Archana Agrawal
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Archana Agrawal has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
K.K. Sahu
Metal Extraction & Recycling Division, National Metallurgical Laboratory (CSIR), Jamshedpur 831007, India
6 shared publications- Banshi Dhar Pandey
Metal Extraction & Forming Div., CSIR-National Metallurgical Laboratory (NML), Jamshedpur, India
5 shared publications D. Mishra
Metal Extraction and Forming Division, CSIR-National Metallurgical Laboratory, Jamshedpur, India
3 shared publicationsK. K. Sahu
Metal Extraction and Forming Division, CSIR-National Metallurgical Laboratory, Jamshedpur, India
3 shared publicationsS. Kumari
Metal Extraction and Processing Division, National Metallurgical Laboratory , Jamshedpur , India
3 shared publicationsD. Bagchi
Metal Extraction and Forming Division, National Metallurgical Laboratory , Jamshedpur, India
2 shared publications
Latest Publications
- 13 January 2022
- Published by Springer Nature in Journal of Sustainable Metallurgy
- Vol. 8 (1) , 207-217
Selective Separation of Iron and Cobalt from Leached Tungsten Carbide Scrap by Solvent Extraction
- 13 January 2022
- Published by Springer Nature in Journal of Sustainable Metallurgy
- Vol. 8 (1) , 207-217
Selective Separation of Iron and Cobalt from Leached Tungsten Carbide Scrap by Solvent Extraction
- 1 February 2018
- Published by Elsevier in Journal of Hazardous Materials
- Vol. 344, 169-178
Process integration for material synthesis from a deactivated catalyst: Studies on the interaction of metal ions between two immiscible phases
- 1 February 2018
- Published by Elsevier in Journal of Hazardous Materials
- Vol. 344, 169-178
Process integration for material synthesis from a deactivated catalyst: Studies on the interaction of metal ions between two immiscible phases
- 1 August 2016
- Published by Elsevier in Journal of Molecular Liquids
- Vol. 220, 82-91
Comparative performance assessment of solvents for the extraction of H2SO4 from spent electrolytic bleed stream of copper industry
- 1 August 2016
- Published by Elsevier in Journal of Molecular Liquids
- Vol. 220, 82-91
Comparative performance assessment of solvents for the extraction of H2SO4 from spent electrolytic bleed stream of copper industry
- 15 May 2012
- Published by Taylor & Francis in Mineral Processing and Extractive Metallurgy Review
- Vol. 33 (5) , 339-351
Exploitation of Copper Bleed Stream for the Extraction and Recovery of Copper and Nickel by Bis(2,4,4-trimethylpentyl)phosphinic Acid
Bleed streams from copper electrolysis/electrowinning processes potentially contain high amounts of acid, copper, and nickel which need an effective treatment before disposal. A systematic study was carried out to optimize the parameters for the extraction and recovery of metal values using bis(2,4,4-trimethylpentyl)phosphinic acid (Cyanex 272) diluted with kerosene. Since pH has a major role to play in the separation of Cu from Ni, a 60% saponified solvent was used for extraction studies. With an increase in equilibrium pH from 3.32 to 5.48 and extractant concentration from 5 to 20%, there is an increase in the percentage extraction of metal ions. With a solvent concentration of 20%, the separation factor for Cu with respect to Ni ( ) increases from 39.1 to 118.8 with the increase in pH from 3.3 to 5.5. Loading capacity of 20% Cyanex 272 was found to be 30.8 g/L Cu and 0.024 g/L Ni. After scrubbing of coextracted Ni(II) with 15 g/L H2SO4, the loaded organic containing 30.59 g/L Cu(II) and 4 ppm Ni(II) was stripped with 75 g/L sulfuric acid. A McCabe-Thiele plot shows the requirement of two counter-current stages at an O:A ratio of 1:1 for extraction and two counter-current stages at O:A ratio of 2:1 for the stripping of copper. Results of the present investigation indicate the possibility of the use of saponified Cyanex 272 for the extraction, separation, and recovery of copper and nickel from the actual spent copper bleed streams.
- 15 May 2012
- Published by Taylor & Francis in Mineral Processing and Extractive Metallurgy Review
- Vol. 33 (5) , 339-351
Exploitation of Copper Bleed Stream for the Extraction and Recovery of Copper and Nickel by Bis(2,4,4-trimethylpentyl)phosphinic Acid
Bleed streams from copper electrolysis/electrowinning processes potentially contain high amounts of acid, copper, and nickel which need an effective treatment before disposal. A systematic study was carried out to optimize the parameters for the extraction and recovery of metal values using bis(2,4,4-trimethylpentyl)phosphinic acid (Cyanex 272) diluted with kerosene. Since pH has a major role to play in the separation of Cu from Ni, a 60% saponified solvent was used for extraction studies. With an increase in equilibrium pH from 3.32 to 5.48 and extractant concentration from 5 to 20%, there is an increase in the percentage extraction of metal ions. With a solvent concentration of 20%, the separation factor for Cu with respect to Ni ( ) increases from 39.1 to 118.8 with the increase in pH from 3.3 to 5.5. Loading capacity of 20% Cyanex 272 was found to be 30.8 g/L Cu and 0.024 g/L Ni. After scrubbing of coextracted Ni(II) with 15 g/L H2SO4, the loaded organic containing 30.59 g/L Cu(II) and 4 ppm Ni(II) was stripped with 75 g/L sulfuric acid. A McCabe-Thiele plot shows the requirement of two counter-current stages at an O:A ratio of 1:1 for extraction and two counter-current stages at O:A ratio of 2:1 for the stripping of copper. Results of the present investigation indicate the possibility of the use of saponified Cyanex 272 for the extraction, separation, and recovery of copper and nickel from the actual spent copper bleed streams.
- 1 December 2011
- Published by Elsevier in Journal of Environmental Management
- Vol. 92 (12) , 3105-3111
Studies on solvent extraction of iron(III) as a step for conversion of a waste effluent to a value added product
- 1 December 2011
- Published by Elsevier in Journal of Environmental Management
- Vol. 92 (12) , 3105-3111
Studies on solvent extraction of iron(III) as a step for conversion of a waste effluent to a value added product
- 7 May 2010
- Published by Taylor & Francis in Mineral Processing and Extractive Metallurgy Review
- Vol. 31 (3) , 121-134
Treatment of Chloride Waste Pickle Liquor by Solvent Extraction for the Recovery of Iron
A systematic study of the extraction of Fe(III) from chloride waste pickle liquor has been investigated using Cyanex 923 diluted with kerosene to recover iron values from the pickle liquor. Various parameters were studied to optimize the conditions for maximum recovery of iron. Extraction increases with increasing concentration of both hydrochloric acid and extractant. The species extracted into the organic phase appears to be HFeCl2 with 1 M of the solvent. Effect of various salts as additives on Fe extraction was also studied and it was found that addition of NaCl enhanced the extraction about 2.5 times as compared to that without its addition. Saturated loading capacity was found to be 60.9 g/L Fe in four contacts at O/A of 1. The stripping of Fe(III) with different concentration of hydrochloric acid and nitric acid from the loaded Cyanex 923 was found to increase up to 1 M of both the acids and then decrease with further increase in acid concentration up to 10 M. However, 100% stripping efficiency of Fe(III) was achieved with 0.8 M oxalic acid in two countercurrent stages at an aqueous:organic phase ratio of 3:1. Extraction parameters for maximum extraction of Fe(III) were optimized.
- 7 May 2010
- Published by Taylor & Francis in Mineral Processing and Extractive Metallurgy Review
- Vol. 31 (3) , 121-134
Treatment of Chloride Waste Pickle Liquor by Solvent Extraction for the Recovery of Iron
A systematic study of the extraction of Fe(III) from chloride waste pickle liquor has been investigated using Cyanex 923 diluted with kerosene to recover iron values from the pickle liquor. Various parameters were studied to optimize the conditions for maximum recovery of iron. Extraction increases with increasing concentration of both hydrochloric acid and extractant. The species extracted into the organic phase appears to be HFeCl2 with 1 M of the solvent. Effect of various salts as additives on Fe extraction was also studied and it was found that addition of NaCl enhanced the extraction about 2.5 times as compared to that without its addition. Saturated loading capacity was found to be 60.9 g/L Fe in four contacts at O/A of 1. The stripping of Fe(III) with different concentration of hydrochloric acid and nitric acid from the loaded Cyanex 923 was found to increase up to 1 M of both the acids and then decrease with further increase in acid concentration up to 10 M. However, 100% stripping efficiency of Fe(III) was achieved with 0.8 M oxalic acid in two countercurrent stages at an aqueous:organic phase ratio of 3:1. Extraction parameters for maximum extraction of Fe(III) were optimized.
- Top Cited Papers
- 1 November 2009
- Published by Elsevier in Journal of Hazardous Materials
- Vol. 171 (1-3) , 61-75
An overview of the recovery of acid from spent acidic solutions from steel and electroplating industries
- 1 November 2009
- Published by Elsevier in Journal of Hazardous Materials
- Vol. 171 (1-3) , 61-75
Top Cited PapersAn overview of the recovery of acid from spent acidic solutions from steel and electroplating industries
- 3 September 2009
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 40 (6) , 877-885
Value Addition to Sulfate Waste Pickle Liquor of Steel Industry Using Hydrometallurgical Processes
- 3 September 2009
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 40 (6) , 877-885
Value Addition to Sulfate Waste Pickle Liquor of Steel Industry Using Hydrometallurgical Processes
- 30 March 2009
- Published by Taylor & Francis in Mineral Processing and Extractive Metallurgy Review
- Vol. 30 (2) , 136-162
AN OVERVIEW OF PROCESS OPTIONS AND BEHAVIORAL ASPECTS OF THE COPPER VALUES RECOVERED FROM THE COPPER BLEED STREAM OF A COPPER SMELTER DEVELOPED AT THE NATIONAL METALLURGICAL LABORATORY
In the present research, an effort has been made to prepare copper salt/powder from the copper bleed stream generated during the electrowinning of pure copper from the copper anode in a copper smelter. Various approaches have been opted for the complete recovery of copper values such as: evaporation–crystallization, electrolytic process, and direct hydrogen reduction. Physical and chemical properties of copper powder/salt produced from the large-scale experiments from actual plant and model solutions have been evaluated for P/M applications and compared with the standard properties. Thus, mixed crystal suitable for recycling back to the system as a makeup salt containing nickel in a tolerable range could be recovered by evaporation and crystallization of the bleed stream up, to 50%. Copper powder recovery by the electrolysis process at a current density of 700 A/m2 was about 95%. Scanning electron microscope examination showed that the powder was dendritic in nature. On annealing, the purity of the copper powder was found to be 99.95%. The annealed powder had apparent density of 3.04 g/cc, hydrogen loss 0.72%, and acid insoluble as 0.27%. On compaction of 99% and the annealed powder had an apparent density of 3.50 g/cc, flow rate 35.6 g/min, hydrogen loss 0.195%, purity 99.8%, and green density of 8.57 g/cc while the powder from the actual plant solution was found to have an apparent density of 3.49 g/cc, flow rate 46.0 g/min, hydrogen loss 0.598%, purity 99.4%, and green density 8.57 g/cc for the powder < 100 µm in size. Thus, the properties of copper powder produced by hydrogen reduction and electrolytic route were compared and were found to be suitable for the P/M applications.
