In-Pile Diameter Measurement of Light Water Reactor Test Fuel Rods for Assessment of Pellet-Cladding Mechanical Interaction
Authors:
- 1 November 1980
- journal article
- research article
- Published by Taylor & Francis in Nuclear Technology
- Vol. 51 (1) , 33-44
Abstract
Three Zircaloy-clad UO2 test fuel rods were irradiated at 50 kW/m to a burnup of 15 000 MWd/MTU with an in-pile rod diameter scanning device, and cladding deformations were measured at various power and burnup levels. Major mode of deformation was ridging at pellet interface positions. Magnitude and relevant power levels for various modes of cladding deformation were found to be strongly dependent on initial pellet-cladding gap size. During the first approach to power, smaller gap size caused larger cladding deformation; however, the effect was reversed at higher burnup. Cladding diametral deformation was found to be dictated not only by local thermal expansion of a single pellet, but also by long-range axial force in the pellet stack. In the first power cycle, cladding deformations caused by power ramp were found to decrease during subsequent power holding, but their rate was much reduced at high burnup.Keywords
This publication has 4 references indexed in Scilit:
- Effects of fill gas composition and pellet eccentricity. [BWR]1977
- MATPRO: a handbook of materials properties for use in the analysis of light water reactor fuel rod behavior1976
- Creep behavior of ceramic nuclear fuels under neutron irradiationJournal of Nuclear Materials, 1972