Sang-Won Kang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Sang-Won Kang has a total of 25 co-authors. Here are the top co-authors by number of shared publications:
Jin-Hyock Kim
Hynix Semiconductor Incorporated, Kyoungki-do 467-701, Korea
4 shared publicationsOh-Kyum Kwon
Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, Kusong-dong, Yusong-gu, Taejon 305-701, Korea
4 shared publicationsSe-Hun Kwon
Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, 335 Gwahangno, Yuseong-gu, Daejeon 305-701, Korea
4 shared publications- Ji-Hoon Ahn
Hanyang University
3 shared publications - Sung-Wook Kim
Nuclear Facility Cleanup Technology Division, Korea Atomic Energy Research Institute, 111 Daedeok-daero 989 Beon-gil, Yuseong-gu, Daejeon 34057, Republic of Korea
3 shared publications Ja-Yong Kim
Hynix Semiconductor Incorporated, Kyoungki-do 467-701, Korea
2 shared publications
Latest Publications
- 1 January 2009
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 12 (3) , H77-H79
Enhancement of the TiO[sub 2] Thin-Film Dielectric Constant Through Pretreatment of Ir Substrate
Films were deposited via plasma-enhanced atomic layer deposition on an Ir electrode. The phase of the films on the Ir electrode were changed from anatase to anatase and rutile multiphases with oxygen plasma time due to oxidation of Ir surface to , resulting in the increase of dielectric constant (from 50 to 83). In order to improve the rutile crystallinity, seed layer was formed by annealing at for in ambient oxygen before films deposition. As a result, the rutile crystallinity of films was enhanced and its dielectric constant increased to 90.
- 1 January 2009
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 12 (3) , H77-H79
Enhancement of the TiO[sub 2] Thin-Film Dielectric Constant Through Pretreatment of Ir Substrate
Films were deposited via plasma-enhanced atomic layer deposition on an Ir electrode. The phase of the films on the Ir electrode were changed from anatase to anatase and rutile multiphases with oxygen plasma time due to oxidation of Ir surface to , resulting in the increase of dielectric constant (from 50 to 83). In order to improve the rutile crystallinity, seed layer was formed by annealing at for in ambient oxygen before films deposition. As a result, the rutile crystallinity of films was enhanced and its dielectric constant increased to 90.
- 1 January 2009
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 12 (2) , G5-G8
Enhanced Dielectric Properties of SrTiO[sub 3] Films with a SrRuO[sub 3] Seed by Plasma-Enhanced Atomic Layer Deposition
The dielectric properties of thin films deposited on seed layer were investigated. The thin films were deposited by plasma-enhanced atomic layer deposition using and as precursors and plasma as an oxidant. The seed layer was formed through deposition of an SrO layer on a substrate and postannealing in ambient. As a result of introducing seed layers, the dielectric constant of thick thin films increased to 83 compared with that of 16 and 50 for film deposited on Ru directly and seed formed on Ru substrate, respectively.
- 1 January 2009
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 12 (2) , G5-G8
Enhanced Dielectric Properties of SrTiO[sub 3] Films with a SrRuO[sub 3] Seed by Plasma-Enhanced Atomic Layer Deposition
The dielectric properties of thin films deposited on seed layer were investigated. The thin films were deposited by plasma-enhanced atomic layer deposition using and as precursors and plasma as an oxidant. The seed layer was formed through deposition of an SrO layer on a substrate and postannealing in ambient. As a result of introducing seed layers, the dielectric constant of thick thin films increased to 83 compared with that of 16 and 50 for film deposited on Ru directly and seed formed on Ru substrate, respectively.
- 1 January 2008
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 155 (5) , H296-H300
Initial Stages of Ruthenium Film Growth in Plasma-Enhanced Atomic Layer Deposition
The initial stages of ruthenium film growth in plasma-enhanced atomic layer deposition (PEALD) on titanium nitride (TiN) substrate were investigated in detail. During the initial stages of ruthenium film growth, the influence of the substrate surface was significant and controlling thickness by counting the number of deposition cycles is no longer valid. The time required for saturated adsorption of as well as the amount of deposited ruthenium atoms per cycle changed during the initial stage. The time required for saturated adsorption of on homogeneous ruthenium surfaces was 7 s. However, it increased up to 25 s during the initial stage of the ruthenium film growth where the film growth on heterogeneous TiN substrate is dominant. By considering these changes during the initial stages of ruthenium PEALD growth, the full coverage of PEALD ruthenium can be obtained at a minimum thickness of 2.7 nm.
