S. P. Nikanorov
Research Subjects
S. P. Nikanorov has a total of 28 co-authors. Here are the top co-authors by number of shared publications:
V. N. Osipov
Ioffe Institute, 194021, St. Petersburg, Russia
9 shared publicationsB. N. Korchunov
Russian Academy of Sciences
7 shared publicationsB. K. Kardashev
Russian Academy of Sciences
5 shared publications- Andrei V. Chikiryaka
Ioffe Institute, St. Petersburg, Russia
2 shared publications L. I. Derkachenko
Russian Academy of Sciences
2 shared publicationsL. M. Egorova
Russian Academy of Sciences
2 shared publications
Latest Publications
- 1 January 2023
- Published by Ioffe Institute Russian Academy of Sciences in Technical Physics
- Vol. 68 (4) , 517
Influence of the rate of directional crystallization and silicon content on the structure and strength of the Al-Si-Cu alloy
Influence of the rate of directional crystallization and silicon content on the structure and strength of the Al-Si-Cu alloy
- 1 January 2023
- Published by Ioffe Institute Russian Academy of Sciences in Technical Physics
- Vol. 68 (4) , 517
Influence of the rate of directional crystallization and silicon content on the structure and strength of the Al-Si-Cu alloy
Influence of the rate of directional crystallization and silicon content on the structure and strength of the Al-Si-Cu alloy
- 1 January 2023
- Published by Ioffe Institute Russian Academy of Sciences in Журнал технической физики
- Vol. 93 (4) , 554
Влияние скорости направленной кристаллизации и содержания кремния на структуру и прочность Al-Si-Cu-сплава
The structure and strength of Al−xSi−2wt.%Cu (x = 15, 17 and 20wt.%) alloys obtained by directional solidification at a rate of 0.1 and 0.8mm/s are investigated. It is shown that the tensile strength increases with an increase in the rate of solidification due to a decrease in the size of eutectic silicon and the transformation of its crystal flake into a fine-fiber one. In addition, there was an increase in tensile strength due to an increase of the share of the intermetallic phase, exceeding the reduced tensile strength due to an increase in the amount of the α-Al phase. An increase in the silicon content in the samples during solidification at a rate of 0.1 mm/s does not lead to a change in structure and strength. At a higher rate of solidification, there is a reduction of the share of eutectic and a decrease in strength.
- 1 January 2023
- Published by Ioffe Institute Russian Academy of Sciences in Журнал технической физики
- Vol. 93 (4) , 554
Влияние скорости направленной кристаллизации и содержания кремния на структуру и прочность Al-Si-Cu-сплава
The structure and strength of Al−xSi−2wt.%Cu (x = 15, 17 and 20wt.%) alloys obtained by directional solidification at a rate of 0.1 and 0.8mm/s are investigated. It is shown that the tensile strength increases with an increase in the rate of solidification due to a decrease in the size of eutectic silicon and the transformation of its crystal flake into a fine-fiber one. In addition, there was an increase in tensile strength due to an increase of the share of the intermetallic phase, exceeding the reduced tensile strength due to an increase in the amount of the α-Al phase. An increase in the silicon content in the samples during solidification at a rate of 0.1 mm/s does not lead to a change in structure and strength. At a higher rate of solidification, there is a reduction of the share of eutectic and a decrease in strength.
- 11 December 2020
- Published by Pleiades Publishing Ltd in Technical Physics
- Vol. 65 (12) , 1981-1986
Wear and Coefficient of Friction of a Supermodified Hypereutectic Aluminum–Silicon Alloy
The friction coefficient and the wear of a hypereutectic aluminum alloy with 15 wt % silicon and a supermodified eutectic structure without primary silicon crystals, obtained by directional crystallization at a solidification rate of 1 mm/s, are studied. It is shown that this alloy, which has high strength and ductility, has a lower friction coefficient and a higher wear resistance than the alloy with 20 wt % silicon. After modification with strontium, its tribological properties are superior to those of the hypereutectic commercial alloy.
- 11 December 2020
- Published by Pleiades Publishing Ltd in Technical Physics
- Vol. 65 (12) , 1981-1986
Wear and Coefficient of Friction of a Supermodified Hypereutectic Aluminum–Silicon Alloy
The friction coefficient and the wear of a hypereutectic aluminum alloy with 15 wt % silicon and a supermodified eutectic structure without primary silicon crystals, obtained by directional crystallization at a solidification rate of 1 mm/s, are studied. It is shown that this alloy, which has high strength and ductility, has a lower friction coefficient and a higher wear resistance than the alloy with 20 wt % silicon. After modification with strontium, its tribological properties are superior to those of the hypereutectic commercial alloy.
- 1 January 2020
- Published by Ioffe Institute Russian Academy of Sciences in Журнал технической физики
- Vol. 90 (12) , 2072
Износ и коэффициент трения супермодифицированного заэвтектического сплава алюминия с кремнием
Изучены коэффициент трения и износ заэвтектического по составу сплава алюминия с 15 wt.% кремния с супермодифицированной эвтектической структурой без первичных кристаллов кремния, полученного направленной кристаллизацией при скорости затвердевания 1 mm/s. Показано, что этот сплав с высокой прочностью и пластичностью имеет более низкий коэффициент трения и более высокое сопротивление износу, чем сплав с 20 wt.% кремния. После модификации стронцием его трибологические свойства превосходят свойства заэвтектического коммерческого сплава. Ключевые слова: микроструктура и механические свойства, трение и износ.
- 1 January 2020
- Published by Ioffe Institute Russian Academy of Sciences in Журнал технической физики
- Vol. 90 (12) , 2072
Износ и коэффициент трения супермодифицированного заэвтектического сплава алюминия с кремнием
Изучены коэффициент трения и износ заэвтектического по составу сплава алюминия с 15 wt.% кремния с супермодифицированной эвтектической структурой без первичных кристаллов кремния, полученного направленной кристаллизацией при скорости затвердевания 1 mm/s. Показано, что этот сплав с высокой прочностью и пластичностью имеет более низкий коэффициент трения и более высокое сопротивление износу, чем сплав с 20 wt.% кремния. После модификации стронцием его трибологические свойства превосходят свойства заэвтектического коммерческого сплава. Ключевые слова: микроструктура и механические свойства, трение и износ.
- 2 December 2019
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 28 (12) , 7302-7323
Structural and Mechanical Properties of Directionally Solidified Al-Si Alloys
- 2 December 2019
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 28 (12) , 7302-7323
Structural and Mechanical Properties of Directionally Solidified Al-Si Alloys
- 1 January 2019
- Published by Ioffe Institute Russian Academy of Sciences in Журнал технической физики
- Vol. 89 (8) , 1219
Неупругость и наноструктурная дислокационная деформация сплава алюминия с кремнием с супермодифицированной эвтектической структурой
Young’s modulus and the logarithmic decrement of oscillations at a frequency of ~100 kHz as well as the subgrain size and residual stresses in the strontium modified alloy of aluminum with 15 wt % silicon have been studied. The alloy was obtained with a solidification rate of 1 mm/s at the shifted eutectic point. The dependence of inelastic dislocation deformation on the applied oscillating stress has been obtained and analyzed. The effect of strontium modification on the microstrain diagram can be accounted for by transformation of the lamellar fiber structure of eutectic silicon into a superfine fiber structure.
- 1 January 2019
- Published by Ioffe Institute Russian Academy of Sciences in Журнал технической физики
- Vol. 89 (8) , 1219
Неупругость и наноструктурная дислокационная деформация сплава алюминия с кремнием с супермодифицированной эвтектической структурой
Young’s modulus and the logarithmic decrement of oscillations at a frequency of ~100 kHz as well as the subgrain size and residual stresses in the strontium modified alloy of aluminum with 15 wt % silicon have been studied. The alloy was obtained with a solidification rate of 1 mm/s at the shifted eutectic point. The dependence of inelastic dislocation deformation on the applied oscillating stress has been obtained and analyzed. The effect of strontium modification on the microstrain diagram can be accounted for by transformation of the lamellar fiber structure of eutectic silicon into a superfine fiber structure.
- 1 February 2016
- Published by Pleiades Publishing Ltd in Technical Physics Letters
- Vol. 42 (2) , 201-203
The effect of strontium on the mechanical properties of aluminum–silicon alloy
- 1 February 2016
- Published by Pleiades Publishing Ltd in Technical Physics Letters
- Vol. 42 (2) , 201-203
The effect of strontium on the mechanical properties of aluminum–silicon alloy
- 4 August 2015
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 57 (8) , 1555-1558
Inelasticity and precipitation of germanium from a solid solution in Al-Ge binary alloys
The influence of precipitation of germanium atoms in a solid solution on the dependence of the inelasticity characteristics on the germanium content in aluminum-germanium alloys prepared by directional crystallization has been studied. It has been shown that the Young’s modulus defect, the amplitude-dependent decrement, and the microplastic flow stress at a specified cyclic strain amplitude have extreme values at the eutectic germanium content in the alloy. The eutectic composition of the alloy undergoes a ductilebrittle transition. It has been found that there is a correlation between the dependences of the Young’s modulus defect, amplitude-dependent decrement, microplastic flow stress, and specific entropy of the exothermal process of germanium precipitation on the germanium content in the hypoeutectic alloy. The concentration dependences of the inelasticity characteristics and their changes after annealing have been explained by the change in the resistance to the motion of intragrain dislocations due to different structures of the Guinier-Preston zones formed during the precipitation of germanium atoms.
- 4 August 2015
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 57 (8) , 1555-1558
Inelasticity and precipitation of germanium from a solid solution in Al-Ge binary alloys
The influence of precipitation of germanium atoms in a solid solution on the dependence of the inelasticity characteristics on the germanium content in aluminum-germanium alloys prepared by directional crystallization has been studied. It has been shown that the Young’s modulus defect, the amplitude-dependent decrement, and the microplastic flow stress at a specified cyclic strain amplitude have extreme values at the eutectic germanium content in the alloy. The eutectic composition of the alloy undergoes a ductilebrittle transition. It has been found that there is a correlation between the dependences of the Young’s modulus defect, amplitude-dependent decrement, microplastic flow stress, and specific entropy of the exothermal process of germanium precipitation on the germanium content in the hypoeutectic alloy. The concentration dependences of the inelasticity characteristics and their changes after annealing have been explained by the change in the resistance to the motion of intragrain dislocations due to different structures of the Guinier-Preston zones formed during the precipitation of germanium atoms.
- 18 February 2015
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 57 (2) , 229-233
Kinetics of the precipitation of germanium in binary aluminum-germanium alloys produced by directed crystallization
The precipitation of germanium in aluminum-germanium alloys produced by directed crystallization according to the Stepanov’s method at a rate of 102 μm/s has been investigated using differential scanning calorimetry. The activation energy of the precipitation has been measured, and the dependence of the enthalpy of this process on the germanium content in the alloys in the range from 43 to 64 wt % has been studied. The change in the character of this dependence in the range of the eutectic concentration (53 wt % Ge) has been established.
- 18 February 2015
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 57 (2) , 229-233
Kinetics of the precipitation of germanium in binary aluminum-germanium alloys produced by directed crystallization
The precipitation of germanium in aluminum-germanium alloys produced by directed crystallization according to the Stepanov’s method at a rate of 102 μm/s has been investigated using differential scanning calorimetry. The activation energy of the precipitation has been measured, and the dependence of the enthalpy of this process on the germanium content in the alloys in the range from 43 to 64 wt % has been studied. The change in the character of this dependence in the range of the eutectic concentration (53 wt % Ge) has been established.
- 6 July 2014
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 56 (7) , 1363-1367
Elasticity, anelasticity, and microplasticity of directionally crystallized aluminum-germanium alloys
The structure, Young’s modulus defect, and internal friction in aluminum-germanium alloys have been studied under conditions of longitudinal elastic vibrations with a strain amplitude in the range of...
- 6 July 2014
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 56 (7) , 1363-1367
Elasticity, anelasticity, and microplasticity of directionally crystallized aluminum-germanium alloys
The structure, Young’s modulus defect, and internal friction in aluminum-germanium alloys have been studied under conditions of longitudinal elastic vibrations with a strain amplitude in the range of...