BACKGROUND: The incorporation of 4HB units into P(3HB) improves the material application potential as the copolymer exhibits a wide range of physical properties ranging from crystalline plastic to elastic rubber depending on the copolymer composition. Thus, the prospects of synthesizing P(3HB‐co‐4HB) copolymer with various compositions of 4HB would increase its effectiveness as biomaterial.RESULTS: The residual cell dry weight (RCDW) and PHA concentration obtained under optimized conditions, namely C/N ratio 30, K2HPO4 6.1 g L‐1, incubation period 66 h, temperature 32°C and volume‐to‐flask ratio 47/250 mL increased from 2.9 g L‐1 to 4.9 g L‐1 and 4.2 g L‐1 to 7.6 g L‐1, respectively. P(3HB‐co‐4HB) with varied Mn between 26 kDa and 270 kDa were successfully synthesized using combinations of oleic acid, 1,6‐hexanediol and/or 1,4‐butanediol. The tensile strength and Young's modulus of the copolymers varied from 2 MPa to 24 MPa and 13 MPa to 192 MPa, respectively. Tm and Tg decreased with increasing 4HB molar fractions from 170°C to 68°C and 2.5°C to −31°C, respectively.CONCLUSION: Oleic acid and (NH4)2SO4 was the best carbon and nitrogen source for PHA biosynthesis. P(3HB‐co‐4HB) copolymer with targeted 4HB molar fractions ranged from 0–65 mol% were synthesized using combinations of two or more carbon substrates by Cupriavidus sp. USMAA2‐4 (DSM 19379) using mixture design. © 2013 Society of Chemical Industry

This publication has 44 references indexed in Scilit: