Preparation and luminescence of nano-sized In2O3and rare-earth co-doped SiO2thin films

Authors:
  • TLTao Lin
    Tao Lin
  • JXJun Xu
    Jun Xu
  • LXLing Xu
    Ling Xu
  • KCKunji Chen
    Kunji Chen

Abstract
The sol-gel method was used to prepare SiO(2) thin films co-doped with In(2)O(3) nano-particles and Eu(3+). The formation of nano-sized In(2)O(3) particles after annealing at 900 °C was confirmed by the x-ray diffraction technique. A novel phase transition from a hexagonal rhombic centered to a body centered cubic structure of In(2)O(3) nano-particles was observed at around 1100 °C. It is found that the particle size and the particle density of In(2)O(3) can be tuned by changing the annealing temperature and the indium doping concentration, respectively. The characteristic emission bands from Eu(3+) ions can be observed at room temperature and the luminescence intensity is increased 20 times by introducing In(2)O(3) nano-particles into Eu(3+)-doped silica films. The integrated luminescence intensity was gradually enhanced by increasing the In(3+) concentration, suggesting effective energy transfer from nano-sized In(2)O(3) to Eu(3+) ions.

This publication has 17 references indexed in Scilit: