J. R. White
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
J. R. White has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
A. F. Abdelkader
School of Chemical Engineering and Advanced Materials, University of Newcastle upon Tyne, Herschel Building, Newcastle upon Tyne, NE1 7RU, United Kingdom
3 shared publicationsI.H. Craig
School of Chemical Engineering and Advanced Materials, Herschel Building, University of Newcastle upon Tyne, Newcastle upon Tyne NE1 7RU, UK
2 shared publicationsJ. M. Hale
University of Newcastle upon Tyne
2 shared publicationsR. Stephenson
University of Newcastle upon Tyne
2 shared publicationsA.V. Shyichuk
Faculty of Chemical Technology and Engineering, University of Technology and Agriculture, Seminaryjna 3, 85‐326 Bydgoszcz, Poland
1 shared publicationB. de Poumeyrol
1 shared publication
Latest Publications
- 30 November 2009
- Published by Elsevier in Polymer Degradation and Stability
- Vol. 94 (11) , 1999-2003
Photogeneration of carbon dioxide from polypropylene film stabilized by hindered amines
- 30 November 2009
- Published by Elsevier in Polymer Degradation and Stability
- Vol. 94 (11) , 1999-2003
Photogeneration of carbon dioxide from polypropylene film stabilized by hindered amines
- 21 July 2006
- Published by Wiley in Polymer Engineering & Science
- Vol. 46 (9) , 1160-1172
Dynamic nanoindentation of some polyolefins
Nanoindentation tests have been conducted on five different polyolefins, comprising a high density polyethylene, a low density polyethylene, a linear low density polyethylene, a polypropylene homopolymer and a polypropylene copolymer. The nanoindenter was fitted with a “Dynamic Stiffness Measurement” (DSM) facility that permits measurement of storage modulus and loss modulus at frequent intervals during an indentation test. The results were quite scattered, especially those for the loss modulus, and methods of processing the data to derive meaningful results were examined and are discussed. The storage modulus measurements were found to give the same stiffness ranking as the monotonic load‐displacement data when comparing indentations on the same material. Some correlation was found between the storage modulus and fractional crystallinity. An averaging procedure was developed for the loss modulus values that appeared to give a consistent assessment of the dissipation properties of the different materials. Analysis of the monotonic component of the load‐displacement data indicated that the nature of the deformation changed from mainly elastic/viscoelastic to mainly viscoelastic/plastic during the course of the indentation tests. POLYM. ENG. SCI. 46:1160–1172, 2006. © 2006 Society of Plastics Engineers
- 21 July 2006
- Published by Wiley in Polymer Engineering & Science
- Vol. 46 (9) , 1160-1172
Dynamic nanoindentation of some polyolefins
Nanoindentation tests have been conducted on five different polyolefins, comprising a high density polyethylene, a low density polyethylene, a linear low density polyethylene, a polypropylene homopolymer and a polypropylene copolymer. The nanoindenter was fitted with a “Dynamic Stiffness Measurement” (DSM) facility that permits measurement of storage modulus and loss modulus at frequent intervals during an indentation test. The results were quite scattered, especially those for the loss modulus, and methods of processing the data to derive meaningful results were examined and are discussed. The storage modulus measurements were found to give the same stiffness ranking as the monotonic load‐displacement data when comparing indentations on the same material. Some correlation was found between the storage modulus and fractional crystallinity. An averaging procedure was developed for the loss modulus values that appeared to give a consistent assessment of the dissipation properties of the different materials. Analysis of the monotonic component of the load‐displacement data indicated that the nature of the deformation changed from mainly elastic/viscoelastic to mainly viscoelastic/plastic during the course of the indentation tests. POLYM. ENG. SCI. 46:1160–1172, 2006. © 2006 Society of Plastics Engineers
- 1 February 2006
- Published by Springer Nature in Journal of Materials Science
- Vol. 41 (3) , 993-1006
Mechanical properties of photo-degraded recycled photo-degraded polyolefins
- 1 February 2006
- Published by Springer Nature in Journal of Materials Science
- Vol. 41 (3) , 993-1006
Mechanical properties of photo-degraded recycled photo-degraded polyolefins
- 29 September 2005
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 98 (6) , 2544-2549
Water absorption in epoxy resins: The effects of the crosslinking agent and curing temperature
Epoxy systems were prepared with the same epoxide (diglycidyl ether of bisphenol A) with five different hardeners: 4,4′‐diaminodiphenylmethane (H1), diethylenetriamine (H2), a cycloaliphatic amine based on isophorone diamine (H3), a polyaminoimidazoline‐based hardener (H4), and a polyamidoamine‐based adduct hardener (H5). Samples were subjected to four different postcure treatment temperatures (23, 55, 75, and 150°C). Water absorption kinetics were obtained for each material and for each postcure treatment. The water absorption behaviors for the materials with H1, H2, and H3 were similar, whereas those for H4 and H5 were quite different. This is discussed in terms of the molecular structures of the hardeners. © 2005 Wiley Periodicals, Inc. J Appl Polym Sci 98: 2544–2549, 2005
- 29 September 2005
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 98 (6) , 2544-2549
Water absorption in epoxy resins: The effects of the crosslinking agent and curing temperature
Epoxy systems were prepared with the same epoxide (diglycidyl ether of bisphenol A) with five different hardeners: 4,4′‐diaminodiphenylmethane (H1), diethylenetriamine (H2), a cycloaliphatic amine based on isophorone diamine (H3), a polyaminoimidazoline‐based hardener (H4), and a polyamidoamine‐based adduct hardener (H5). Samples were subjected to four different postcure treatment temperatures (23, 55, 75, and 150°C). Water absorption kinetics were obtained for each material and for each postcure treatment. The water absorption behaviors for the materials with H1, H2, and H3 were similar, whereas those for H4 and H5 were quite different. This is discussed in terms of the molecular structures of the hardeners. © 2005 Wiley Periodicals, Inc. J Appl Polym Sci 98: 2544–2549, 2005
- 1 April 2005
- Published by Springer Nature in Journal of Materials Science
- Vol. 40 (8) , 1843-1854
Curing characteristics and internal stresses in epoxy coatings: Effect of crosslinking agent
- 1 April 2005
- Published by Springer Nature in Journal of Materials Science
- Vol. 40 (8) , 1843-1854
Curing characteristics and internal stresses in epoxy coatings: Effect of crosslinking agent
- 24 February 2005
- Published by Wiley in Polymer Engineering & Science
- Vol. 45 (4) , 588-595
Crystallization and chemi‐crystallization of recycled photodegraded polyethylenes
Test bars (3 mm thick) made from a high‐density polyethylene (HDPE), a low‐density polyethylene (LDPE), and a linear low‐density polyethylene (LLDPE) were injection‐molded from virgin polymer and from blends containing recycled photodegraded polymer of the same kind. The molded bars were then subjected to ultraviolet (UV) exposure. Crystallinity measurements were made at different depths from the exposed surface using differential scanning calorimetry. The effects caused by processing and photodegradation were separated by comparing thermograms obtained in the initial DSC run and in a reheating run, respectively. Chemi‐crystallization was produced by UV exposure. The results are interpreted in terms of molecular scission and photo‐initiated molecular defects. Scission accounts for the observed chemi‐crystallization, whereas the molecular defects inhibit crystallization and eventually limit chemi‐crystallization. After remelting, crystallization of the photodegraded materials is influenced both by the molecular mass distribution and by the defect content of the material. The changes in crystallization behavior caused by photodegradation are different for the three polyethylenes. The results obtained using blends that included photodegraded recyclate were consistent with this material acting as a pro‐degradent. The recyclability of the materials is discussed. POLYM. ENG. SCI., 45:588–595, 2005. © 2005 Society of Plastics Engineers
- 24 February 2005
- Published by Wiley in Polymer Engineering & Science
- Vol. 45 (4) , 588-595
Crystallization and chemi‐crystallization of recycled photodegraded polyethylenes
Test bars (3 mm thick) made from a high‐density polyethylene (HDPE), a low‐density polyethylene (LDPE), and a linear low‐density polyethylene (LLDPE) were injection‐molded from virgin polymer and from blends containing recycled photodegraded polymer of the same kind. The molded bars were then subjected to ultraviolet (UV) exposure. Crystallinity measurements were made at different depths from the exposed surface using differential scanning calorimetry. The effects caused by processing and photodegradation were separated by comparing thermograms obtained in the initial DSC run and in a reheating run, respectively. Chemi‐crystallization was produced by UV exposure. The results are interpreted in terms of molecular scission and photo‐initiated molecular defects. Scission accounts for the observed chemi‐crystallization, whereas the molecular defects inhibit crystallization and eventually limit chemi‐crystallization. After remelting, crystallization of the photodegraded materials is influenced both by the molecular mass distribution and by the defect content of the material. The changes in crystallization behavior caused by photodegradation are different for the three polyethylenes. The results obtained using blends that included photodegraded recyclate were consistent with this material acting as a pro‐degradent. The recyclability of the materials is discussed. POLYM. ENG. SCI., 45:588–595, 2005. © 2005 Society of Plastics Engineers
- 24 February 2005
- Published by Wiley in Polymer Engineering & Science
- Vol. 45 (4) , 579-587
Photo‐induced scission and crosslinking in LDPE, LLDPE, and HDPE
The molecular degradation characteristics of three different polyethylenes were determined by deriving chain scission and crosslinking concentrations from gel permeation chromatography molecular weight distributions obtained after 3 weeks and 6 weeks laboratory ultraviolet exposure. Injection‐molded bars (3 mm thick) made from a low‐density polyethylene (LDPE), a linear low‐density polyethylene (LLDPE), and a high‐density polyethylene (HDPE) were used and all showed strong depth variations in degradation. Degradation was rapid near the exposed surfaces but very little change occurred in the bar centers, due to oxygen starvation. The most rapid rises in scission and crosslink concentrations were observed with LDPE, for which the concentrations after 6 weeks exposure were approximately double those measured after 3 weeks. With LLDPE and HDPE the scission and crosslink concentrations after 6 weeks exposure were very much greater than twice those after 3 weeks. Scission dominated over crosslinking at all depths and for all materials the scission/crosslink ratio was always ≥3, with a value of ∼9 recorded for HDPE near the exposed surface after 6 weeks exposure. POLYM. ENG. SCI., 45:579–587, 2005. © 2005 Society of Plastics Engineers
- 24 February 2005
- Published by Wiley in Polymer Engineering & Science
- Vol. 45 (4) , 579-587
Photo‐induced scission and crosslinking in LDPE, LLDPE, and HDPE
The molecular degradation characteristics of three different polyethylenes were determined by deriving chain scission and crosslinking concentrations from gel permeation chromatography molecular weight distributions obtained after 3 weeks and 6 weeks laboratory ultraviolet exposure. Injection‐molded bars (3 mm thick) made from a low‐density polyethylene (LDPE), a linear low‐density polyethylene (LLDPE), and a high‐density polyethylene (HDPE) were used and all showed strong depth variations in degradation. Degradation was rapid near the exposed surfaces but very little change occurred in the bar centers, due to oxygen starvation. The most rapid rises in scission and crosslink concentrations were observed with LDPE, for which the concentrations after 6 weeks exposure were approximately double those measured after 3 weeks. With LLDPE and HDPE the scission and crosslink concentrations after 6 weeks exposure were very much greater than twice those after 3 weeks. Scission dominated over crosslinking at all depths and for all materials the scission/crosslink ratio was always ≥3, with a value of ∼9 recorded for HDPE near the exposed surface after 6 weeks exposure. POLYM. ENG. SCI., 45:579–587, 2005. © 2005 Society of Plastics Engineers
- 1 October 2004
- Published by Springer Nature in Journal of Materials Science
- Vol. 39 (19) , 6079-6081
Effect of exposure of piezoelectric paint to water and salt solution
- 1 October 2004
- Published by Springer Nature in Journal of Materials Science
- Vol. 39 (19) , 6079-6081
Effect of exposure of piezoelectric paint to water and salt solution
- 1 May 2004
- Published by Springer Nature in Journal of Materials Science
- Vol. 39 (9) , 3105-3114
Piezoelectric paint: Ceramic-polymer composites for vibration sensors
- 1 May 2004
- Published by Springer Nature in Journal of Materials Science
- Vol. 39 (9) , 3105-3114
Piezoelectric paint: Ceramic-polymer composites for vibration sensors
- 1 November 2002
- Published by Springer Nature in Journal of Materials Science
- Vol. 37 (22) , 4769-4773
Influence of relative humidity on the development of internal stresses in epoxy resin based coatings
- 1 November 2002
- Published by Springer Nature in Journal of Materials Science
- Vol. 37 (22) , 4769-4773
Influence of relative humidity on the development of internal stresses in epoxy resin based coatings