Coordination engineering in Nd3+-doped silica glass for improving repetition rate of 920-nm ultrashort-pulse fiber laser

Authors:

Abstract
Owing to their excellent performance in terms of short pulse duration and high peak power, ultrashort pulse lasers have gained much attention in the fields of fiber-optics communication, biophotonics, and industrial processing.1 – 8 Recently, because of the advantages of compactness, robustness, and freedom from maintenance over conventional solid-state lasers,9 – 13 fiberized ultrashort pulses operating in the wavelength range from 900 to 950 nm produced by passive mode-locking techniques have become highly desirable for use in two-photon bioimaging (TPM) systems for the efficient excitation of green fluorescent proteins and their variants.14 – 18 Combined with nonlinear frequency conversion, 1.0-μm Yb3+-doped,12 1.5-μm Er3+-doped,19 and 1.9-μm Tm3+-doped10,13 ultrashort fiber lasers have been utilized to achieve 900- ∼950-nm ultrashort pulses, which have propelled the advances of TPM systems, with the only drawback being the reduced all-fiber configuration as a result of using these additional nonlinear media. As a comparison, the direct generation of ultrashort pulses at 920 nm using Nd3+-doped fibers is a more straightforward method9,20 – 24 and has attracted considerable research interest because the emission of its three-level (F43/2→I49/2) transition falls into the 900 to 950 nm wavelength band.

This publication has 42 references indexed in Scilit: