Numerical Simulation of Meso-Damage Evolution Laws in Concrete Subjected to Open-Flame High-Temperature

Authors:
  • KZKaiyue Zhang
    Kaiyue Zhang
  • YZYue Zhai
    Yue Zhai
  • YHYaoying Huang
    Yaoying Huang
  • JZJunnan Zhao
    Junnan Zhao

Abstract
High temperatures caused by tunnel fires can easily lead to performance degradation or even collapse of concrete lining structures. A scientific understanding of the meso-damage evolution mechanism is crucial for enhancing structural fire resistance and post-disaster safety assessment. In this research, C35 concrete, commonly used in tunnel engineering, was subjected to open-flame high-temperature exposure for durations of 0, 10, 20, and 30 minutes using a self-designed open-flame combustion device following the ISO-834 standard heating curve. Based on CT slices, a three-dimensional segregated mesoscale model of the actual concrete mesostructure was reconstructed using Avizo software. The temperature field, thermal stress field, and the random initiation and propagation of thermal cracks within the concrete after single-sided fire exposure were simulated using indirect thermo-mechanical coupling and the eXtended Finite Element Method (XFEM). The results reveal that the interfacial transition zone (ITZ) between aggregate and mortar, due to the disparity in thermal properties, becomes the core area of thermal stress concentration and the primary site for micro-crack initiation, following a damage path of temperature gradient driving-thermal stress concentration- micro-crack initiation and propagation. Quantitative results show that after 30 minutes of high-temperature exposure, the mass loss rate of the specimen reached 6.68%, the maximum temperature on the heated surface reached 1049°C, while the central region temperature was only 363°C, resulting in a temperature difference of 686°C. The temperature difference between aggregates and mortar at nodal points decreased to 77°C at 20 minutes and stabilized between 50°C and 70°C after 30 minutes. The temperature field exhibited a three-stage evolution characteristic of gradient transmission-rate decay-steady-state convergence. Thermal stress concentrated on the aggregate surface and the ITZ, where cracks preferentially initiated, and the damage evolution followed a progressive pattern of local initiation-connectivity-global saturation. This study systematically reveals the failure mechanism of concrete under open-flame high-temperature exposure, providing a quantitative and meso-scale theoretical basis for the fire resistance design of tunnel linings, post-fire safety assessment, and emergency repair decision-making.

This publication has 18 references indexed in Scilit: