Evaluation of the compensation ratio of heavily-Ga doped Ge for far-infrared detectors in astronomy

Authors:
  • TSToyoaki Suzuki
    Toyoaki Suzuki
  • HKHidehiro Kaneda
    Hidehiro Kaneda
  • TWTakehiko Wada
    Takehiko Wada
  • SUSouta Ukai
    Souta Ukai
  • MHMisaki Hanaoka
    Misaki Hanaoka
  • KSKazuyuki Shichi
    Kazuyuki Shichi
  • HMHiroki Maeda
    Hiroki Maeda
  • SOShinki Oyabu
    Shinki Oyabu
  • KWKentaroh Watanabe
    Kentaroh Watanabe

Abstract
Ge-based blocked impurity band detectors fabricated with the surface-activated wafer bonding (SAB) method are expected to realize larger format arrays for far-infrared astronomical observations. To make sensitive p-type Ge detectors, the minor impurity ( N D ) concentration of a heavily-impurity doped Ge wafers is required to be 14 cm −3 in addition to the major impurity ( N A ) concentration of ∼10 16 cm −3 . Thus, a compensation ratio K (= N D / N A ) below 10 −2 should be achieved in advance to SAB. We measured the resistivity and carrier density of heavily-Ga doped Ge wafers at temperatures of 3–300 K. However, N D and N A of the wafers cannot be obtained from the conventional model for p-type semiconductors due to the significant contribution of the impurity band conduction (IBC). Then, an extended model including the IBC process was constructed, which was found to well reproduce the measured data over the whole temperature range. From the values obtained from the model fitting, it is revealed that our heavily-Ga doped Ge wafers show N A ∼ 10 16 cm −3 with ultra-low K below 10 −3 .

This publication has 32 references indexed in Scilit: