Abstract
The dielectric properties of solid solutions in the system SrTiO3-La2/3TiO3 were measured in a frequency range from 200 to 105 Hz and at temperatures from -190 to 400°C. The relative permittivity of the solid solutions is lower that of pure SrTiO3 and pronounced dielectric nonlinearity was not observed. Two separate groups of dielectric relaxation peaks were observed, a low temperature relaxation which occured in a temperature region below room temperature and a higher temperature process which occured at about 200°C. The experimental results were analyzed in the light of current theories for relaxation in high permittivity materials. It is suggested that the higher temperature relaxation is associated with a Maxwell-Wagner phenomenon due to the different properties of grain and grain boundaries in the ceramic specimen. For the lower temperature process the evidence is compatible with an ionic model of the Debye type. It is suggested that the existence of the A site vacancy in the perovskite ABO3 lattice introduced by the lanthanum substitution distorts the oxygen octahedron, producing more than one possible “non central” sites for the Ti4+ ion. The relaxation arises from the thermal motion over potential barriers separating these alternative sites.Keywords
This publication has 11 references indexed in Scilit:
- Dielectric Loss due to Impurity Cation Migration in α QuartzJournal of Applied Physics, 1964
- Mechanical and Electrical Relaxation in ThContaining CaOPhysical Review B, 1963
- Some Structural and Electrical Properties of Lithium Silicate GlassesJournal of the American Ceramic Society, 1963
- Ferroelectric Behavior in Barium Zirconium MetaniobateJournal of the American Ceramic Society, 1960
- Dielectric properties of single crystals of SrTiO3 at low temperaturesJournal of Physics and Chemistry of Solids, 1959
- The structure and dielectric properties of compounds with the formula BAx(Ti8–xMgx)O16Transactions of the Faraday Society, 1958
- Dielectric Relaxation and the Internal FieldThe Journal of Chemical Physics, 1953
- On the Dispersion of Resistivity and Dielectric Constant of Some Semiconductors at AudiofrequenciesPhysical Review B, 1951
- Electric Moments of Molecules in LiquidsJournal of the American Chemical Society, 1936
- Rochelle Salt as a DielectricPhysical Review B, 1930