Effects of Ni and Si on Delayed Fracture Properties of High Strength Steels with 1420 MPa Grade
Open Access
- 1 January 1996
- journal article
- Published by Iron and Steel Institute of Japan in Tetsu-to-Hagane
- Vol. 82 (9) , 777-782
Abstract
Effects of Ni and Si on delayed fracture properties of high strength steels with 1420MPa grade were investigated. 0.25% to 3.5% of Ni or 0.25% to 1.7% of Si was added respectively to 0.3%C-boron-containing steel. Delayed fracture test and measurement of diffusible hydrogen were carried out using bar steels for prestressed concrete with a diameter of 7.1 mm. As each addition of Ni or Si was increased, diffusible hydrogen decreased and delayed fracture properties improved in condition as heat treated. Diffusible hydrogen in Ni-containing steels increased after polishing the surface in comparison with as heat treated and no diffusible hydrogen in Si-containing steels was varied. In Ni-containing steels, Ni concentrating and Ni-sulphide forming at the surface retarded the absorption of hydrogen and delayed fracture properties were improved, while in Si-containing steels, variation of microstructure decreased trapping sites of hydrogen and consequently the absorption of hydrogen was prevented and delayed fracture properties improved.Keywords
This publication has 3 references indexed in Scilit:
- Thermal analysis of trapped hydrogen in pure ironMetallurgical Transactions A, 1982
- Effects of hydrogen on the properties of iron and steelMetallurgical Transactions A, 1980
- The effects of alloying elements on the susceptibility to stress-corrosion cracking of martensitic steels in salt waterMetallurgical Transactions, 1971