Ricardo Walter
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Ricardo Walter has a total of 23 co-authors. Here are the top co-authors by number of shared publications:
- Lee W. Boushell
Department of Operative Dentistry; School of Dentistry; University of North Carolina at Chapel Hill
3 shared publications - Patricia Nobrega Rodrigues Pereira
Center for Dental Biomaterials, Department of Restorative Dental Sciences University of Florida, College of Dentistry Gainesville Florida USA
3 shared publications Yunro Chung
Department of Biostatistics University of North Carolina Gillings School of Global Public Health Chapel Hill NC USA
3 shared publicationsEdward J. Swift
Department of Operative Dentistry University of North Carolina at Chapel Hill Chapel Hill NC USA
2 shared publications- Edward J. Swift
Department of Operative Dentistry, University of North Carolina
2 shared publications Whitley Bartholomew
University of North Carolina School of Dentistry, USA
2 shared publications
Latest Publications
- 1 November 2015
- Published by Wiley in Journal of Dental Education
- Vol. 79 (11) , 1330-1338
Are All Dentiform Teeth with Simulated Caries the Same? A Six-Year Retrospective Study in Preclinical Operative Dentistry
Dentiform teeth with simulated caries (DTSC), frequently used in preclinical courses, should show no variability in the amount of simulated caries from tooth to tooth. However, the level of caries variability among DTSC is currently unknown. The aim of this study was to assess the variation in simulated caries levels in one group of DTSC and determine whether variation among DTSC impacted the preclinical performance of dental students. In the study, 80 commercially available mandibular first molar DTSC with simulated mesio-occluso-distal caries were sectioned in coronal (n=40) and sagittal (n=40) planes where the caries depth/width was greatest. Section images were analyzed for variation in levels of simulated caries using image-processing software. Three years of practical performance data using DTSC were compared with three years of practical performance data using dentiform teeth without simulated caries, for a total of six years (students' performance on two exams, Practical 1 and Practical 2). The results showed that 70% of the coronally sectioned teeth had manufacturing defects that resulted in caries overextension at the dentino-enamel junctions (DEJs). Overextensions were found at the DEJ in 41.3% of the sagittally sectioned teeth. There was a statistically significant decrease in Practical 1 performance of the students who used DTSC as compared with students who used teeth without simulated caries (p=0.0001); there was no statistically significant difference on Practical 2 performance. Of the DTSC evaluated in this study, 56.6% contained manufacturing defects, and more than 80% were found to have excessive caries variation. Prediction of which DTSC will have caries overextension is not possible. Students preparing DTSC that contain caries overextension are therefore at increased risk of receiving undeserved negative summative assessment on practical examinations.
- 1 November 2015
- Published by Wiley in Journal of Dental Education
- Vol. 79 (11) , 1330-1338
Are All Dentiform Teeth with Simulated Caries the Same? A Six-Year Retrospective Study in Preclinical Operative Dentistry
Dentiform teeth with simulated caries (DTSC), frequently used in preclinical courses, should show no variability in the amount of simulated caries from tooth to tooth. However, the level of caries variability among DTSC is currently unknown. The aim of this study was to assess the variation in simulated caries levels in one group of DTSC and determine whether variation among DTSC impacted the preclinical performance of dental students. In the study, 80 commercially available mandibular first molar DTSC with simulated mesio-occluso-distal caries were sectioned in coronal (n=40) and sagittal (n=40) planes where the caries depth/width was greatest. Section images were analyzed for variation in levels of simulated caries using image-processing software. Three years of practical performance data using DTSC were compared with three years of practical performance data using dentiform teeth without simulated caries, for a total of six years (students' performance on two exams, Practical 1 and Practical 2). The results showed that 70% of the coronally sectioned teeth had manufacturing defects that resulted in caries overextension at the dentino-enamel junctions (DEJs). Overextensions were found at the DEJ in 41.3% of the sagittally sectioned teeth. There was a statistically significant decrease in Practical 1 performance of the students who used DTSC as compared with students who used teeth without simulated caries (p=0.0001); there was no statistically significant difference on Practical 2 performance. Of the DTSC evaluated in this study, 56.6% contained manufacturing defects, and more than 80% were found to have excessive caries variation. Prediction of which DTSC will have caries overextension is not possible. Students preparing DTSC that contain caries overextension are therefore at increased risk of receiving undeserved negative summative assessment on practical examinations.
