Ashok Kumar
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Ashok Kumar has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
- Makoto Hirai
University of South Florida
2 shared publications Sathyaharish Jeedigunta
Nanomaterials and Nanomanufacturing Research Center, University of South Florida, Tampa, FL and Department of Electrical Engineering, University of South Florida, Tampa, FL
2 shared publicationsA.K. Sikder
Nanomaterials and Nanomanufacturing Research Center, University of South Florida, Tampa, Florida 33620
1 shared publicationChristopher L. Frewin
University of South Florida, Electrical Engineering Department, Tampa, Florida, United States
1 shared publication- Christopher Locke
University of South Florida, 4202 E. Fowler Ave, ENB 118, Tampa, Florida, 33620, United States
1 shared publication Elias Stefanakos
Clean Energy Research Center, University of South Florida, Tampa, FL 33620, USA
1 shared publication
Latest Publications
- Open Access
- 1 July 2009
- Published by Springer Nature in Discover Nano
- Vol. 4 (10) , 1191-1196
Pd Nanoparticles and Thin Films for Room Temperature Hydrogen Sensor
We report the application of palladium nanoparticles and thin films for hydrogen sensor. Electrochemically grown palladium particles with spherical shapes deposited on Si substrate and sputter deposited Pd thin films were used to detect hydrogen at room temperature. Grain size dependence of H2sensing behavior has been discussed for both types of Pd films. The electrochemically grown Pd nanoparticles were observed to show better hydrogen sensing response than the sputtered palladium thin films. The demonstration of size dependent room temperature H2sensing paves the ways to fabricate the room temperature metallic and metal–metal oxide semiconductor sensor by tuning the size of metal catalyst in mixed systems. H2sensing by the Pd nanostructures is attributed to the chemical and electronic sensitization mechanisms.
- 1 July 2009
- Published by Springer Nature in Discover Nano
- Vol. 4 (10) , 1191-1196
Open AccessPd Nanoparticles and Thin Films for Room Temperature Hydrogen Sensor
We report the application of palladium nanoparticles and thin films for hydrogen sensor. Electrochemically grown palladium particles with spherical shapes deposited on Si substrate and sputter deposited Pd thin films were used to detect hydrogen at room temperature. Grain size dependence of H2sensing behavior has been discussed for both types of Pd films. The electrochemically grown Pd nanoparticles were observed to show better hydrogen sensing response than the sputtered palladium thin films. The demonstration of size dependent room temperature H2sensing paves the ways to fabricate the room temperature metallic and metal–metal oxide semiconductor sensor by tuning the size of metal catalyst in mixed systems. H2sensing by the Pd nanostructures is attributed to the chemical and electronic sensitization mechanisms.
- 1 April 2009
- Published by Springer Nature
- p. 425-429
Electrodeposition of Bi1−xSbx Nanowires as an Advanced Material for Thermoelectric Applications
- 1 April 2009
- Published by Springer Nature
- p. 425-429
Electrodeposition of Bi1−xSbx Nanowires as an Advanced Material for Thermoelectric Applications
- 1 January 2009
- Published by Springer Nature in MRS Proceedings
- Vol. 1203
Study of the Adhesion and Biocompatibility of Nanocrystalline Diamond (NCD) Films on 3C-SiC Substrates
- 1 January 2009
- Published by Springer Nature in MRS Proceedings
- Vol. 1203
Study of the Adhesion and Biocompatibility of Nanocrystalline Diamond (NCD) Films on 3C-SiC Substrates
- Open Access
- 1 January 2008
- Published by Wiley in Journal of Nanomaterials
- Vol. 2008 (1)
Fabrication and Characterization of ZnO Nanowire Arrays with an Investigation into Electrochemical Sensing Capabilities
ZnO nanowire arrays were grown on a Si (100) substrate using the vapor‐liquid‐solid (VLS) method. ZnO nanowires were characterized by XRD, SEM, bright field TEM, and EDS. They were found to have a preferential orientation along the c‐axis. The as‐prepared sample was functionalized with glucose oxidase by physical adsorption. FTIR was taken before and after functionalization to verify the presence of the attached enzyme. Electrochemical measurements were performed on the nanowire array by differential pulse voltammetry in the range of −0.6 to 0.4 V. The nanoarray sensor displayed high sensitivity to glucose in the range of 1.0 ×10−4 to 1.0 ×10−2 mol L−1.
- 1 January 2008
- Published by Wiley in Journal of Nanomaterials
- Vol. 2008 (1)
Open AccessFabrication and Characterization of ZnO Nanowire Arrays with an Investigation into Electrochemical Sensing Capabilities
ZnO nanowire arrays were grown on a Si (100) substrate using the vapor‐liquid‐solid (VLS) method. ZnO nanowires were characterized by XRD, SEM, bright field TEM, and EDS. They were found to have a preferential orientation along the c‐axis. The as‐prepared sample was functionalized with glucose oxidase by physical adsorption. FTIR was taken before and after functionalization to verify the presence of the attached enzyme. Electrochemical measurements were performed on the nanowire array by differential pulse voltammetry in the range of −0.6 to 0.4 V. The nanoarray sensor displayed high sensitivity to glucose in the range of 1.0 ×10−4 to 1.0 ×10−2 mol L−1.
- 28 September 2007
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 25 (6) , 1534-1538
Effect of nitrogen doping on bonding state of ZnO thin films
Nitrogen (N) is the most promising -type dopant for zinc oxide (ZnO) with wurtzite structure. The substitution of N atoms for partial replacement of O atoms in wurtzite structure is predicted to cause the slight change in bonding state. We have synthesized ZnO and N-doped ZnO thin films by utilizing a pulsed laser deposition method. Compared with the ultraviolet-visible spectrum of the ZnO thin film, since the absorption edge of the N-doped ZnO thin film denoted a clear redshift, the band gap shrank for the incorporation of N atoms. The band-gap shrinkage of the N-doped ZnO thin film was considered to be due to the existence of Zn–N bond having smaller ionicity than Zn–O bond. Additionally, from the results of Fourier transform infrared measurements, the absorption peaks of the ZnO and N-doped ZnO thin films emerged at 415 and , respectively, and were attributed to transverse optical phonon of mode. The reduction in phonon frequency of approximately can be induced by the complex factors consisting of not only the decrease in reduced mass and interionic distance but also the increase in covalency.- 28 September 2007
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 25 (6) , 1534-1538
Effect of nitrogen doping on bonding state of ZnO thin films
Nitrogen (N) is the most promising -type dopant for zinc oxide (ZnO) with wurtzite structure. The substitution of N atoms for partial replacement of O atoms in wurtzite structure is predicted to cause the slight change in bonding state. We have synthesized ZnO and N-doped ZnO thin films by utilizing a pulsed laser deposition method. Compared with the ultraviolet-visible spectrum of the ZnO thin film, since the absorption edge of the N-doped ZnO thin film denoted a clear redshift, the band gap shrank for the incorporation of N atoms. The band-gap shrinkage of the N-doped ZnO thin film was considered to be due to the existence of Zn–N bond having smaller ionicity than Zn–O bond. Additionally, from the results of Fourier transform infrared measurements, the absorption peaks of the ZnO and N-doped ZnO thin films emerged at 415 and , respectively, and were attributed to transverse optical phonon of mode. The reduction in phonon frequency of approximately can be induced by the complex factors consisting of not only the decrease in reduced mass and interionic distance but also the increase in covalency.- 1 April 2007
- Published by Springer Nature in Journal of Materials Research
- Vol. 22 (4) , 1012-1017
Analysis of residual stresses in diamond coatings deposited on cemented tungsten carbide substrates
Residual stresses in diamond films grown on WC–Co substrates have been investigated by Raman spectroscopy, x-ray diffraction (XRD), and curvature methods. Microcrystalline diamond films were deposited at 650–700 °C in a conventional hydrogen–methane environment by the microwave plasma-enhanced chemical vapor deposition technique. The film thickness, measured from cross-sectional micrographs taken by scanning electron microscopy, changed from 1.5 to 16.5 μm as the growth time increased from 1 to 12 h. The type and the magnitude of the total residual stress obtained from curvature and XRD measurements agreed very well in all of the samples and changed from tensile to compressive as film thickness increased. However, Raman spectroscopy results showed that all films exhibited compressive stress due to the domain size effect. Different methane fractions, varying from 1% to 3%, have been utilized for diamond growth, and the total residual stress increased as more methane was included.
- 1 April 2007
- Published by Springer Nature in Journal of Materials Research
- Vol. 22 (4) , 1012-1017
Analysis of residual stresses in diamond coatings deposited on cemented tungsten carbide substrates
Residual stresses in diamond films grown on WC–Co substrates have been investigated by Raman spectroscopy, x-ray diffraction (XRD), and curvature methods. Microcrystalline diamond films were deposited at 650–700 °C in a conventional hydrogen–methane environment by the microwave plasma-enhanced chemical vapor deposition technique. The film thickness, measured from cross-sectional micrographs taken by scanning electron microscopy, changed from 1.5 to 16.5 μm as the growth time increased from 1 to 12 h. The type and the magnitude of the total residual stress obtained from curvature and XRD measurements agreed very well in all of the samples and changed from tensile to compressive as film thickness increased. However, Raman spectroscopy results showed that all films exhibited compressive stress due to the domain size effect. Different methane fractions, varying from 1% to 3%, have been utilized for diamond growth, and the total residual stress increased as more methane was included.
- 1 January 2007
- Published by Springer Nature in MRS Proceedings
- Vol. 1035
Infrared Lattice Vibrations of Nitrogen-doped ZnO Thin Films
Nitrogen (N) is the most promising p-type dopant for zinc oxide (ZnO), and its bonding state must be governed by the substitution of N atoms into anion sites. We have synthesized un-doped ZnO and N-doped ZnO thin films by utilizing a pulsed laser deposition (PLD) method. The N-doped ZnO thin film possessed shorter c-axis length than the un-doped ZnO thin film. This fact seems to be owing to that Zn-N bond length is shorter than Zn-O bond length in wurtzite structure. Besides, from the result of Fourier transform infrared (FT-IR) measurement, the absorption peak of the N-doped ZnO thin film emerged at 406 cm−1, and was attributed to transverse optical (TO) phonon of E1 mode. The infrared lattice vibrations of the N-doped ZnO thin films can be induced by the complex factors consisting of not only the decreases in reduced mass and interionic distance, but also the increase in covalency.
- 1 January 2007
- Published by Springer Nature in MRS Proceedings
- Vol. 1035
Infrared Lattice Vibrations of Nitrogen-doped ZnO Thin Films
Nitrogen (N) is the most promising p-type dopant for zinc oxide (ZnO), and its bonding state must be governed by the substitution of N atoms into anion sites. We have synthesized un-doped ZnO and N-doped ZnO thin films by utilizing a pulsed laser deposition (PLD) method. The N-doped ZnO thin film possessed shorter c-axis length than the un-doped ZnO thin film. This fact seems to be owing to that Zn-N bond length is shorter than Zn-O bond length in wurtzite structure. Besides, from the result of Fourier transform infrared (FT-IR) measurement, the absorption peak of the N-doped ZnO thin film emerged at 406 cm−1, and was attributed to transverse optical (TO) phonon of E1 mode. The infrared lattice vibrations of the N-doped ZnO thin films can be induced by the complex factors consisting of not only the decreases in reduced mass and interionic distance, but also the increase in covalency.
- 1 January 2007
- Published by Springer Nature in MRS Proceedings
- Vol. 1039
Role of Nucleation on the Growth of Nanocrystalline Diamond (NCD) Films: A Particular Study in the Fabrication of Micro-cantilevers
- 1 January 2007
- Published by Springer Nature in MRS Proceedings
- Vol. 1039
Role of Nucleation on the Growth of Nanocrystalline Diamond (NCD) Films: A Particular Study in the Fabrication of Micro-cantilevers
- 20 September 2006
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 32 (8) , 1010-1015
Polyaniline-based nanocomposite materials for hydrogen storage
- 20 September 2006
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 32 (8) , 1010-1015
Polyaniline-based nanocomposite materials for hydrogen storage
- 1 January 2006
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 153 (5) , G372-G378
Effects of Slurry Flow Rate and Pad Conditioning Temperature on Dishing, Erosion, and Metal Loss during Copper CMP
The effect of slurry flow rate, pad surface temperature, and temperature during the pad conditioning process on surface tribology and pattern-related defects like dishing, erosion, and metal loss was studied. Experimental results suggest that dishing and erosion levels decreased with increase in slurry flow rate. Conditioning experiments at various temperatures revealed a significant impact of temperature on the effectiveness of the conditioning process and also on subsequent polishing performance. The polishing pad was conditioned more aggressively at lower temperatures compared to conditioning at elevated temperatures. The removal rate and coefficient of friction were found to be significantly affected by the pad surface temperature. The amount of dishing increased with increase in pad surface temperature and the uniformity of polishing. The study ascertains a correlation between process parameters and the extent of planarity defects. This study also demonstrates the use of a modified bench-top chemical mechanical polish (CMP) tester and large-stage atomic force microscope with automatic multiscan imaging procedure.
- 1 January 2006
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 153 (5) , G372-G378
Effects of Slurry Flow Rate and Pad Conditioning Temperature on Dishing, Erosion, and Metal Loss during Copper CMP
The effect of slurry flow rate, pad surface temperature, and temperature during the pad conditioning process on surface tribology and pattern-related defects like dishing, erosion, and metal loss was studied. Experimental results suggest that dishing and erosion levels decreased with increase in slurry flow rate. Conditioning experiments at various temperatures revealed a significant impact of temperature on the effectiveness of the conditioning process and also on subsequent polishing performance. The polishing pad was conditioned more aggressively at lower temperatures compared to conditioning at elevated temperatures. The removal rate and coefficient of friction were found to be significantly affected by the pad surface temperature. The amount of dishing increased with increase in pad surface temperature and the uniformity of polishing. The study ascertains a correlation between process parameters and the extent of planarity defects. This study also demonstrates the use of a modified bench-top chemical mechanical polish (CMP) tester and large-stage atomic force microscope with automatic multiscan imaging procedure.