Sabine H. Dickens
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Sabine H. Dickens has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
Glenn M. Flaim
American Dental Association Foundation, National Institute of Standards and Technology, Gaithersburg, MD
4 shared publicationsBaosheng Xie
2 shared publicationsA A Giuseppetti
1 shared publicationAnthony A Giuseppetti
1 shared publicationAnthony A. Giuseppetti
American Dental Association Foundation, Paffenbarger Research Center, National Institute of Standards and Technology, Gaithersburg, MD, USA
1 shared publicationCynthia J.E. Floyd
1 shared publication
Latest Publications
- 31 July 2010
- Published by Elsevier in Journal of Endodontics
- Vol. 36 (7) , 1222-1225
Preclinical Effectiveness of a Novel Pulp Capping Material
- 31 July 2010
- Published by Elsevier in Journal of Endodontics
- Vol. 36 (7) , 1222-1225
Preclinical Effectiveness of a Novel Pulp Capping Material
- 1 July 2010
- Published by Elsevier in Dental Materials
- Vol. 26 (7) , 675-681
Effects of adhesive, base and diluent monomers on water sorption and conversion of experimental resins
- 1 July 2010
- Published by Elsevier in Dental Materials
- Vol. 26 (7) , 675-681
Effects of adhesive, base and diluent monomers on water sorption and conversion of experimental resins
- 1 September 2008
- Published by Elsevier in Dental Materials
- Vol. 24 (9) , 1273-1280
Effect of a bonding agent on in vitro biochemical activities of remineralizing resin-based calcium phosphate cements
- 1 September 2008
- Published by Elsevier in Dental Materials
- Vol. 24 (9) , 1273-1280
Effect of a bonding agent on in vitro biochemical activities of remineralizing resin-based calcium phosphate cements
- 1 June 2008
- Published by Elsevier in Dental Materials
- Vol. 24 (6) , 778-785
Degree of cure and fracture properties of experimental acid-resin modified composites under wet and dry conditions
- 1 June 2008
- Published by Elsevier in Dental Materials
- Vol. 24 (6) , 778-785
Degree of cure and fracture properties of experimental acid-resin modified composites under wet and dry conditions
- 29 September 2004
- Published by Wiley in European Journal of Oral Sciences
- Vol. 112 (5) , 452-457
Dentin adhesion and microleakage of a resin‐based calcium phosphate pulp capping and basing cement
An experimental resin‐based bioactive calcium phosphate cement, intended as a pulp capping and basing material, was evaluated for dentin shear bond strength and microleakage. The interfacial morphology was examined by scanning electron microscopy (SEM). For microleakage, dentin cavities without (Group A) or after (Group B) acid etching were restored with the calcium phosphate cement. A resin‐based calcium hydroxide (VLC Dycal; Group C) was used as control material according to the manufacturer's instructions. After water storage and thermocycling, the microleakage was scored using a AgNO3 staining procedure. For the shear bond strength, flat exposed dentin surfaces were treated as for the microleakage test. Metal irises pressed against the dentin surface were filled with the cements, which were photocured. Both tests were carried out after 1 wk. While acid etching did not result in significantly greater microleakage, it led to higher shear bond strength, and allowed, as shown by SEM, the formation of a hybrid layer and resin tags. Both groups treated with the calcium phosphate cement had significantly lower microleakage scores and higher mean shear bond strength values than the groups treated with the control material.
- 29 September 2004
- Published by Wiley in European Journal of Oral Sciences
- Vol. 112 (5) , 452-457
Dentin adhesion and microleakage of a resin‐based calcium phosphate pulp capping and basing cement
An experimental resin‐based bioactive calcium phosphate cement, intended as a pulp capping and basing material, was evaluated for dentin shear bond strength and microleakage. The interfacial morphology was examined by scanning electron microscopy (SEM). For microleakage, dentin cavities without (Group A) or after (Group B) acid etching were restored with the calcium phosphate cement. A resin‐based calcium hydroxide (VLC Dycal; Group C) was used as control material according to the manufacturer's instructions. After water storage and thermocycling, the microleakage was scored using a AgNO3 staining procedure. For the shear bond strength, flat exposed dentin surfaces were treated as for the microleakage test. Metal irises pressed against the dentin surface were filled with the cements, which were photocured. Both tests were carried out after 1 wk. While acid etching did not result in significantly greater microleakage, it led to higher shear bond strength, and allowed, as shown by SEM, the formation of a hybrid layer and resin tags. Both groups treated with the calcium phosphate cement had significantly lower microleakage scores and higher mean shear bond strength values than the groups treated with the control material.
- 1 September 2003
- Published by Elsevier in Dental Materials
- Vol. 19 (6) , 558-566
Mechanical properties and biochemical activity of remineralizing resin-based Ca–PO4 cements
- 1 September 2003
- Published by Elsevier in Dental Materials
- Vol. 19 (6) , 558-566
Mechanical properties and biochemical activity of remineralizing resin-based Ca–PO4 cements
- 1 April 2003
- Vol. 34 (2) , 270-3
[Studies on bonding interfaces of two dentin adhesives by scanning electron microscopy].
To purpose of this study was to investigate the microstructure and bonding mechanism of bonding interfaces of two current one-bottle dentin bond systems(Prime & Bond NT, PBNT; Prime one Mirage, P-One). Fifteen extracted, caries-free human molars were prepared according to a modified method used for microtensile bond strength measurement. Each crown was divided into nearly equal halves with a 5 mm deep slot for accepting treatment of the two dentin bond systems, respectively. After 24 h storage in distilled water at 37 degrees C, the bonded teeth were subjected to two treatments: 5 teeth were observed by and tested for microtensile bond strengths without further treatment and 10 teeth were thermocycled(2400 cycles, between 5 degrees C and 55 degrees C) prior to SEM observation and bond strength testing. Hour-glass shaped microspecimens with a thickness of approximately 0.5 mm were cut from each tooth and used for SEM observation and microtensile bond strength measurement. A typical resin-infiltrated zone (hybrid layer) with a thickness of 3-5 microns and well-formed cone shaped resin tags that penetrated the dentinal tubules were clearly observed at the resin-dentin interfaces in the two bond systems. There were multiple lateral branches of tubular resin tags that interconnected to form a micro-network of resin. No evident differences in SEM images between the two bond systems as well as between thermocycling and without thermocycling in each bond system were found. PBNT and P-One provided good resin infiltration, producing a three-dimensional interlocking micro-network of resin tags in the dentin tubules with multiple lateral branches that penetrate the intertubular dentin, which positively influenced the adhesion between dentin and the two bond systems.
- 1 April 2003
- Vol. 34 (2) , 270-3
[Studies on bonding interfaces of two dentin adhesives by scanning electron microscopy].
To purpose of this study was to investigate the microstructure and bonding mechanism of bonding interfaces of two current one-bottle dentin bond systems(Prime & Bond NT, PBNT; Prime one Mirage, P-One). Fifteen extracted, caries-free human molars were prepared according to a modified method used for microtensile bond strength measurement. Each crown was divided into nearly equal halves with a 5 mm deep slot for accepting treatment of the two dentin bond systems, respectively. After 24 h storage in distilled water at 37 degrees C, the bonded teeth were subjected to two treatments: 5 teeth were observed by and tested for microtensile bond strengths without further treatment and 10 teeth were thermocycled(2400 cycles, between 5 degrees C and 55 degrees C) prior to SEM observation and bond strength testing. Hour-glass shaped microspecimens with a thickness of approximately 0.5 mm were cut from each tooth and used for SEM observation and microtensile bond strength measurement. A typical resin-infiltrated zone (hybrid layer) with a thickness of 3-5 microns and well-formed cone shaped resin tags that penetrated the dentinal tubules were clearly observed at the resin-dentin interfaces in the two bond systems. There were multiple lateral branches of tubular resin tags that interconnected to form a micro-network of resin. No evident differences in SEM images between the two bond systems as well as between thermocycling and without thermocycling in each bond system were found. PBNT and P-One provided good resin infiltration, producing a three-dimensional interlocking micro-network of resin tags in the dentin tubules with multiple lateral branches that penetrate the intertubular dentin, which positively influenced the adhesion between dentin and the two bond systems.
- 1 June 2002
- Vol. 15 (3) , 177-84
Microtensile bond strength of thermally stressed composite-dentin bonds mediated by one-bottle adhesives.
To evaluate the effects of thermally stressing composite-dentin bonds in teeth subjected to a modified microtensile bond test that allowed application of two bonding agents side-by-side to the same tooth. Extracted human molars with a slot dissecting the occlusal dentin surface were conditioned and primed on one side with Prime & Bond NT (PBNT) and Prime One Mirage (P-One) on the other side. The composite was light-cured onto the surface. Approximately 0.5 mm thick dumbbell-shaped tensile specimens were tested after 24-hour water storage or after thermocycling 2400 times at 5 and 55 degrees C. Interfacial morphologies were evaluated by scanning electron microscopy (SEM). Mean tensile bond strengths (TBS +/- standard deviation) were (36 +/- 24 MPa and 31 +/- 16 MPa) for PBNT, and (51 +/- 25 MPa and 40 +/- 18 MPa) for P-One without and with thermocycling, respectively. 97% of all tested specimens failed adhesively. Differences between the bonding systems and the therrmal treatments were significant (two-way ANOVA, P < 0.05). Regression analysis showed regional correlation between mean TBS of each bonding agent when grouped by the teeth from which they were obtained (r = 0.66, P = 0.002). SEM revealed that both bonding agents effectively wetted the conditioned dentin producing a typical hybrid layer, surface-textured resin tags with multiple lateral branches.
