High‐Temperature Strength and Creep Behavior of Melt‐Infiltrated SiC‐Mo≤5Si3C≤1 Composites

Authors:

Abstract
Molybdenum carbosilicide composites (SiC‐Mo≤5Si3C≤1) were fabricated via the melt‐infiltration process. The fracture behavior of the composites was studied from room temperature up to 1800°C in 1 atm (∼105 Pa) of argon. The bend strength of the composites slightly increased at ∼1200°C, because of the brittle‐ductile transition of the intermetallic phase. The composites retained ∼90% of their room‐temperature strength, even at 1700°C. Compressive creep tests were performed over a temperature range of 1760°‐1850°C and a stress range of 200–250 MPa. The creep rate of the SiC‐Mo≤5Si3C≤1 composites was approximately an order of magnitude higher than that of reaction‐bonded SiC.