- 1 January 2008
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 155 (5) , H296-H300
Initial Stages of Ruthenium Film Growth in Plasma-Enhanced Atomic Layer Deposition
The initial stages of ruthenium film growth in plasma-enhanced atomic layer deposition (PEALD) on titanium nitride (TiN) substrate were investigated in detail. During the initial stages of ruthenium film growth, the influence of the substrate surface was significant and controlling thickness by counting the number of deposition cycles is no longer valid. The time required for saturated adsorption of as well as the amount of deposited ruthenium atoms per cycle changed during the initial stage. The time required for saturated adsorption of on homogeneous ruthenium surfaces was 7 s. However, it increased up to 25 s during the initial stage of the ruthenium film growth where the film growth on heterogeneous TiN substrate is dominant. By considering these changes during the initial stages of ruthenium PEALD growth, the full coverage of PEALD ruthenium can be obtained at a minimum thickness of 2.7 nm.
- 1 January 2008
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 155 (11) , H885-H888
Improvement of Copper Diffusion Barrier Properties of Tantalum Nitride Films by Incorporating Ruthenium Using PEALD
Ru-incorporated TaN (Ru–TaN) films were investigated as a Cu diffusion barrier material. Ru–TaN films were prepared by sequential deposition of Ru and TaN using plasma-enhanced atomic layer deposition (PEALD). The film composition was controlled by the number of Ru unit cycles. While the resistivity of Ru–TaN films was increased abruptly at low Ru composition (∼0.06)(∼0.06) , the resistivity of Ru–TaN films was decreased gradually as the Ru composition increased after that composition. The crystal structures of Ru–TaN films were amorphous at the Ru composition range from 0.19 to 0.52 due to disturbance of grain growth. However, the Ru–TaN films had TaN-like structure below this range and Ru-like structure above this range. The amorphous Ru–TaN films had nanocrystallite embedded structure in an amorphous matrix. This amorphous Ru–TaN barrier showed a better Cu diffusion barrier property (∼700°C)(∼700°C) than the TaN barrier (∼650°C)(∼650°C) because the Cu diffusion through the grain boundary was suppressed by the amorphization. In addition, the Ru–TaN barrier exhibited good adhesion to both Cu and SiO2SiO2 .
- 1 January 2008
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 155 (11) , H885-H888
Improvement of Copper Diffusion Barrier Properties of Tantalum Nitride Films by Incorporating Ruthenium Using PEALD
Ru-incorporated TaN (Ru–TaN) films were investigated as a Cu diffusion barrier material. Ru–TaN films were prepared by sequential deposition of Ru and TaN using plasma-enhanced atomic layer deposition (PEALD). The film composition was controlled by the number of Ru unit cycles. While the resistivity of Ru–TaN films was increased abruptly at low Ru composition (∼0.06)(∼0.06) , the resistivity of Ru–TaN films was decreased gradually as the Ru composition increased after that composition. The crystal structures of Ru–TaN films were amorphous at the Ru composition range from 0.19 to 0.52 due to disturbance of grain growth. However, the Ru–TaN films had TaN-like structure below this range and Ru-like structure above this range. The amorphous Ru–TaN films had nanocrystallite embedded structure in an amorphous matrix. This amorphous Ru–TaN barrier showed a better Cu diffusion barrier property (∼700°C)(∼700°C) than the TaN barrier (∼650°C)(∼650°C) because the Cu diffusion through the grain boundary was suppressed by the amorphization. In addition, the Ru–TaN barrier exhibited good adhesion to both Cu and SiO2SiO2 .
- 1 January 2008
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 11 (11) , H303-H305
Improvement of Morphological Stability of PEALD-Iridium Thin Films by Adopting Two-Step Annealing Process
Plasma-enhanced atomic layer deposition (PEALD) of iridium (Ir) films was investigated using Ir(EtCp)(COD) and plasma. Deposited Ir films had smooth surface and preferred (111) orientation. After simple annealing in ambient oxygen, surface roughening occurred because Ir was oxidized above , and the oxidized during temperature rising was reduced to Ir at . However, by adopting two-step annealing, Ir films showed excellent thermal and morphological stability at . During two-step annealing at , the oxidation during temperature rising was suppressed by supplying argon, and annealing in ambient oxygen progressed after the temperature reached .
- 1 January 2008
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 11 (11) , H303-H305
Improvement of Morphological Stability of PEALD-Iridium Thin Films by Adopting Two-Step Annealing Process
Plasma-enhanced atomic layer deposition (PEALD) of iridium (Ir) films was investigated using Ir(EtCp)(COD) and plasma. Deposited Ir films had smooth surface and preferred (111) orientation. After simple annealing in ambient oxygen, surface roughening occurred because Ir was oxidized above , and the oxidized during temperature rising was reduced to Ir at . However, by adopting two-step annealing, Ir films showed excellent thermal and morphological stability at . During two-step annealing at , the oxidation during temperature rising was suppressed by supplying argon, and annealing in ambient oxygen progressed after the temperature reached .