- 1 June 2002
- Vol. 15 (3) , 177-84
Microtensile bond strength of thermally stressed composite-dentin bonds mediated by one-bottle adhesives.
To evaluate the effects of thermally stressing composite-dentin bonds in teeth subjected to a modified microtensile bond test that allowed application of two bonding agents side-by-side to the same tooth. Extracted human molars with a slot dissecting the occlusal dentin surface were conditioned and primed on one side with Prime & Bond NT (PBNT) and Prime One Mirage (P-One) on the other side. The composite was light-cured onto the surface. Approximately 0.5 mm thick dumbbell-shaped tensile specimens were tested after 24-hour water storage or after thermocycling 2400 times at 5 and 55 degrees C. Interfacial morphologies were evaluated by scanning electron microscopy (SEM). Mean tensile bond strengths (TBS +/- standard deviation) were (36 +/- 24 MPa and 31 +/- 16 MPa) for PBNT, and (51 +/- 25 MPa and 40 +/- 18 MPa) for P-One without and with thermocycling, respectively. 97% of all tested specimens failed adhesively. Differences between the bonding systems and the therrmal treatments were significant (two-way ANOVA, P < 0.05). Regression analysis showed regional correlation between mean TBS of each bonding agent when grouped by the teeth from which they were obtained (r = 0.66, P = 0.002). SEM revealed that both bonding agents effectively wetted the conditioned dentin producing a typical hybrid layer, surface-textured resin tags with multiple lateral branches.
- 1 June 2002
- Vol. 15 (3) , 185-92
Relationship of dentin shear bond strengths to different laboratory test designs.
To compare 6 shear bond test procedures using 2 primers by evaluating differences in strength and fracture surfaces. Part I - a 2(3)-factorial design evaluated the effects of (1) 2 primer systems, (2) the dentin moisture level, and (3) the application technique defining the bond area. The outcome of Part I then led to choosing for Part II one primer system, applying the primer the entire surface with moist dentin as the substrate while comparing 6 shear test designs: (1) knife-edged chisel-on-iris; (2) similar to 1 with support added to the tooth; (3) chisel on composite plug; (4) similar to 3 with support added; (5) wire loop on composite plug; (6) modified Watanabe assembly. In Part I mean shear bond strengths (SBS) ranged from 14-36 MPa. SBS was highest for either primer when it was applied to moist dentin over the entire dentin surface. Each of the factors, moisture level, primer system and application technique significantly affected SBS (3-way ANOVA, P<0.05). The effects from each primer system on SBS depended on the surface moisture or the application technique, indicating significant interactions. In Part II, mean SBS ranged from 18-32 MPa with Groups 1 and 2 having significantly higher bond strengths than the others (P<0.05).
- 1 June 2002
- Vol. 15 (3) , 185-92
Relationship of dentin shear bond strengths to different laboratory test designs.
To compare 6 shear bond test procedures using 2 primers by evaluating differences in strength and fracture surfaces. Part I - a 2(3)-factorial design evaluated the effects of (1) 2 primer systems, (2) the dentin moisture level, and (3) the application technique defining the bond area. The outcome of Part I then led to choosing for Part II one primer system, applying the primer the entire surface with moist dentin as the substrate while comparing 6 shear test designs: (1) knife-edged chisel-on-iris; (2) similar to 1 with support added to the tooth; (3) chisel on composite plug; (4) similar to 3 with support added; (5) wire loop on composite plug; (6) modified Watanabe assembly. In Part I mean shear bond strengths (SBS) ranged from 14-36 MPa. SBS was highest for either primer when it was applied to moist dentin over the entire dentin surface. Each of the factors, moisture level, primer system and application technique significantly affected SBS (3-way ANOVA, P<0.05). The effects from each primer system on SBS depended on the surface moisture or the application technique, indicating significant interactions. In Part II, mean SBS ranged from 18-32 MPa with Groups 1 and 2 having significantly higher bond strengths than the others (P<0.05).