- 18 December 2013
- Published by Wiley in Journal of Esthetic and Restorative Dentistry
- Vol. 26 (3) , 179-190
Three‐Year Clinical Evaluation of a Silorane Composite Resin
Statement of Problem: Composite resins are still outperformed by amalgams in the clinical practice with secondary caries and fractures being their most common failures. A material that suffers less polymerization shrinkage might improve the clinical performance of composite resins.Purpose: To evaluate the clinical performance of a low‐shrink silorane‐based composite resin (Filtek LS Low Shrink Posterior Restorative, 3M ESPE, St. Paul, MN, USA) in comparison with a methacrylate‐based composite resin (Tetric EvoCeram, Ivoclar Vivadent, Schaan, Principality of Liechtenstein) over time.Materials and Methods: Candidates in need of Class II composite resin restorations participated in this randomized controlled clinical trial. Those were 25 female and six male subjects with average age of 44.3 ± 12.7 years. Participants received 82 restorations, being 54 in premolars and 28 in molars. Procedures, which included the restoration of primary caries lesions or replacement of failing restorations, were done using modified preparations with no bevels or additional retention. Restorations were placed using Filtek LS (and dedicated self‐etch adhesive) or Tetric EvoCeram (with AdheSE, Ivoclar Vivadent), following manufacturers' instructions. Incremental placement technique was applied and the restorations were immediately finished. Follow‐up evaluations occurred at six, 12, 24, and 36 months and were done using the Fédération Dentaire Internationale criteria. Statistical analysis was performed using generalized estimating equations.Results: The recall rate at 36 months was 89%. All interaction terms were not significant.Conclusions: Filtek LS performs as well as Tetric EvoCeram performs in the clinical setting at 36 months.Clinical Significance: The silorane‐based composite resin Filtek LS and the conventional methacrylate‐based composite resin Tetric EvoCeram performed similarly well in posterior restorations over at least 36 months of clinical service.
- 18 December 2013
- Published by Wiley in Journal of Esthetic and Restorative Dentistry
- Vol. 26 (3) , 179-190
Three‐Year Clinical Evaluation of a Silorane Composite Resin
Statement of Problem: Composite resins are still outperformed by amalgams in the clinical practice with secondary caries and fractures being their most common failures. A material that suffers less polymerization shrinkage might improve the clinical performance of composite resins.Purpose: To evaluate the clinical performance of a low‐shrink silorane‐based composite resin (Filtek LS Low Shrink Posterior Restorative, 3M ESPE, St. Paul, MN, USA) in comparison with a methacrylate‐based composite resin (Tetric EvoCeram, Ivoclar Vivadent, Schaan, Principality of Liechtenstein) over time.Materials and Methods: Candidates in need of Class II composite resin restorations participated in this randomized controlled clinical trial. Those were 25 female and six male subjects with average age of 44.3 ± 12.7 years. Participants received 82 restorations, being 54 in premolars and 28 in molars. Procedures, which included the restoration of primary caries lesions or replacement of failing restorations, were done using modified preparations with no bevels or additional retention. Restorations were placed using Filtek LS (and dedicated self‐etch adhesive) or Tetric EvoCeram (with AdheSE, Ivoclar Vivadent), following manufacturers' instructions. Incremental placement technique was applied and the restorations were immediately finished. Follow‐up evaluations occurred at six, 12, 24, and 36 months and were done using the Fédération Dentaire Internationale criteria. Statistical analysis was performed using generalized estimating equations.Results: The recall rate at 36 months was 89%. All interaction terms were not significant.Conclusions: Filtek LS performs as well as Tetric EvoCeram performs in the clinical setting at 36 months.Clinical Significance: The silorane‐based composite resin Filtek LS and the conventional methacrylate‐based composite resin Tetric EvoCeram performed similarly well in posterior restorations over at least 36 months of clinical service.
- Open Access
- 1 July 2013
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 24 (4) , 344-348
One-Year Water Sorption and Solubility of All-in-One Adhesives
The aim of this study was to evaluate the water sorption and solubility of different adhesives. Adper Easy Bond, Adper Single Bond Plus, Bond Force, Clearfil SE Bond (bonding resin only), and Xeno IV were the materials evaluated. Ten disks of each adhesive were made in Teflon molds and evaporation of any volatile components was allowed. The disks were weighed daily in an analytical balance until a constant mass was obtained (m1). Disks were then immersed in water for 12 months when their wet weight was recorded (m2). The disks were again weighed daily until a constant mass was obtained and the final weight recorded (m3). Water sorption and solubility (percentages) were calculated using the recorded mass values. Kruskal-Wallis tests were used to compare the average water sorption and solubility among the different adhesives. Mann-Whitney tests with a Bonferroni correction were used to determine the pairwise differences between adhesives in water sorption and solubility. The level of significance was set at 0.05. Water sorption and solubility were significantly different among the groups (p0.05) between Adper Single Bond Plus and Bond Force, or between Clearfil SE Bond and Xeno IV in either water sorption or solubility. Xeno IV did not differ from Adper Easy Bond in water sorption (p>0.05). Water sorption and solubility of all-in-one adhesives increased with time, and the rates of increase were composition-dependent. The results suggest that monomers other than HEMA contribute to water sorption and solubility of adhesive systems from different categories.
- 1 July 2013
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 24 (4) , 344-348
Open AccessOne-Year Water Sorption and Solubility of All-in-One Adhesives
The aim of this study was to evaluate the water sorption and solubility of different adhesives. Adper Easy Bond, Adper Single Bond Plus, Bond Force, Clearfil SE Bond (bonding resin only), and Xeno IV were the materials evaluated. Ten disks of each adhesive were made in Teflon molds and evaporation of any volatile components was allowed. The disks were weighed daily in an analytical balance until a constant mass was obtained (m1). Disks were then immersed in water for 12 months when their wet weight was recorded (m2). The disks were again weighed daily until a constant mass was obtained and the final weight recorded (m3). Water sorption and solubility (percentages) were calculated using the recorded mass values. Kruskal-Wallis tests were used to compare the average water sorption and solubility among the different adhesives. Mann-Whitney tests with a Bonferroni correction were used to determine the pairwise differences between adhesives in water sorption and solubility. The level of significance was set at 0.05. Water sorption and solubility were significantly different among the groups (p0.05) between Adper Single Bond Plus and Bond Force, or between Clearfil SE Bond and Xeno IV in either water sorption or solubility. Xeno IV did not differ from Adper Easy Bond in water sorption (p>0.05). Water sorption and solubility of all-in-one adhesives increased with time, and the rates of increase were composition-dependent. The results suggest that monomers other than HEMA contribute to water sorption and solubility of adhesive systems from different categories.
- 1 July 2012
- Published by Elsevier in Journal of Dentistry
- Vol. 40 (7) , 549-555
Two-year bond strengths of “all-in-one” adhesives to dentine
- 1 July 2012
- Published by Elsevier in Journal of Dentistry
- Vol. 40 (7) , 549-555
Two-year bond strengths of “all-in-one” adhesives to dentine
- 1 April 2011
- Vol. 24 (2) , 93-6
Bond strengths of a silorane composite to various substrates.
To evaluate the shear bond strength (SBS) of a novel low-shrink posterior resin composite (Filtek LS) to various substrates. The dedicated LS System Adhesive was used to bond Filtek LS to bovine dentin, ground bovine enamel, resin-modified glass-ionomer liner (Vitrebond Plus), conventional glass-ionomer restorative material (Fuji IX GP Extra), and bovine dentin previously exposed to zinc oxide-eugenol (IRM) (n=10 for each group). Vitrebond Plus and Fuji IX GP Extra substrates were fabricated by filling standardized preparations that had been made in epoxy resin. Adper Scotchbond SE/Filtek Z250 was used as a control. Composites were applied using the Ultradent specimen former. The bonded specimens were stored in water at 37 degrees C for 24 hours, and SBS testing was done using an Instron universal testing machine. The data were analyzed using ANOVA and Tukey-Kramer HSD test at a significance level of 0.05. The mean SBS values of the Filtek LS system were generally somewhat lower than the values of Adper Scotchbond SE/Filtek Z250 to the various substrates, but the differences were not statistically significant. Exposure of dentin to IRM resulted in a statistically significant reduction in the mean SBS values of Adper Scotchbond SE/Z250 and a slight but statistically insignificant reduction for the Filtek LS system.
- 1 April 2011
- Vol. 24 (2) , 93-6
Bond strengths of a silorane composite to various substrates.
To evaluate the shear bond strength (SBS) of a novel low-shrink posterior resin composite (Filtek LS) to various substrates. The dedicated LS System Adhesive was used to bond Filtek LS to bovine dentin, ground bovine enamel, resin-modified glass-ionomer liner (Vitrebond Plus), conventional glass-ionomer restorative material (Fuji IX GP Extra), and bovine dentin previously exposed to zinc oxide-eugenol (IRM) (n=10 for each group). Vitrebond Plus and Fuji IX GP Extra substrates were fabricated by filling standardized preparations that had been made in epoxy resin. Adper Scotchbond SE/Filtek Z250 was used as a control. Composites were applied using the Ultradent specimen former. The bonded specimens were stored in water at 37 degrees C for 24 hours, and SBS testing was done using an Instron universal testing machine. The data were analyzed using ANOVA and Tukey-Kramer HSD test at a significance level of 0.05. The mean SBS values of the Filtek LS system were generally somewhat lower than the values of Adper Scotchbond SE/Filtek Z250 to the various substrates, but the differences were not statistically significant. Exposure of dentin to IRM resulted in a statistically significant reduction in the mean SBS values of Adper Scotchbond SE/Z250 and a slight but statistically insignificant reduction for the Filtek LS system.
- 1 January 2003
- Vol. 5 (2) , 107-12
Effect of acid-etching on the enamel bond of two self-etching systems.
To evaluate enamel bond strengths of self-etching primer systems with and without the use of phosphoric acid etching. The enamel of sixteen bovine incisors was ground with wet 600-grit SiC paper, and specimens were divided into seven groups. Group SE and group ABF were bonded with Clearfil SE Bond (Kuraray) and an experimental self-etching primer system ABF (Kuraray) in accordance with the manufacturer's instructions. The enamel of groups SE+AC and ABF+AC was acid-etched (AC) prior to application of the primers. The enamel of groups AC+SE-P and AC+ABF-P was acid-etched and the bonding resin was applied without primer. All of these groups were restored with Clearfil AP-X (Kuraray). For the control group (SB), enamel was etched and bonded with Single Bond (3M) according to manufacturer's instructions and restored with Z-250 (3M). After 24 h of water storage, the teeth were sectioned into 0.7-mm-thick slabs, trimmed for microtensile bond testing and subjected to tensile forces at a cross-head speed of 1 mm/min. After testing, all samples were analyzed with SEM. Data were evaluated by one-way ANOVA and Fisher's PLSD (alpha = 0.05). Acid etching prior to application of the self-etching primer produced higher bond strengths to enamel than self-etching priming only. Omission of the primer step provided bond strengths similar to the other acid-etched groups. SEM analysis revealed that when the acid was applied prior to the self-etching primers, an increase in failure within enamel occurred. Since high bond strength to enamel is critical for good margins and seal of the restorations, applying the etching step should be considered in case of restorations that rely mainly on enamel bonding.
- 1 January 2003
- Vol. 5 (2) , 107-12
Effect of acid-etching on the enamel bond of two self-etching systems.
To evaluate enamel bond strengths of self-etching primer systems with and without the use of phosphoric acid etching. The enamel of sixteen bovine incisors was ground with wet 600-grit SiC paper, and specimens were divided into seven groups. Group SE and group ABF were bonded with Clearfil SE Bond (Kuraray) and an experimental self-etching primer system ABF (Kuraray) in accordance with the manufacturer's instructions. The enamel of groups SE+AC and ABF+AC was acid-etched (AC) prior to application of the primers. The enamel of groups AC+SE-P and AC+ABF-P was acid-etched and the bonding resin was applied without primer. All of these groups were restored with Clearfil AP-X (Kuraray). For the control group (SB), enamel was etched and bonded with Single Bond (3M) according to manufacturer's instructions and restored with Z-250 (3M). After 24 h of water storage, the teeth were sectioned into 0.7-mm-thick slabs, trimmed for microtensile bond testing and subjected to tensile forces at a cross-head speed of 1 mm/min. After testing, all samples were analyzed with SEM. Data were evaluated by one-way ANOVA and Fisher's PLSD (alpha = 0.05). Acid etching prior to application of the self-etching primer produced higher bond strengths to enamel than self-etching priming only. Omission of the primer step provided bond strengths similar to the other acid-etched groups. SEM analysis revealed that when the acid was applied prior to the self-etching primers, an increase in failure within enamel occurred. Since high bond strength to enamel is critical for good margins and seal of the restorations, applying the etching step should be considered in case of restorations that rely mainly on enamel bonding.