Yumei Yue
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yumei Yue has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
- Shude Ji
College of Aerospace Engineering, Shenyang Aerospace University, Shenyang 110136, China
2 shared publications - Baolei Cui
School of Mechanical and Electrical Engineering, Shenyang Aerospace University, Shenyang 110136, China
1 shared publication - Jingwei Xing
Faculty of Aerospace Engineering, Shenyang Aerospace University, Shenyang 110136, China
1 shared publication Kang Yang
College of Aerospace Engineering, Shenyang Aerospace University, Shenyang, 110136, China
1 shared publicationLan Zhang
1 shared publicationLiguo Zhang
Faculty of Aerospace Engineering, Shenyang Aerospace University, Shenyang, People’s Republic of China
1 shared publication
Latest Publications
- Open Access
The Influence of Al Addition on Cracks, Microstructure and Properties of Laser Deposition Manufacturing TiAl Alloys
Aluminum volatilization during laser deposition manufacturing severely deteriorates the microstructure and service performance of TiAl alloys, causing aggravated brittleness, elevated crack sensitivity and structural degradation. To tackle this issue, this work proposes an aluminum composition compensation strategy based on Ti-48Al-2Cr-2Nb pre-alloyed powder, with three mass fractions of elemental Al (15 wt.%, 20 wt.% and 25 wt.%) added to systematically investigate their influences on the macroscopic cracking behavior, microstructure evolution, phase constitution and mechanical properties of the deposited alloys. The results demonstrate that 15 wt.% Al addition achieves crack-free laser deposition, yielding a uniform microstructure dominated by γ-TiAl phase with dispersedly distributed TiAl2 and minor B2 phases as well as low residual internal stress. No α2-Ti3Al phase is detected in all samples, as the Al-rich composition shift thermodynamically suppresses the stability of Ti-rich α2 phase. Excessive Al addition induces the massive formation of brittle Al-rich intermetallics (TiAl2 and TiAl3), which gradually evolve from isolated particles to a continuous network structure, leading to a sharp increase in crack susceptibility. Al addition continuously improves the microhardness of the alloys, and the 25 wt.% Al sample attains the maximum hardness of 522.3 HV, benefiting from the synergistic effects of grain refinement strengthening and second-phase strengthening. The 15 wt.% Al sample delivers the optimal comprehensive mechanical performance, with an ultimate tensile strength of 550.2 Mpa and a fracture elongation of 0.76%, where the finely dispersed TiAl2 precipitates exert a remarkable dispersion strengthening effect without causing severe embrittlement. This work provides a feasible experimental basis and technical reference for crack control and property optimization of laser deposition-manufactured TiAl alloys.
Open AccessThe Influence of Al Addition on Cracks, Microstructure and Properties of Laser Deposition Manufacturing TiAl Alloys
Aluminum volatilization during laser deposition manufacturing severely deteriorates the microstructure and service performance of TiAl alloys, causing aggravated brittleness, elevated crack sensitivity and structural degradation. To tackle this issue, this work proposes an aluminum composition compensation strategy based on Ti-48Al-2Cr-2Nb pre-alloyed powder, with three mass fractions of elemental Al (15 wt.%, 20 wt.% and 25 wt.%) added to systematically investigate their influences on the macroscopic cracking behavior, microstructure evolution, phase constitution and mechanical properties of the deposited alloys. The results demonstrate that 15 wt.% Al addition achieves crack-free laser deposition, yielding a uniform microstructure dominated by γ-TiAl phase with dispersedly distributed TiAl2 and minor B2 phases as well as low residual internal stress. No α2-Ti3Al phase is detected in all samples, as the Al-rich composition shift thermodynamically suppresses the stability of Ti-rich α2 phase. Excessive Al addition induces the massive formation of brittle Al-rich intermetallics (TiAl2 and TiAl3), which gradually evolve from isolated particles to a continuous network structure, leading to a sharp increase in crack susceptibility. Al addition continuously improves the microhardness of the alloys, and the 25 wt.% Al sample attains the maximum hardness of 522.3 HV, benefiting from the synergistic effects of grain refinement strengthening and second-phase strengthening. The 15 wt.% Al sample delivers the optimal comprehensive mechanical performance, with an ultimate tensile strength of 550.2 Mpa and a fracture elongation of 0.76%, where the finely dispersed TiAl2 precipitates exert a remarkable dispersion strengthening effect without causing severe embrittlement. This work provides a feasible experimental basis and technical reference for crack control and property optimization of laser deposition-manufactured TiAl alloys.
- Open Access
- 1 January 2026
- Published by Tech Science Press in Journal of Polymer Materials
- Vol. 43 (1) , 1-10
The Influence of Temperature Environment and Polymeric Binder Proportion on the Static/Dynamic Mechanical Properties of Polymer Materials
To comprehensively explore the impact of binder content on the mechanical properties of the Polymer bonded explosive (PBX) substitute material (Polymer-bonded Analogue Explosive (PAE)—it is renowned for its outstanding high-temperature resistance, exceptional mechanical properties, excellent chemical stability, and superior electrical insulation), a series of experiments are meticulously carried out. The dynamic and static mechanical properties, along with the microstructure of PAE, are precisely measured through the Split Hopkinson Pressure Bar (SHPB) test, static compression tests, and Scanning Electron Microscopy (SEM). The dynamic performance test outcomes clearly indicate that both the binder content (2%, 4%, 6%) and temperature (25°C, 45°C, 70°C) exert a substantial influence on the dynamic mechanical properties of PAE. Specifically, as the binder content increases, the elastic modulus increases, demonstrating higher stiffness, and the longer failure duration represents a prolonged fracture process rather than an improved deformation strain to failure. This means the strength-related stiffness rises with binder content, but the overall ductility does not increase. Notably, PAE with 2% the Ethylene-Vinyl Acetate Copolymer (EVA)—it bonds well with a variety of materials, such as metal, wood, and plastic—exhibits distinct plastic deformation behavior, while PAE samples with 4% and 6% EVA display evident brittle fracture characteristics. Additionally, the mechanical properties of PAE are highly sensitive to temperature variations. Among the tested temperatures, PAE showcases the most favorable performance at 45°C. The static performance test results reveal that an increment in binder content effectively helps to reduce the temperature sensitivity of temperature (−40°C, 25°C, 50°C, 70°C) on PAE and enhance its static mechanical properties. The maximum compressive strength gradually diminishes as the temperature rises. However, it should be noted that an excessively high binder content will undermine the mechanical properties of PAE. With the increase in binder content, the compressive modulus demonstrates relatively stable changes under both low-temperature and high-temperature conditions. The SEM analysis results demonstrate that, aside from the initial defects inherent in the material preparation process, the components of PAE are firmly combined. Throughout the tests, no new pores or microcracks emerge, which strongly indicates that the mechanical properties of PAE remain stable.
- 1 January 2026
- Published by Tech Science Press in Journal of Polymer Materials
- Vol. 43 (1) , 1-10
Open AccessThe Influence of Temperature Environment and Polymeric Binder Proportion on the Static/Dynamic Mechanical Properties of Polymer Materials
To comprehensively explore the impact of binder content on the mechanical properties of the Polymer bonded explosive (PBX) substitute material (Polymer-bonded Analogue Explosive (PAE)—it is renowned for its outstanding high-temperature resistance, exceptional mechanical properties, excellent chemical stability, and superior electrical insulation), a series of experiments are meticulously carried out. The dynamic and static mechanical properties, along with the microstructure of PAE, are precisely measured through the Split Hopkinson Pressure Bar (SHPB) test, static compression tests, and Scanning Electron Microscopy (SEM). The dynamic performance test outcomes clearly indicate that both the binder content (2%, 4%, 6%) and temperature (25°C, 45°C, 70°C) exert a substantial influence on the dynamic mechanical properties of PAE. Specifically, as the binder content increases, the elastic modulus increases, demonstrating higher stiffness, and the longer failure duration represents a prolonged fracture process rather than an improved deformation strain to failure. This means the strength-related stiffness rises with binder content, but the overall ductility does not increase. Notably, PAE with 2% the Ethylene-Vinyl Acetate Copolymer (EVA)—it bonds well with a variety of materials, such as metal, wood, and plastic—exhibits distinct plastic deformation behavior, while PAE samples with 4% and 6% EVA display evident brittle fracture characteristics. Additionally, the mechanical properties of PAE are highly sensitive to temperature variations. Among the tested temperatures, PAE showcases the most favorable performance at 45°C. The static performance test results reveal that an increment in binder content effectively helps to reduce the temperature sensitivity of temperature (−40°C, 25°C, 50°C, 70°C) on PAE and enhance its static mechanical properties. The maximum compressive strength gradually diminishes as the temperature rises. However, it should be noted that an excessively high binder content will undermine the mechanical properties of PAE. With the increase in binder content, the compressive modulus demonstrates relatively stable changes under both low-temperature and high-temperature conditions. The SEM analysis results demonstrate that, aside from the initial defects inherent in the material preparation process, the components of PAE are firmly combined. Throughout the tests, no new pores or microcracks emerge, which strongly indicates that the mechanical properties of PAE remain stable.
- 27 May 2017
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 71 (1) , 139-145
Refill Friction Stir Spot Welding of 2198-T8 Aluminum Alloy
- 27 May 2017
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 71 (1) , 139-145
Refill Friction Stir Spot Welding of 2198-T8 Aluminum Alloy
- Open Access
Design of Friction Stir Welding Tool for Avoiding Root Flaws
In order to improve material flow behavior during friction stir welding and avoid root flaws of weld, a tool with a half-screw pin and a tool with a tapered-flute pin are suggested. The effect of flute geometry in tool pins on material flow velocity is investigated by the software ANSYS FLUENT. Numerical simulation results show that high material flow velocity appears near the rotational tool and material flow velocity rapidly decreases with the increase of distance away from the axis of the tool. Maximum material flow velocity by the tool with the tapered-flute pin appears at the beginning position of flute and the velocity decreases with the increase of flow length in flute. From the view of increasing the flow velocity of material near the bottom of the workpiece or in the middle of workpiece, the tool with the half-screw pin and the tool with the tapered-flute pin are both better than the conventional tool.
Open AccessDesign of Friction Stir Welding Tool for Avoiding Root Flaws
In order to improve material flow behavior during friction stir welding and avoid root flaws of weld, a tool with a half-screw pin and a tool with a tapered-flute pin are suggested. The effect of flute geometry in tool pins on material flow velocity is investigated by the software ANSYS FLUENT. Numerical simulation results show that high material flow velocity appears near the rotational tool and material flow velocity rapidly decreases with the increase of distance away from the axis of the tool. Maximum material flow velocity by the tool with the tapered-flute pin appears at the beginning position of flute and the velocity decreases with the increase of flow length in flute. From the view of increasing the flow velocity of material near the bottom of the workpiece or in the middle of workpiece, the tool with the half-screw pin and the tool with the tapered-flute pin are both better than the conventional tool.
- 31 January 2012
- Published by Elsevier in Scripta Materialia
- Vol. 66 (2) , 81-84
Stress-induced growth of well-aligned Cu2O nanowire arrays and their photovoltaic effect
- 31 January 2012
- Published by Elsevier in Scripta Materialia
- Vol. 66 (2) , 81-84
Stress-induced growth of well-aligned Cu2O nanowire arrays and their photovoltaic effect