Effect of Rapid Heating on a Cold-Rolled Mn–Al Transformation-Induced Plasticity Steel with Coarse Delta-Ferrite

Authors:
  • ZHZhi-Ping Hu
    Zhi-Ping Hu
  • XTXiao-Dong Tan
    Xiao-Dong Tan
  • FPFei Peng
    Fei Peng
  • XGXing-Li Gu
    Xing-Li Gu
  • YZYing Zou
    Ying Zou
  • SYShi-Chuan Yu
    Shi-Chuan Yu

Abstract
In this study, the effect of rapid heating on the microstructure and tensile properties of intercritically annealed Mn–Al transformation-induced plasticity (TRIP) steel with coarse δ-ferrite was evaluated. Cold-rolled Fe–0.18C–6.4Mn–2.8Al TRIP steel was heated to the intercritical annealing temperature (730–850 °C) at three different heating rates (5 °C/s, 50 °C/s, and 150 °C/s). With increasing heating rate, the optimized annealing temperature increased, and the optimized annealing time decreased. Through rapid heating at 150 °C/s and intercritical annealing at 820 °C, an excellent combination of tensile strength (1010 MPa) and elongation (31%) was obtained with a microstructure composition of coarse δ-ferrite, α-ferrite, and retained austenite. Some retained austenite with an adequate enrichment of C and Mn were observed in the areas surrounded by coarse δ-ferrite. Because of rapid heating, the intercritically annealed steels had an adequate volume fraction of retained austenite (32.9%), leading to a good work-hardening behavior owing to the efficient TRIP effect.