- 1 April 2007
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 101 (7) , 073502
Step coverage modeling of thin films in atomic layer deposition
A film growth model on microfeatures is proposed to evaluate step coverage depending on precursor injection time in atomic layer deposition. The proposed model is based on that the chemisorption rate of precursors at a certain position along the depth of a microfeature is determined by the total flux of precursors and the sticking probability. The total flux includes the flux coming from the entrance of a microfeature and the flux reflected from other positions inside a microfeature, and the sticking probability depends on the surface coverage of chemisorbed precursor, which is a function of precursor injection time. The proposed model was applied to the deposition of Al2O3 films on 0.3μm diameter holes with an aspect ratio of 10. It was confirmed that the experimental data for step coverage depending on precursor injection time follow the trend predicted by the proposed model.
- 1 April 2007
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 101 (7) , 073502
Step coverage modeling of thin films in atomic layer deposition
A film growth model on microfeatures is proposed to evaluate step coverage depending on precursor injection time in atomic layer deposition. The proposed model is based on that the chemisorption rate of precursors at a certain position along the depth of a microfeature is determined by the total flux of precursors and the sticking probability. The total flux includes the flux coming from the entrance of a microfeature and the flux reflected from other positions inside a microfeature, and the sticking probability depends on the surface coverage of chemisorbed precursor, which is a function of precursor injection time. The proposed model was applied to the deposition of Al2O3 films on 0.3μm diameter holes with an aspect ratio of 10. It was confirmed that the experimental data for step coverage depending on precursor injection time follow the trend predicted by the proposed model.
- 1 January 2007
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 154 (12) , H1008-H1013
Applicability of Step-Coverage Modeling to TiO[sub 2] Thin Films in Atomic Layer Deposition
The applicability of a step-coverage model in atomic layer deposition was extended to the deposition of TiO2TiO2 films, focusing on the effect of a precursor partial pressure and a deposition temperature, as well as the number of cycles in step coverage. Using the extracted model parameters, step coverage depending on the number of cycles was predicted, which shows a nonlinear dependence of film thickness inside a hole on the number of cycles because the area of a hole entrance decreases as the deposition proceeds. The experimental data agreed well with the model predictions. To confirm the validity of the step-coverage model, the effect of a precursor partial pressure and a deposition temperature on step coverage was also investigated. The flux of precursors that strikes the flat surface is the model parameter related to a precursor partial pressure, and the initial sticking probability and the adsorption order are the model parameters related to a deposition temperature. For different experimental conditions, by obtaining the model parameters related to changed experimental conditions from the experimental data at the flat surface, film thickness per cycle at the bottom inside a hole depending on precursor injection time could be predicted within reasonable accuracy.
- 1 January 2007
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 154 (12) , H1008-H1013
Applicability of Step-Coverage Modeling to TiO[sub 2] Thin Films in Atomic Layer Deposition
The applicability of a step-coverage model in atomic layer deposition was extended to the deposition of TiO2TiO2 films, focusing on the effect of a precursor partial pressure and a deposition temperature, as well as the number of cycles in step coverage. Using the extracted model parameters, step coverage depending on the number of cycles was predicted, which shows a nonlinear dependence of film thickness inside a hole on the number of cycles because the area of a hole entrance decreases as the deposition proceeds. The experimental data agreed well with the model predictions. To confirm the validity of the step-coverage model, the effect of a precursor partial pressure and a deposition temperature on step coverage was also investigated. The flux of precursors that strikes the flat surface is the model parameter related to a precursor partial pressure, and the initial sticking probability and the adsorption order are the model parameters related to a deposition temperature. For different experimental conditions, by obtaining the model parameters related to changed experimental conditions from the experimental data at the flat surface, film thickness per cycle at the bottom inside a hole depending on precursor injection time could be predicted within reasonable accuracy.
- 1 January 2007
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 154 (9) , H773-H777
Improvement of the Morphological Stability by Stacking RuO[sub 2] on Ru Thin Films with Atomic Layer Deposition
Stacked RuO2∕RuRuO2∕Ru structures were produced by atomic layer deposition (ALD) using an alternating supply of bis(ethylcyclopentadienyl)ruthenium [Ru(EtCp)2][Ru(EtCp)2] and O2O2 gas at a deposition temperature of 270°C270°C . The type of the deposited film, either Ru or RuO2RuO2 , was controlled by the total pressure in the ALD system as well as the ratio of the adsorbed Ru(EtCp)2Ru(EtCp)2 to the partial pressure of O2O2 in the following O2O2 gas pulse. The resistivity of the deposited Ru and RuO2RuO2 thin films was about 15 and 70μΩcm70μΩcm , respectively. The surface morphology of Ru films annealed in O2O2 ambient was seriously degraded by surface oxidation. Moreover, RuO2RuO2 films were also agglomerated due to the residual stress releasing during the annealing process. However, a stacked RuO2∕RuRuO2∕Ru structure produced using ALD maintained a smooth surface even at an annealing temperature of 800°C800°C in ambient O2O2 . Auger electron spectroscopy confirmed that the stacked RuO2∕RuRuO2∕Ru structure successfully blocked oxygen and silicon diffusion. Therefore, the stacked RuO2∕RuRuO2∕Ru structure produced by ALD is suitable for use as the bottom electrode material for high dielectric applications.
