Abstract
The present study investigates the effect of grain boundary on the electrical conductivity of α-La2Mo2O9 (LAMOX) below transition its temperature i.e. 580 °C. The grain boundary effect was characterised by electrochemical impedance spectroscopy (EIS) at temperatures from 27 °C to 400 °C. The calculated value of grain boundary width for bulk La2Mo2O9 is found to be 14.6 nm and specific grain boundary conductivity is 0.0146 μS/cm. The total ionic conductivity for La2Mo2O9 calculated by EIS at 300 °C comes out to be 1 μS/cm. The conductivity value for grain boundary is two orders less than the total conductivity. This clearly suggests the high activation energy is required for grain boundary conduction. The electrical conductivity for La2Mo2O9 treated in Ar-H2 atmosphere is almost three orders higher than the conductivity values of LAMOX treated in air. This may be attributed to reduction of Mo to lower valance states in LAMOX confirmed as by x-ray photoelectron spectroscopy (XPS). Therefore, the low ionic conductivity nature of monoclinic phase of La2Mo2O9 is explained on the basis of grain boundary conduction mechanism.

This publication has 28 references indexed in Scilit: