 2007
- Improving the properties of cement–fly ash grout using fiber and superplasticizerCement and Concrete Research, 2001
- Analytical models for estimating yield stress of high-performance pseudoplastic groutCement and Concrete Research, 2001