Effects of different activating fluxes on the surface tension of molten metal in gas tungsten arc welding
- 1 April 2018
- journal article
- research article
- Published by Elsevier in Journal of Manufacturing Processes
- Vol. 32, 395-402
Abstract
No abstract availableKeywords
Funding Information
- National Natural Science Foundation of China (51765037)
This publication has 20 references indexed in Scilit:
- Development of simplified active flux tungsten inert gas welding for deep penetrationMaterials & Design (1980-2015), 2014
- Measurement of surface tension and specific heat of Ni-18.8 at.% Si alloy melt by containerless processingJournal of Materials Science, 2011
- GTAW liquid pool convections and the weld shape variations under helium gas shieldingInternational Journal of Heat and Mass Transfer, 2011
- Solidification Velocities in Deeply Undercooled SilverPhysical Review Letters, 2009
- Effect of oxide fluxes on activation mechanisms of tungsten inert gas processScience and Technology of Welding and Joining, 2006
- Measurement of the density and surface tension of Ni-based superalloys in the liquid and mushy statesMetallurgical and Materials Transactions B, 2005
- Investigation into arc constriction by active fluxes for tungsten inert gas weldingScience and Technology of Welding and Joining, 2000
- The surface tension of molten aluminum and Al-Si-Mg alloy under vacuum and hydrogen atmospheresMetallurgical and Materials Transactions B, 1999
- Measurements of surface tension on levitated oscillating metallic dropsMaterials Science and Engineering: A, 1991
- Effects of wetting and surface oxidation on the measurement of the surface tension of Al by the maximum bubble pressure methodScripta Metallurgica et Materialia, 1991