- 30 March 2009
- Published by Taylor & Francis in Mineral Processing and Extractive Metallurgy Review
- Vol. 30 (2) , 136-162
AN OVERVIEW OF PROCESS OPTIONS AND BEHAVIORAL ASPECTS OF THE COPPER VALUES RECOVERED FROM THE COPPER BLEED STREAM OF A COPPER SMELTER DEVELOPED AT THE NATIONAL METALLURGICAL LABORATORY
In the present research, an effort has been made to prepare copper salt/powder from the copper bleed stream generated during the electrowinning of pure copper from the copper anode in a copper smelter. Various approaches have been opted for the complete recovery of copper values such as: evaporation–crystallization, electrolytic process, and direct hydrogen reduction. Physical and chemical properties of copper powder/salt produced from the large-scale experiments from actual plant and model solutions have been evaluated for P/M applications and compared with the standard properties. Thus, mixed crystal suitable for recycling back to the system as a makeup salt containing nickel in a tolerable range could be recovered by evaporation and crystallization of the bleed stream up, to 50%. Copper powder recovery by the electrolysis process at a current density of 700 A/m2 was about 95%. Scanning electron microscope examination showed that the powder was dendritic in nature. On annealing, the purity of the copper powder was found to be 99.95%. The annealed powder had apparent density of 3.04 g/cc, hydrogen loss 0.72%, and acid insoluble as 0.27%. On compaction of 99% and the annealed powder had an apparent density of 3.50 g/cc, flow rate 35.6 g/min, hydrogen loss 0.195%, purity 99.8%, and green density of 8.57 g/cc while the powder from the actual plant solution was found to have an apparent density of 3.49 g/cc, flow rate 46.0 g/min, hydrogen loss 0.598%, purity 99.4%, and green density 8.57 g/cc for the powder < 100 µm in size. Thus, the properties of copper powder produced by hydrogen reduction and electrolytic route were compared and were found to be suitable for the P/M applications.
- 1 April 2006
- Published by Taylor & Francis in Mineral Processing and Extractive Metallurgy Review
- Vol. 27 (2) , 159-175
SYNTHESIS OF COPPER METAL/SALTS FROM COPPER BLEED SOLUTION OF A COPPER PLANT
Copper bleed solution (CBS) generated during the electrorefining of anode copper contains 40 g/L Cu, 10–20 g/L Ni, and 170–200 g/L H2SO4, along with other impurities in different quantities. In order to get the valuable metals from this CBS, studies have been carried out to crystallize and recover metal salts on bench scale with/without partial decopperization from the point of view of reuse and the recycling of the sulphate salts and the acid recovered back to the system. Studies showed the possibility of recovering copper sulphate salt without affecting its purity with respect to nickel by controlling the extent of evaporation. In an alternative approach, a part of copper metal of purity 99.85% produced during partial decopperization of copper from 39.8 to 9.64 g/L Cu without affecting the current efficiency at a current density of 100 A/m2. Subsequently, mixed salt containing 9.80% Cu and 13.19% Ni has also been produced from the partially decopperized solution. The mixed salt could be processed for metal recovery by solvent extraction. The mother and wash liquor could be recycled in the electrorefining plant for acid and copper make-up.
- 1 April 2006
- Published by Taylor & Francis in Mineral Processing and Extractive Metallurgy Review
- Vol. 27 (2) , 159-175
SYNTHESIS OF COPPER METAL/SALTS FROM COPPER BLEED SOLUTION OF A COPPER PLANT
Copper bleed solution (CBS) generated during the electrorefining of anode copper contains 40 g/L Cu, 10–20 g/L Ni, and 170–200 g/L H2SO4, along with other impurities in different quantities. In order to get the valuable metals from this CBS, studies have been carried out to crystallize and recover metal salts on bench scale with/without partial decopperization from the point of view of reuse and the recycling of the sulphate salts and the acid recovered back to the system. Studies showed the possibility of recovering copper sulphate salt without affecting its purity with respect to nickel by controlling the extent of evaporation. In an alternative approach, a part of copper metal of purity 99.85% produced during partial decopperization of copper from 39.8 to 9.64 g/L Cu without affecting the current efficiency at a current density of 100 A/m2. Subsequently, mixed salt containing 9.80% Cu and 13.19% Ni has also been produced from the partially decopperized solution. The mixed salt could be processed for metal recovery by solvent extraction. The mother and wash liquor could be recycled in the electrorefining plant for acid and copper make-up.