Abstract
Low temperature deposited coatings have the potential to reduce the production costs of silicon (Si) photovoltaic devices, such as the buried-contact (BC) solar cell. This work investigates the potential of titanium dioxide ( TiO 2 ) films to replace silicon dioxide ( SiO 2 ) or nitride coatings currently implemented in the BC fabrication sequence, which requires films to be stable at temperatures up to 1000 °C in a variety of gas atmospheres. The authors demonstrate that: (i) TiO 2 films do not reduce the bulk minority carrier lifetime of the silicon wafer after lengthy high temperature processing, however chemical reduction of the TiO 2 film can occur if samples are not loaded in an oxygen-containing ambient; (ii) a thin SiO 2 passivation layer can be formed at the TiO 2 : Si interface by performing a brief oxidation after TiO 2 film deposition; (iii) while TiO 2 coatings function as a phosphorus diffusion barrier, reactions between TiO 2 and the phosphorus source result in irreversible damage to the TiO 2 film; (iv) phosphorus-doped TiO 2 films can act as an n-type dopant source, however further reactions with phosphorus limit the usefulness of the film. Thus, TiO 2 films are compatible with the high temperature processing required for BC solar cells, but not with any phosphorus diffusion steps.

This publication has 31 references indexed in Scilit: