Kenji Iwase
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Kenji Iwase has a total of 64 co-authors. Here are the top co-authors by number of shared publications:
Kazuhiro Mori
Research Reactor Institute, Kyoto University, 2-1010 Asashiro-nishi, Kumatori, Sennan, Osaka 590-0494, Japan
5 shared publicationsToru Ishigaki
Frontier Research Center for Applied Sciences, Ibaraki University, 162-1 Shirakata, Tokai, Naka, Ibaraki 319-1106, Japan
5 shared publicationsT Ito
Shizuoka Univ
4 shared publicationsEtsuo Akiba
National Institute of Advanced Industrial Science and Technology (AIST), AIST Central-5, 1-1-1 Higashi, Tsukuba, Ibaraki 305-8565, Japan
3 shared publications- Kouji Sakaki
Energy Process Research Institute, National Institute of Advanced Industrial Science and Technology (AIST), Tsukuba 305-8569, Japan
3 shared publications T Matsumaru
Shizuoka Univ
3 shared publications
Latest Publications
- 1 September 2015
- Published by Elsevier in Clinical Nutrition
- Vol. 34, S224
MON-PP262: Perioperative Management Using Formulation (PN-2) Contained Collagen Peptides for Patients with Colorectal Cancer: A Preliminary Report
- 1 September 2015
- Published by Elsevier in Clinical Nutrition
- Vol. 34, S224
MON-PP262: Perioperative Management Using Formulation (PN-2) Contained Collagen Peptides for Patients with Colorectal Cancer: A Preliminary Report
- 5 December 2013
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 52 (24) , 14270-14274
Crystal Structure and Cyclic Hydrogenation Property of Pr4MgNi19
The hydrogen absorption–desorption property and the crystal structure of Pr4MgNi19 was investigated by pressure–composition isotherm measurement and X-ray diffraction (XRD). Pr4MgNi19 consisted of two phases: 52.9% Ce5Co19-type structure (3R) and 47.0% Gd2Co7-type structure (3R). Sm5Co19-type structure (2H) and Ce2Ni7-type structure (2H) were not observed in the XRD profile. The Mg atoms substituted at the Pr sites in a MgZn2-type cell. The maximum hydrogen capacity reached 1.14 H/M (1.6 mass%) at 2 MPa. The hysteresis factor, Hf = ln(Pabs/Pdes), was 1.50. The cyclic hydrogenation property of Pr4MgNi19 was investigated up to 1000 absorption–desorption cycles. After 250, 500, 750, and 1000 cycles, the retention rates of hydrogen were reduced to 94%, 92%, 91%, and 90%, respectively. These properties were superior to those of Pr2MgNi9 and Pr3MgNi14.
- 5 December 2013
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 52 (24) , 14270-14274
Crystal Structure and Cyclic Hydrogenation Property of Pr4MgNi19
The hydrogen absorption–desorption property and the crystal structure of Pr4MgNi19 was investigated by pressure–composition isotherm measurement and X-ray diffraction (XRD). Pr4MgNi19 consisted of two phases: 52.9% Ce5Co19-type structure (3R) and 47.0% Gd2Co7-type structure (3R). Sm5Co19-type structure (2H) and Ce2Ni7-type structure (2H) were not observed in the XRD profile. The Mg atoms substituted at the Pr sites in a MgZn2-type cell. The maximum hydrogen capacity reached 1.14 H/M (1.6 mass%) at 2 MPa. The hysteresis factor, Hf = ln(Pabs/Pdes), was 1.50. The cyclic hydrogenation property of Pr4MgNi19 was investigated up to 1000 absorption–desorption cycles. After 250, 500, 750, and 1000 cycles, the retention rates of hydrogen were reduced to 94%, 92%, 91%, and 90%, respectively. These properties were superior to those of Pr2MgNi9 and Pr3MgNi14.
- 20 August 2013
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 52 (17) , 10105-10111
In Situ XRD Study of La2Ni7Hx During Hydrogen Absorption–Desorption
Structural changes of La2Ni7Hx during the first and second absorption–desorption processes along the P–C isotherm were investigated by in situ X-ray diffraction (XRD). Orthorhombic (Pbcn) and monoclinic (C2/c) hydrides coexisted in the first absorption plateau, but only a monoclinic (C2/c) hydride was observed in the first desorption plateau. Phase transformation of La2Ni7Hx was irreversible between the first as well as the second absorption–desorption process. The lattice parameters and expansion of the La2Ni4 and LaNi5 cells during the absorption–desorption process were refined using the Rietveld method. The lattice parameters a and b of the orthorhombic hydride (Pbcn) decreased, while the lattice parameter c increased with increasing hydrogen content in the first absorption. During the first absorption, the volume of the orthorhombic La2Ni4 cell expanded by more than 50%, while the expansion of the LaNi5 cell was below 10%. The monoclinic La2Ni4 cell expanded to approximately four times the size of the LaNi5 cell in the first absorption. The lattice parameters a, b, and c of the monoclinic hydride (C2/c) decreased with decreasing hydrogen content in the first desorption. These La2Ni4 and LaNi5 cells contracted isotropically in the first desorption.
- 20 August 2013
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 52 (17) , 10105-10111
In Situ XRD Study of La2Ni7Hx During Hydrogen Absorption–Desorption
Structural changes of La2Ni7Hx during the first and second absorption–desorption processes along the P–C isotherm were investigated by in situ X-ray diffraction (XRD). Orthorhombic (Pbcn) and monoclinic (C2/c) hydrides coexisted in the first absorption plateau, but only a monoclinic (C2/c) hydride was observed in the first desorption plateau. Phase transformation of La2Ni7Hx was irreversible between the first as well as the second absorption–desorption process. The lattice parameters and expansion of the La2Ni4 and LaNi5 cells during the absorption–desorption process were refined using the Rietveld method. The lattice parameters a and b of the orthorhombic hydride (Pbcn) decreased, while the lattice parameter c increased with increasing hydrogen content in the first absorption. During the first absorption, the volume of the orthorhombic La2Ni4 cell expanded by more than 50%, while the expansion of the LaNi5 cell was below 10%. The monoclinic La2Ni4 cell expanded to approximately four times the size of the LaNi5 cell in the first absorption. The lattice parameters a, b, and c of the monoclinic hydride (C2/c) decreased with decreasing hydrogen content in the first desorption. These La2Ni4 and LaNi5 cells contracted isotropically in the first desorption.
- 17 October 2012
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 51 (21) , 11805-11810
Structural Parameters of Pr3MgNi14 during Hydrogen Absorption–Desorption Process
Structural parameters of Pr3MgNi14 after a cyclic hydrogen absorption–desorption process were investigated by X-ray diffraction. Pr3MgNi14 consisted of two phases: 80% Gd2Co7-type structure and 20% PuNi3-type structure. The pressure–composition (P–C) isotherm of Pr3MgNi14 indicates a maximum hydrogen capacity of 1.12 H/M (1.61 mass %) at 298 K. The cyclic property of Pr3MgNi14 up to 1000 cycles was measured at 313 K. The retention rate of the sample was 87.5% at 1000 cycles, which compares favorably with that of LaNi5. After 1000 cycles, the expansions of lattice parameters a and c and the lengths along the c-axes of the PrNi5 and PrMgNi4 cells of the Gd2Co7-type structures were 0.20%, 1.26%, 0.47%, and 3.68%, respectively. The metal sublattice expanded anisotropically after the cyclic test. The isotropic and anisotropic lattice strains can be refined by Rietveld analysis. The anisotropic and isotropic lattice strains were almost saturated at the first activation process and reached values of 0.2% and 0.1%, respectively, after 1000 cycles. These values are smaller by 1 order of magnitude than those of LaNi5.
- 17 October 2012
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 51 (21) , 11805-11810
Structural Parameters of Pr3MgNi14 during Hydrogen Absorption–Desorption Process
Structural parameters of Pr3MgNi14 after a cyclic hydrogen absorption–desorption process were investigated by X-ray diffraction. Pr3MgNi14 consisted of two phases: 80% Gd2Co7-type structure and 20% PuNi3-type structure. The pressure–composition (P–C) isotherm of Pr3MgNi14 indicates a maximum hydrogen capacity of 1.12 H/M (1.61 mass %) at 298 K. The cyclic property of Pr3MgNi14 up to 1000 cycles was measured at 313 K. The retention rate of the sample was 87.5% at 1000 cycles, which compares favorably with that of LaNi5. After 1000 cycles, the expansions of lattice parameters a and c and the lengths along the c-axes of the PrNi5 and PrMgNi4 cells of the Gd2Co7-type structures were 0.20%, 1.26%, 0.47%, and 3.68%, respectively. The metal sublattice expanded anisotropically after the cyclic test. The isotropic and anisotropic lattice strains can be refined by Rietveld analysis. The anisotropic and isotropic lattice strains were almost saturated at the first activation process and reached values of 0.2% and 0.1%, respectively, after 1000 cycles. These values are smaller by 1 order of magnitude than those of LaNi5.
- 14 January 2012
- Published by International Union of Crystallography (IUCr) in Journal of Applied Crystallography
- Vol. 45 (1) , 113-118
In situlattice strain mapping during tensile loading using the neutron transmission and diffraction methods
In this study, the change in internal lattice strain in an iron plate during tensile deformation was investigated by performingin situmeasurements under applied force. The lattice strain was evaluated by neutron diffraction and Bragg-edge transmission. The neutron diffraction results showed that the averaged 110 lattice strain along the direction perpendicular to the applied force was between −422 and −109 × 10−6. The position dependence of the lattice strain and the change in the distribution of elastic strain in an iron plate with notches during tensile deformation was obtained by Bragg-edge transmission. It was also observed that, when the load increased over 30 kN, the area of plastic deformation increased around the positions of the notches.
- 14 January 2012
- Published by International Union of Crystallography (IUCr) in Journal of Applied Crystallography
- Vol. 45 (1) , 113-118
In situlattice strain mapping during tensile loading using the neutron transmission and diffraction methods
In this study, the change in internal lattice strain in an iron plate during tensile deformation was investigated by performingin situmeasurements under applied force. The lattice strain was evaluated by neutron diffraction and Bragg-edge transmission. The neutron diffraction results showed that the averaged 110 lattice strain along the direction perpendicular to the applied force was between −422 and −109 × 10−6. The position dependence of the lattice strain and the change in the distribution of elastic strain in an iron plate with notches during tensile deformation was obtained by Bragg-edge transmission. It was also observed that, when the load increased over 30 kN, the area of plastic deformation increased around the positions of the notches.
- 17 October 2011
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 50 (22) , 11631-11635
Synthesis of New Compound Gd5Ni19 with a Superlattice Structure and Hydrogen Absorption Properties
We successfully synthesized the new intermetallic compound Gd5Ni19 and determined its crystal structure by X-ray diffraction (XRD) and scanning transmission electron microscopy (STEM). The structure is a Sm5Co19-type superlattice structure (2H, space group P63/mmc), and the lattice parameters were determined as a = 0.4950(1) nm and c = 3.2161(5) nm by X-ray Rietveld refinement. The XRD results agreed with the STEM analysis results. The P–C isotherm of Gd5Ni19 was measured at 233 K. In the first absorption cycle, the maximum hydrogen capacity reached 1.07 H/M at 2.0 MPa. The sloping plateau was observed in the first absorption–desorption cycle. The maximum hydrogen capacity decreased by 0.87 H/M in the second absorption cycle, implying that hydrogen in the amount of H/M = 0.20 remained in the alloy before the second absorption–desorption cycle.
- 17 October 2011
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 50 (22) , 11631-11635
Synthesis of New Compound Gd5Ni19 with a Superlattice Structure and Hydrogen Absorption Properties
We successfully synthesized the new intermetallic compound Gd5Ni19 and determined its crystal structure by X-ray diffraction (XRD) and scanning transmission electron microscopy (STEM). The structure is a Sm5Co19-type superlattice structure (2H, space group P63/mmc), and the lattice parameters were determined as a = 0.4950(1) nm and c = 3.2161(5) nm by X-ray Rietveld refinement. The XRD results agreed with the STEM analysis results. The P–C isotherm of Gd5Ni19 was measured at 233 K. In the first absorption cycle, the maximum hydrogen capacity reached 1.07 H/M at 2.0 MPa. The sloping plateau was observed in the first absorption–desorption cycle. The maximum hydrogen capacity decreased by 0.87 H/M in the second absorption cycle, implying that hydrogen in the amount of H/M = 0.20 remained in the alloy before the second absorption–desorption cycle.
- 18 April 2011
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 50 (10) , 4548-4552
Synthesis and Crystal Structure of a Pr5Ni19 Superlattice Alloy and Its Hydrogen Absorption–Desorption Property
The intermetallic compound Pr5Ni19, which is not shown in the Pr–Ni binary phase diagram, was synthesized, and the crystal structure was investigated by X-ray diffraction (XRD) and transmission electron microscopy (TEM). Two superlattice reflections with the Sm5Co19-type structure (002 and 004) and the Pr5Co19-type structure (003 and 006) were observed in the 2θ region between 2° and 15° in the XRD pattern using Cu Kα radiation. Rietveld refinement provided the goodness-of-fit parameter S = 6.7 for the Pr5Co19-type (3R) structure model and S = 1.7 for the Sm5Co19-type (2H) structure model, indicating that the synthesized compound has a Sm5Co19 structure. The refined lattice parameters were a = 0.50010(9) nm and c = 3.2420(4) nm. The high-resolution TEM image also clearly revealed that the crystal structure of Pr5Ni19 is of the Sm5Co19 type, which agrees with the results from Rietveld refinement of the XRD data. The P–C isotherm of Pr5Ni19 in the first absorption was clearly different from that in the first desorption. A single plateau in absorption and three plateaus in desorption were observed. The maximum hydrogen storage capacity of the first cycle reached 1.1 H/M, and that of the second cycle was 0.8 H/M. The 0.3 H/M of hydrogen remained in the metal lattice after the first desorption process.
- 18 April 2011
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 50 (10) , 4548-4552
Synthesis and Crystal Structure of a Pr5Ni19 Superlattice Alloy and Its Hydrogen Absorption–Desorption Property
The intermetallic compound Pr5Ni19, which is not shown in the Pr–Ni binary phase diagram, was synthesized, and the crystal structure was investigated by X-ray diffraction (XRD) and transmission electron microscopy (TEM). Two superlattice reflections with the Sm5Co19-type structure (002 and 004) and the Pr5Co19-type structure (003 and 006) were observed in the 2θ region between 2° and 15° in the XRD pattern using Cu Kα radiation. Rietveld refinement provided the goodness-of-fit parameter S = 6.7 for the Pr5Co19-type (3R) structure model and S = 1.7 for the Sm5Co19-type (2H) structure model, indicating that the synthesized compound has a Sm5Co19 structure. The refined lattice parameters were a = 0.50010(9) nm and c = 3.2420(4) nm. The high-resolution TEM image also clearly revealed that the crystal structure of Pr5Ni19 is of the Sm5Co19 type, which agrees with the results from Rietveld refinement of the XRD data. The P–C isotherm of Pr5Ni19 in the first absorption was clearly different from that in the first desorption. A single plateau in absorption and three plateaus in desorption were observed. The maximum hydrogen storage capacity of the first cycle reached 1.1 H/M, and that of the second cycle was 0.8 H/M. The 0.3 H/M of hydrogen remained in the metal lattice after the first desorption process.
- 23 March 2011
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 42 (8) , 2296-2300
Position Dependence of SS304 and Iron Phases in Welded Specimen by Neutron Diffraction and Bragg-Edge Transmission Method
- 23 March 2011
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 42 (8) , 2296-2300
Position Dependence of SS304 and Iron Phases in Welded Specimen by Neutron Diffraction and Bragg-Edge Transmission Method
- 28 February 2011
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 36 (4) , 3062-3066
Development of sample holder for in situ neutron measurement of hydrogen absorbing alloy
- 28 February 2011
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 36 (4) , 3062-3066
Development of sample holder for in situ neutron measurement of hydrogen absorbing alloy
- 2 September 2010
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 49 (19) , 8763-8768
Phase Transformation and Crystal Structure of La2Ni7Hx Studied by in situ X-ray Diffraction
The phase transformation of La2Ni7 during hydrogenation was investigated by in situ X-ray diffraction. We found two hydride phases, La2Ni7H7.1 (phase I) and La2Ni7H10.8 (phase II), during the first absorption cycle. The metal sublattice of phase I was orthorhombic (space group Pbcn) with lattice parameters a = 0.50128(6) nm, b = 0.8702(1) nm, and c = 3.0377(1) nm. The sublattice for phase II was monoclinic (space group C2/c) with lattice parameters a = 0.51641(9) nm, b = 0.8960(1) nm, c = 3.1289(1) nm, and β = 90.17(1)°. The lattice parameter c increased with the hydrogen content, while a and b decreased in the formation of phase I from the alloy. Phase transformation from phase I to phase II was accompanied by isotropic expansion. The La2Ni4 and LaNi5 subunit expanded by 48.9% and 6.0% in volume, respectively, during hydrogenation to phase I. They expanded an additional 14% and 5.8%, respectively, in the formation of phase II. The obtained volume expansion suggested different hydrogen distribution in the La2Ni4 and LaNi5 subunit during hydrogenation.
- 2 September 2010
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 49 (19) , 8763-8768
Phase Transformation and Crystal Structure of La2Ni7Hx Studied by in situ X-ray Diffraction
The phase transformation of La2Ni7 during hydrogenation was investigated by in situ X-ray diffraction. We found two hydride phases, La2Ni7H7.1 (phase I) and La2Ni7H10.8 (phase II), during the first absorption cycle. The metal sublattice of phase I was orthorhombic (space group Pbcn) with lattice parameters a = 0.50128(6) nm, b = 0.8702(1) nm, and c = 3.0377(1) nm. The sublattice for phase II was monoclinic (space group C2/c) with lattice parameters a = 0.51641(9) nm, b = 0.8960(1) nm, c = 3.1289(1) nm, and β = 90.17(1)°. The lattice parameter c increased with the hydrogen content, while a and b decreased in the formation of phase I from the alloy. Phase transformation from phase I to phase II was accompanied by isotropic expansion. The La2Ni4 and LaNi5 subunit expanded by 48.9% and 6.0% in volume, respectively, during hydrogenation to phase I. They expanded an additional 14% and 5.8%, respectively, in the formation of phase II. The obtained volume expansion suggested different hydrogen distribution in the La2Ni4 and LaNi5 subunit during hydrogenation.