A. S. Aloy
A. S. Aloy has a total of 28 co-authors. Here are the top co-authors by number of shared publications:
- A. Kosilov
International Atomic Energy Agency (IAEA) Wagramerstrasse 5 P.O. Box 200 A-1400 Vienna Austria
1 shared publication A. N. Vizniy
Khlopin Radium Institute, 2-i Murinskii pr. 28, St. Petersburg, Russia
1 shared publicationA. V. Trofimenko
Federal State Unitary Enterprise
1 shared publication- Carol M. Jantzen
Savannah River National Laboratory Savannah River Nuclear Solutions Aiken South Carolina
1 shared publication - D. Bacon
Pacific Northwest National Laboratory PO Box 999 Richland, WA 99352 USA
1 shared publication D. N. Shishkin
Khlopin Radium Institute, 2-i Murinskii pr. 28, St. Petersburg, Russia
1 shared publication
Latest Publications
- 1 December 2024
- Published by Pleiades Publishing Ltd in Radiochemistry
- Vol. 66 (6) , 852-857
Solidification of the Strip Solution with Cesium-137 Using Porous Inorganic Material “Gubka”
At the Khlopin Radium Institute, during the development of extractive partitioning of the liquid high-level radioactive waste (HLW), a strip solution containing up to 6.0 × 1011 Bq/dm3 (16.3 Ci/dm3) of 137Cs in the form of a nitric acid solution was collected and temporary was stored. To solidify this solution, a batch process using Gubka (sponge) porous inorganic material (PIM) was developed and implemented. Since that time, about 18 dm3 of HLW was solidified into 12 sets of Gubka, reducing the liquid HLW volume by a factor of about 50. Gubka sets were placed into special containers, which after sealing by welding were delivered to the long-time storage of the RosRAO Branch in Sosnovy Bor.
- 1 December 2024
- Published by Pleiades Publishing Ltd in Radiochemistry
- Vol. 66 (6) , 852-857
Solidification of the Strip Solution with Cesium-137 Using Porous Inorganic Material “Gubka”
At the Khlopin Radium Institute, during the development of extractive partitioning of the liquid high-level radioactive waste (HLW), a strip solution containing up to 6.0 × 1011 Bq/dm3 (16.3 Ci/dm3) of 137Cs in the form of a nitric acid solution was collected and temporary was stored. To solidify this solution, a batch process using Gubka (sponge) porous inorganic material (PIM) was developed and implemented. Since that time, about 18 dm3 of HLW was solidified into 12 sets of Gubka, reducing the liquid HLW volume by a factor of about 50. Gubka sets were placed into special containers, which after sealing by welding were delivered to the long-time storage of the RosRAO Branch in Sosnovy Bor.
- 1 September 2015
- Published by Pleiades Publishing Ltd in Radiochemistry
- Vol. 57 (5) , 546-551
Leaching of borosilicate glasses containing simulated high-level waste from the experimental and demonstration center of the mining and chemical combine in mineralized water of a granitoid formation
Leaching of borosilicate glass samples containing 10, 15, and 20 wt % simulated high-level waste (HLW) at 20 and 90°C in mineralized water simulating the composition of underground waters on the site
- 1 September 2015
- Published by Pleiades Publishing Ltd in Radiochemistry
- Vol. 57 (5) , 546-551
Leaching of borosilicate glasses containing simulated high-level waste from the experimental and demonstration center of the mining and chemical combine in mineralized water of a granitoid formation
Leaching of borosilicate glass samples containing 10, 15, and 20 wt % simulated high-level waste (HLW) at 20 and 90°C in mineralized water simulating the composition of underground waters on the site
- 1 November 2014
- Published by Pleiades Publishing Ltd in Radiochemistry
- Vol. 56 (6) , 633-638
Leaching of borosilicate glasses containing simulated high-level waste in solutions of hydrogen peroxide as a substance simulating radiolysis products
Experiments on leaching of borosilicate glass samples containing 10, 15, and 20 wt % simulated high-level waste (HLW) were performed at 20 and 90°C in hydrogen peroxide solutions. H2O2 was used as a substance simulating products of underground water radiolysis. The leach rates and diffusion coefficients of the glass components were determined. The character and extent of the effect of the varied experimental parameters on the characteristics being determined were evaluated by correlation analysis. The presence of hydrogen peroxide in the contact solution enhances the chemical durability of borosilicate glasses.
- 1 November 2014
- Published by Pleiades Publishing Ltd in Radiochemistry
- Vol. 56 (6) , 633-638
Leaching of borosilicate glasses containing simulated high-level waste in solutions of hydrogen peroxide as a substance simulating radiolysis products
Experiments on leaching of borosilicate glass samples containing 10, 15, and 20 wt % simulated high-level waste (HLW) were performed at 20 and 90°C in hydrogen peroxide solutions. H2O2 was used as a substance simulating products of underground water radiolysis. The leach rates and diffusion coefficients of the glass components were determined. The character and extent of the effect of the varied experimental parameters on the characteristics being determined were evaluated by correlation analysis. The presence of hydrogen peroxide in the contact solution enhances the chemical durability of borosilicate glasses.
- 1 May 2012
- Published by Pleiades Publishing Ltd in Radiochemistry
- Vol. 54 (3) , 291-297
Formation of surface layers in leaching of borosilicate glasses incorporating different amounts of simulated HLW
Borosilicate glass specimens incorporating 10, 15, and 20 wt % simulated high-level waste (HLW) were leached at 20, 90, and 120°C in deionized water following the procedure accepted in Russia, GOST (State Standard) R 52 126-2003. At 90°C, the altered surface layer is formed already from the first days of leaching. The main interaction in the system occurs at the phase boundary between the altered surface layer and water, rather than at the phase boundary between the glass and water through the porous surface layer as it is commonly believed. The altered surface layer acts as a natural barrier preventing transfer of simulated waste components to the liquid phase. The barrier properties of the altered surface layer are manifested to the greatest extent at 20 wt % content of simulated HLW in the initial glass and leaching temperature of 120°C.
- 1 May 2012
- Published by Pleiades Publishing Ltd in Radiochemistry
- Vol. 54 (3) , 291-297
Formation of surface layers in leaching of borosilicate glasses incorporating different amounts of simulated HLW
Borosilicate glass specimens incorporating 10, 15, and 20 wt % simulated high-level waste (HLW) were leached at 20, 90, and 120°C in deionized water following the procedure accepted in Russia, GOST (State Standard) R 52 126-2003. At 90°C, the altered surface layer is formed already from the first days of leaching. The main interaction in the system occurs at the phase boundary between the altered surface layer and water, rather than at the phase boundary between the glass and water through the porous surface layer as it is commonly believed. The altered surface layer acts as a natural barrier preventing transfer of simulated waste components to the liquid phase. The barrier properties of the altered surface layer are manifested to the greatest extent at 20 wt % content of simulated HLW in the initial glass and leaching temperature of 120°C.
- 1 January 2011
- Published by Elsevier
Contributor contact details