Abstract
The α/β interface in Ti-6Al-2Sn-4Zr-6Mo (Ti-6246) was investigated via center of symmetry analysis, both as-grown and after 10% cold work. Semicoherent interface steps are observed at a spacing of 4.5±1.13 atoms in the as-grown condition, in good agreement with theory. Lattice accommodation is observed, with elongation along [1¯21¯0]α and contraction along [101¯0]α. Deformed α exhibited larger, less coherent steps with slip bands lying in {110}β. This indicates dislocation pile-up at the grain boundary, a precursor to globularization during heat treatment. Atom probe tomography measurements of secondary α plates in the fully heat-treated condition showed a Zr excess at the interface, which was localized into regular structures indicative of Zr association with interface defects, such as dislocations. Such chemo-mechanical stabilization of the interface defects would both inhibit plate growth during elevated temperature service and the interaction of interface defects with gliding dislocations during deformation.
Funding Information
  • Engineering and Physical Sciences Research Council (EP/K034332/1, EP/M506345/1, EP/L025213/1)
  • China Scholarship Council
  • Bundesministerium für Forschung, Technologie und Raumfahrt

This publication has 41 references indexed in Scilit: