Keita Endo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Keita Endo has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Naoto Kudo
Faculty of Engineering, Tohoku Gakuin University, Tagajo 985-8537, Japan
2 shared publications - Hironori Nishihara
Faculty of Science and Technology, Ryukoku University, Otsu 520-2194, Japan
1 shared publication - Hiroyuki Nojiri
Tohoku University
1 shared publication - Kurt R.A. Ziebeck
Department of Physics, Cavendish Laboratory, University of Cambridge, Cambridge CB3 0HE, UK
1 shared publication - Makoto Nagasako
Department of Materials Science, Graduate School of Engineering, Tohoku University, Sendai 980-8579, Japan
1 shared publication - Masayuki Hagiwara
The University of Osaka
1 shared publication
Latest Publications
- Open Access
- 11 September 2025
- Published by IntechOpen
Forced Magnetostriction of Heusler Ferromagnetic Alloy Ni2(Mn,Cu)Ga around Martensitic Transition Temperature
We performed measurements of magnetization and magnetostriction for the ferromagnetic Heusler alloy Ni2Mn0.75Cu0.25Ga. We observed substantial magnetostriction (magnetic-field-induced strain, MFIS) at the temperature of the martensitic structural phase transition (TM), where the ferromagnetic transition coincides. During the crystal structure transition at TM, a pronounced forced magnetostriction caused by the magnetic fields accompanied the magnetic-field-induced martensitic transformation. Thus, this magnetostriction can also be viewed as the martensitic phase transition in the presence of a magnetic field. Magnetization measurements (M-H) revealed a large jump and clear hysteresis around μ0H = 6 T and approximately 310 K, attributed to a meta-magnetic-like transition between the paramagnetic austenite phase and the ferromagnetic martensite phase. These results suggest that the phase transition was a first-order magneto-structural transition induced by the magnetic field. Measurements of forced magnetostriction (∆L/L) were performed at constant temperature and atmospheric pressure (P = 0.1 MPa). A magnetostriction of up to 2000 ppm (0.20%) was observed around the martensitic transition temperature, TM = 308 K. The findings from magnetization (M-H) and magnetostriction (∆L/L) indicate that the large MFIS resulted from the magneto-structural transition from the paramagnetic austenite phase to the ferromagnetic martensite phase. From the considerations of the magnetic entropy change ΔS and magnetostriction ∆L/L, it is conceivable that the ferromagnetic transition and magnetic-field-induced martensitic transition are associated with each other.
- 11 September 2025
- Published by IntechOpen
Open AccessForced Magnetostriction of Heusler Ferromagnetic Alloy Ni2(Mn,Cu)Ga around Martensitic Transition Temperature
We performed measurements of magnetization and magnetostriction for the ferromagnetic Heusler alloy Ni2Mn0.75Cu0.25Ga. We observed substantial magnetostriction (magnetic-field-induced strain, MFIS) at the temperature of the martensitic structural phase transition (TM), where the ferromagnetic transition coincides. During the crystal structure transition at TM, a pronounced forced magnetostriction caused by the magnetic fields accompanied the magnetic-field-induced martensitic transformation. Thus, this magnetostriction can also be viewed as the martensitic phase transition in the presence of a magnetic field. Magnetization measurements (M-H) revealed a large jump and clear hysteresis around μ0H = 6 T and approximately 310 K, attributed to a meta-magnetic-like transition between the paramagnetic austenite phase and the ferromagnetic martensite phase. These results suggest that the phase transition was a first-order magneto-structural transition induced by the magnetic field. Measurements of forced magnetostriction (∆L/L) were performed at constant temperature and atmospheric pressure (P = 0.1 MPa). A magnetostriction of up to 2000 ppm (0.20%) was observed around the martensitic transition temperature, TM = 308 K. The findings from magnetization (M-H) and magnetostriction (∆L/L) indicate that the large MFIS resulted from the magneto-structural transition from the paramagnetic austenite phase to the ferromagnetic martensite phase. From the considerations of the magnetic entropy change ΔS and magnetostriction ∆L/L, it is conceivable that the ferromagnetic transition and magnetic-field-induced martensitic transition are associated with each other.
- Open Access
Magnetic Moment of Cu-Modified Ni2MnGa Magnetic Shape Memory Alloys
The magnetization measurements at 5 K were carried out for Ni2Mn1 − xCuxGa (0 ≤ x ≤ 0.40) and Ni2MnGa1 − yCuy (0 ≤ y ≤ 0.25) alloys. All of the magnetization curves are characteristic of ferromagnetism or ferrimagnetism. By using Arrott plot analysis the spontaneous magnetization of all samples was determined from the magnetization curves. The magnetic moment per formula unit, μs, at 5 K was estimated from the spontaneous magnetization. For Ni2Mn1 − xCuxGa (0 ≤ x ≤ 0.40) alloys μs at 5 K decreases linearly with increasing x. On the other hand, the μs at 5 K for Ni2MnGa1 − yCuy (0 ≤ y ≤ 0.25) alloys decreases more steeply with increasing x compared to the μs for Ni2Mn1 − xCuxGa (0 ≤ x ≤ 0.40) alloys. On the basis of the experimental results, the site-occupation configurations of Ni2Mn1 − xCuxGa (0 ≤ x ≤ 0.40) and Ni2MnGa1 − yCuy (0 ≤ y ≤ 0.25) alloys are proposed.
Open AccessMagnetic Moment of Cu-Modified Ni2MnGa Magnetic Shape Memory Alloys
The magnetization measurements at 5 K were carried out for Ni2Mn1 − xCuxGa (0 ≤ x ≤ 0.40) and Ni2MnGa1 − yCuy (0 ≤ y ≤ 0.25) alloys. All of the magnetization curves are characteristic of ferromagnetism or ferrimagnetism. By using Arrott plot analysis the spontaneous magnetization of all samples was determined from the magnetization curves. The magnetic moment per formula unit, μs, at 5 K was estimated from the spontaneous magnetization. For Ni2Mn1 − xCuxGa (0 ≤ x ≤ 0.40) alloys μs at 5 K decreases linearly with increasing x. On the other hand, the μs at 5 K for Ni2MnGa1 − yCuy (0 ≤ y ≤ 0.25) alloys decreases more steeply with increasing x compared to the μs for Ni2Mn1 − xCuxGa (0 ≤ x ≤ 0.40) alloys. On the basis of the experimental results, the site-occupation configurations of Ni2Mn1 − xCuxGa (0 ≤ x ≤ 0.40) and Ni2MnGa1 − yCuy (0 ≤ y ≤ 0.25) alloys are proposed.