Abstract
The electron and hole conductivity of [(ZrO2)1−x(CeO2)x]0.8(YO1.5)0.2(x=0–1,0.1step)[(ZrO2)1−x(CeO2)x]0.8(YO1.5)0.2(x=0–1,0.1step) solid solutions was measured by dc polarization method using a modified Hebb–Wagner’s ion blocking cell at 973, 1073, 1173, and 1273K1273K as a function of oxygen partial pressure. All measured data were fitted to the sum of the electron conductivity having a pO2−1∕4pO2−1∕4 dependence and the hole conductivity having a pO21∕4pO21∕4 dependence. At all temperatures, with increasing CeO2CeO2 concentration, the electron conductivity drastically increased at x=0x=0 –0.4 and slightly decreased at x=0.6x=0.6 –1.0, leading to a maximum at x=0.4x=0.4 –0.5. The logarithmic hole conductivity linearly increased with CeO2CeO2 concentration for x=0x=0 –1.

This publication has 9 references indexed in Scilit: