Insup Noh
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Insup Noh has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
Giyoong Tae
Department of Materials Science Engineering, Gwangju Institute of Science and Technology, 1 Oryong-dong, Buk-gu, Gwangju 500-712, Republic of Korea
2 shared publicationsYoon‐Jeong Choi
Department of Chemical Engineering, Seoul National University of Technology, Gongnung-dong 172, Nowon-gu, Seoul 139-743, Republic of Korea
2 shared publicationsYoungsook Son
Laboratory of Tissue Engineering, Korea Institute of Radiological and Medical Sciences, 215-4 Gongneung-Dong, Nowon-Gu, Seoul 139-706, Korea
2 shared publicationsBeom‐Young Park
Products and Utility Division, National Livestock Research Institute, 564 Omokchun-Dong, Kwonsun-Gu, Suwon 441-460, Korea
1 shared publicationChoong Man Hong
Biologics Evaluation Department, Korea Food & Drug Administration, Nokbun-dong 5, Eunpyung-Gu, Seoul, 122-704, Korea
1 shared publicationChoong‐Man Hong
Blood Products Division, Korea Food and Drug Administration, 5 Nokbun-dong, Eunpung-Gu, Seoul 122-704, Korea
1 shared publication
Latest Publications
- 30 August 2008
- Published by Elsevier in Surface and Coatings Technology
- Vol. 202 (22-23) , 5713-5717
Evaluation of porous poly(lactide-co-glycolide) scaffold surface-modified by irradiation of nitrogen ion beams
- 30 August 2008
- Published by Elsevier in Surface and Coatings Technology
- Vol. 202 (22-23) , 5713-5717
Evaluation of porous poly(lactide-co-glycolide) scaffold surface-modified by irradiation of nitrogen ion beams
- 25 May 2007
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 83A (3) , 674-682
Synthesis and characterization ofin situchitosan‐based hydrogel via grafting of carboxyethyl acrylate
We developed and characterized a novelin situchitosan‐poly(ethylene oxide) (PEO) hydrogel via two steps: 2‐carboxyethyl acrylate molecules were grafted to the primary amine functional groups in chitosan in the first step and then Michael type addition reaction was processed between the grafted acrylate end groups and the thiol end groups in the PEO. Grafting of acrylate molecules to the amine groups in the deacetylated water soluble chitosan was confirmed by observing the new acrylate peaks by the FTIR and NMR spectra of the acrylated chitosan samples, as well as changes in relative viscosities of chitosan and acrylated chitosan. Formation of the chitosan‐PEO hydrogel was visually observed with digital images after both gelation and hydration. Rheological analyses of the hydrogel formation were performed to detect its gelation time, phase angle changes, and visco‐elastic properties over frequency and strain percentage. Their results indicated that the gelation process was completed within 10 min after mixing the precursor liquid solutions. An extent of water swelling, mechanical strength against compression and the morphologies of the hydrogel surface and cross sections after dehydration process were analyzed by microbalance measurement, texture analyzer, and scanning electron microscopy observation, respectively. Biological activities of the hydrogels were evaluated by observing smooth muscle cell behaviors such as cell adhesion and viability as well as by measuring the number of adhered cells on their surfaces. © 2007 Wiley Periodicals, Inc. J Biomed Mater Res 2007
- 25 May 2007
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 83A (3) , 674-682
Synthesis and characterization ofin situchitosan‐based hydrogel via grafting of carboxyethyl acrylate
We developed and characterized a novelin situchitosan‐poly(ethylene oxide) (PEO) hydrogel via two steps: 2‐carboxyethyl acrylate molecules were grafted to the primary amine functional groups in chitosan in the first step and then Michael type addition reaction was processed between the grafted acrylate end groups and the thiol end groups in the PEO. Grafting of acrylate molecules to the amine groups in the deacetylated water soluble chitosan was confirmed by observing the new acrylate peaks by the FTIR and NMR spectra of the acrylated chitosan samples, as well as changes in relative viscosities of chitosan and acrylated chitosan. Formation of the chitosan‐PEO hydrogel was visually observed with digital images after both gelation and hydration. Rheological analyses of the hydrogel formation were performed to detect its gelation time, phase angle changes, and visco‐elastic properties over frequency and strain percentage. Their results indicated that the gelation process was completed within 10 min after mixing the precursor liquid solutions. An extent of water swelling, mechanical strength against compression and the morphologies of the hydrogel surface and cross sections after dehydration process were analyzed by microbalance measurement, texture analyzer, and scanning electron microscopy observation, respectively. Biological activities of the hydrogels were evaluated by observing smooth muscle cell behaviors such as cell adhesion and viability as well as by measuring the number of adhered cells on their surfaces. © 2007 Wiley Periodicals, Inc. J Biomed Mater Res 2007
- 29 August 2006
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 79A (4) , 943-953
Diffusion of bioactive molecules through the walls of the medial tissue‐engineered hybrid ePTFE grafts for applications in designs of vascular tissue regeneration
Strategies of better vascular tissue engineering may require delivery of soluble bioactive signals in cell culture medium to the cells in tissue-regenerating constructs. We measured the diffusivity and permeability of model tissue-engineering bioactive molecules such as water and heparin through the walls of both a hybrid ePTFE graft and a porcine carotid artery, a model vascular tissue. While diffusivities of H3-water and H3-heparin were measured as 3.9 × 10−6 and 1.6 × 10−6 cm2/s in the artery, respectively, under diffusional circulation of cell culture medium through the lumens of the carotid arteries, their corresponding permeabilities were 4.7 × 10−5 and 2.0 × 10−5 cm/s. On the other hand, diffusivities of H3-water and H3-heparin were also measured as 5.1 × 10−6 and 4.7 × 10−6 cm2/s, respectively, in the tissue-engineered hybrid ePTFE grafts; their corresponding permeabilities were 5.1 × 10−5 and 3.7 × 10−5 cm/s. The hybrid graft tissues were engineered by replacing the biodegradable, porous poly(lactide-co-glycolide) layers coated on the ePTFE surfaces with smooth muscle cell-derived tissues for 6 weeks. We analyzed the morphologies of the artery and the engineered hybrid ePTFE tissues with scanning electron microscopy and H&E stains. While the artery had its typical structure properties with layers of intima, media and adventitia, the tissue-engineered ePTFE hybrid graft had two layers of engineered tissues on the inner and outer surfaces of the ePTFE. There were no significant differences among the luminal tissue morphologies of the test samples from the effects of diffusion flow applications, with minor changes on their luminal surfaces. The results of water and heparin diffusion experiments indicated that these bioactive molecules were well transported from the cell culture medium to the tissue-engineering cells, enough to support tissue regeneration. We hope that these transport results may elucidate the transport behaviors of soluble nutrient molecules and biological signals through the vascular constructs under tissue engineering processes. © 2006 Wiley Periodicals, Inc. J Biomed Mater Res, 2006
- 29 August 2006
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 79A (4) , 943-953
Diffusion of bioactive molecules through the walls of the medial tissue‐engineered hybrid ePTFE grafts for applications in designs of vascular tissue regeneration
Strategies of better vascular tissue engineering may require delivery of soluble bioactive signals in cell culture medium to the cells in tissue-regenerating constructs. We measured the diffusivity and permeability of model tissue-engineering bioactive molecules such as water and heparin through the walls of both a hybrid ePTFE graft and a porcine carotid artery, a model vascular tissue. While diffusivities of H3-water and H3-heparin were measured as 3.9 × 10−6 and 1.6 × 10−6 cm2/s in the artery, respectively, under diffusional circulation of cell culture medium through the lumens of the carotid arteries, their corresponding permeabilities were 4.7 × 10−5 and 2.0 × 10−5 cm/s. On the other hand, diffusivities of H3-water and H3-heparin were also measured as 5.1 × 10−6 and 4.7 × 10−6 cm2/s, respectively, in the tissue-engineered hybrid ePTFE grafts; their corresponding permeabilities were 5.1 × 10−5 and 3.7 × 10−5 cm/s. The hybrid graft tissues were engineered by replacing the biodegradable, porous poly(lactide-co-glycolide) layers coated on the ePTFE surfaces with smooth muscle cell-derived tissues for 6 weeks. We analyzed the morphologies of the artery and the engineered hybrid ePTFE tissues with scanning electron microscopy and H&E stains. While the artery had its typical structure properties with layers of intima, media and adventitia, the tissue-engineered ePTFE hybrid graft had two layers of engineered tissues on the inner and outer surfaces of the ePTFE. There were no significant differences among the luminal tissue morphologies of the test samples from the effects of diffusion flow applications, with minor changes on their luminal surfaces. The results of water and heparin diffusion experiments indicated that these bioactive molecules were well transported from the cell culture medium to the tissue-engineering cells, enough to support tissue regeneration. We hope that these transport results may elucidate the transport behaviors of soluble nutrient molecules and biological signals through the vascular constructs under tissue engineering processes. © 2006 Wiley Periodicals, Inc. J Biomed Mater Res, 2006
- 9 June 2006
- Published by IOP Publishing in Biomedical Materials
- Vol. 1 (3) , 116-123
Effects of cross-linking molecular weights in a hyaluronic acid–poly(ethylene oxide) hydrogel network on its properties
We examined the effects of cross-linking molecular weights on the properties of a hyaluronic acid (HA)-poly(ethylene oxide) (PEO) hydrogel. Swelling behaviors, mechanical strength and rheological behaviors of the HA-PEO hydrogel were evaluated by employing different cross-linking molecular weights (100 kDa and 1.63 mDa) of the HAs in the hydrogel networks. The low molecular weight of HA was obtained in advance by treating high molecular weight HA with a hydrogen chloride solution. Methacrylation of HA was obtained by grafting aminopropylmethacrylate to its caroboxylic acid functional groups. While reduction of the HA molecular weights was confirmed by gel permeation chromatography, the degree of methacrylate grafting to the HA was measured by (1)H-nuclear magnetic resonance. Synthesis of the HA-PEO hydrogel was successfully achieved via the Michael-type addition reaction between the methacrylate arm groups in the HA and the six thiol groups in PEO. The hydrogel formation was not dependent upon the HA molecular weights and its gelation behaviors were markedly different. Compared to the properties of the high molecular weight HA-based PEO one, the low molecular weight HA-based hydrogel induced quicker hydrogelation, as observed from the behaviors of the elastic and viscous modulus. Furthermore, the low molecular weight HA-based hydrogel demonstrated stronger mechanical properties as measured with a texture analyzer, lower water absorption as measured with a microbalance and smaller pore sizes on its surface and cross section as observed with scanning electron microscopy. The information about the effects of the cross-linking molecular weights of the gel network on the properties of the HA-based PEO hydrogel may lead to better design of hydrogels, especially in tissue engineering applications.
- 9 June 2006
- Published by IOP Publishing in Biomedical Materials
- Vol. 1 (3) , 116-123
Effects of cross-linking molecular weights in a hyaluronic acid–poly(ethylene oxide) hydrogel network on its properties
We examined the effects of cross-linking molecular weights on the properties of a hyaluronic acid (HA)-poly(ethylene oxide) (PEO) hydrogel. Swelling behaviors, mechanical strength and rheological behaviors of the HA-PEO hydrogel were evaluated by employing different cross-linking molecular weights (100 kDa and 1.63 mDa) of the HAs in the hydrogel networks. The low molecular weight of HA was obtained in advance by treating high molecular weight HA with a hydrogen chloride solution. Methacrylation of HA was obtained by grafting aminopropylmethacrylate to its caroboxylic acid functional groups. While reduction of the HA molecular weights was confirmed by gel permeation chromatography, the degree of methacrylate grafting to the HA was measured by (1)H-nuclear magnetic resonance. Synthesis of the HA-PEO hydrogel was successfully achieved via the Michael-type addition reaction between the methacrylate arm groups in the HA and the six thiol groups in PEO. The hydrogel formation was not dependent upon the HA molecular weights and its gelation behaviors were markedly different. Compared to the properties of the high molecular weight HA-based PEO one, the low molecular weight HA-based hydrogel induced quicker hydrogelation, as observed from the behaviors of the elastic and viscous modulus. Furthermore, the low molecular weight HA-based hydrogel demonstrated stronger mechanical properties as measured with a texture analyzer, lower water absorption as measured with a microbalance and smaller pore sizes on its surface and cross section as observed with scanning electron microscopy. The information about the effects of the cross-linking molecular weights of the gel network on the properties of the HA-based PEO hydrogel may lead to better design of hydrogels, especially in tissue engineering applications.
- 1 September 2005
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 75A (4) , 824-831
Evaluations of blood compatibility via protein adsorption treatment of the vascular scaffold surfaces fabricated with polylactide and surface‐modified expanded polytetrafluoroethylene for tissue engineering applications
Blood compatibility was evaluated by short-term in vitro blood perfusion on candidate vascular scaffold surfaces of a biodegradable, porous polylactide scaffold and a chemically surface-modified expanded polytetrafluoroethylene (ePTFE) over a clinical ePTFE, by measuring blood cell adhesion either directly or after adsorption treatment with albumin and fibrinogen. The results indicated that the extent of blood cell adhesion was affected by scaffold surface properties and pre-adsorption of proteins such as fibrinogen and albumin. Surface morphologies and porosity of the scaffolds were characterized by scanning electron microscopy and porosimetry, and the amount of fibrinogen and albumin adsorbed on the scaffolds was measured and verified by employing radiolabeled C14 albumin and I125 fibrinogen by a scintillation counter and a gamma counter, respectively. Even though treatment of fibrinogen adsorption on the samples in advance led to higher induction of blood cell adhesion than those with no fibrinogen adsorption, the polylactide scaffold surface itself induced highest amount of the adhered blood cells in this study judged by analyses of their surface area. These results would be employed as guidance in determining a choice of the implant methods, in vitro versus in vivo tissue engineering, of the novel chemically modified ePTFE and the biodegradable polylactide scaffolds. © 2005 Wiley Periodicals, Inc. J Biomed Mater Res, 2005
- 1 September 2005
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 75A (4) , 824-831
Evaluations of blood compatibility via protein adsorption treatment of the vascular scaffold surfaces fabricated with polylactide and surface‐modified expanded polytetrafluoroethylene for tissue engineering applications
Blood compatibility was evaluated by short-term in vitro blood perfusion on candidate vascular scaffold surfaces of a biodegradable, porous polylactide scaffold and a chemically surface-modified expanded polytetrafluoroethylene (ePTFE) over a clinical ePTFE, by measuring blood cell adhesion either directly or after adsorption treatment with albumin and fibrinogen. The results indicated that the extent of blood cell adhesion was affected by scaffold surface properties and pre-adsorption of proteins such as fibrinogen and albumin. Surface morphologies and porosity of the scaffolds were characterized by scanning electron microscopy and porosimetry, and the amount of fibrinogen and albumin adsorbed on the scaffolds was measured and verified by employing radiolabeled C14 albumin and I125 fibrinogen by a scintillation counter and a gamma counter, respectively. Even though treatment of fibrinogen adsorption on the samples in advance led to higher induction of blood cell adhesion than those with no fibrinogen adsorption, the polylactide scaffold surface itself induced highest amount of the adhered blood cells in this study judged by analyses of their surface area. These results would be employed as guidance in determining a choice of the implant methods, in vitro versus in vivo tissue engineering, of the novel chemically modified ePTFE and the biodegradable polylactide scaffolds. © 2005 Wiley Periodicals, Inc. J Biomed Mater Res, 2005