Multiple Stress Creep and Recovery Behavior of SBR-Modified Bitumen Emulsions
- 1 November 2018
- journal article
- research article
- Published by ASTM International in Journal of Testing and Evaluation
- Vol. 48 (4) , 3116-3124
Abstract
The effect of two grades of styrene-butadiene rubber (SBR) at 2, 4, 6, and 8 wt. % on the deformation behavior of cationic polymer-modified bitumen emulsion by a multiple stress creep and recovery test at three different temperatures (58°C, 68°C, and 78°C) was investigated. It was observed that increasing SBR latex content leads to a decrease in nonrecoverable creep compliance (Jnr) of the bituminous residue, whereas increasing temperature leads to an increase in Jnr. The results also revealed that reduction in Jnr is not remarkable for polymer content higher than 6 wt. %. Furthermore, comparing the effect of different SBRs revealed that at equal polymer content, the Jnr of SBR-modified bitumen emulsion residue was found to be twice that of a branched carboxylated styrene-butadiene rubber (X-SBR)–modified one. At the same polymer modification rate and temperature, X-SBR can be used for higher traffic levels compared to an SBR-modified bitumen emulsion.Keywords
This publication has 3 references indexed in Scilit:
- Rheological characteristics of SBR and NR polymer modified bitumen emulsions at average pavement temperaturesConstruction and Building Materials, 2013
- Comparative Study on Recovered Binder Properties Using Three Asphalt Emulsion Recovery MethodsJournal of Testing and Evaluation, 2010
- Preparation of an SBS Latex–Modified Bitumen Emulsion and Performance AssessmentPetroleum Science and Technology, 2010