- 1 January 2007
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 154 (9) , H773-H777
Improvement of the Morphological Stability by Stacking RuO[sub 2] on Ru Thin Films with Atomic Layer Deposition
Stacked RuO2∕RuRuO2∕Ru structures were produced by atomic layer deposition (ALD) using an alternating supply of bis(ethylcyclopentadienyl)ruthenium [Ru(EtCp)2][Ru(EtCp)2] and O2O2 gas at a deposition temperature of 270°C270°C . The type of the deposited film, either Ru or RuO2RuO2 , was controlled by the total pressure in the ALD system as well as the ratio of the adsorbed Ru(EtCp)2Ru(EtCp)2 to the partial pressure of O2O2 in the following O2O2 gas pulse. The resistivity of the deposited Ru and RuO2RuO2 thin films was about 15 and 70μΩcm70μΩcm , respectively. The surface morphology of Ru films annealed in O2O2 ambient was seriously degraded by surface oxidation. Moreover, RuO2RuO2 films were also agglomerated due to the residual stress releasing during the annealing process. However, a stacked RuO2∕RuRuO2∕Ru structure produced using ALD maintained a smooth surface even at an annealing temperature of 800°C800°C in ambient O2O2 . Auger electron spectroscopy confirmed that the stacked RuO2∕RuRuO2∕Ru structure successfully blocked oxygen and silicon diffusion. Therefore, the stacked RuO2∕RuRuO2∕Ru structure produced by ALD is suitable for use as the bottom electrode material for high dielectric applications.
- 1 January 2006
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 9 (5) , F34-F37
Interfacial Layer Properties of HfO[sub 2] Films Formed by Plasma-Enhanced Atomic Layer Deposition on Silicon
The interfacial oxide layers, generated on Si substrates during the initial stage of atomic layer deposition (ALD), have been investigated depending on the oxygen reactants, oxygen plasma and water. In the plasma-enhanced ALD (PEALD) using oxygen plasma, a -thick interfacial layer, which was intermixed with Hf–Si–O and having a dielectric constant of 6.5, was formed, while water made a -thick interfacial layer composed mainly of . Additionally, by utilizing oxygen plasma, the of the film itself was increased up to 22.2 resulting in a higher effective , and a much lower leakage current density was also obtained.
- 1 January 2006
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 9 (5) , F34-F37
Interfacial Layer Properties of HfO[sub 2] Films Formed by Plasma-Enhanced Atomic Layer Deposition on Silicon
The interfacial oxide layers, generated on Si substrates during the initial stage of atomic layer deposition (ALD), have been investigated depending on the oxygen reactants, oxygen plasma and water. In the plasma-enhanced ALD (PEALD) using oxygen plasma, a -thick interfacial layer, which was intermixed with Hf–Si–O and having a dielectric constant of 6.5, was formed, while water made a -thick interfacial layer composed mainly of . Additionally, by utilizing oxygen plasma, the of the film itself was increased up to 22.2 resulting in a higher effective , and a much lower leakage current density was also obtained.
- 1 January 2006
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 153 (6) , G578-G581
Plasma-Enhanced Atomic Layer Deposition of Ru–TiN Thin Films for Copper Diffusion Barrier Metals
Ruthenium-titanium nitride (Ru–TiN) thin films were grown by plasma-enhanced atomic layer deposition (PEALD) at a growth temperature of 200°C200°C . For the Ru–TiN PEALD, Ru and TiN were sequentially deposited to intermix TiN with Ru. The composition of Ru–TiN films was controlled by changing the number of deposition cycles allocated to Ru, while the number of deposition cycles for TiN was fixed to one cycle. The microstructures of Ru–TiN films changed from polycrystalline to amorphous, as the intermixing ratio of Ru increased in the deposited Ru–TiN films. The resistivity of the Ru–TiN film was abruptly increased by adding Ru at the first stage, but after showing a peak resistivity, it decreased with the intermixing ratio of Ru in the films. Especially, the film of Ru0.67–(TiN)0.33Ru0.67–(TiN)0.33 showed an electrical resistivity of 190μΩcm190μΩcm . As a Cu diffusion barrier layer, amorphous Ru–TiN films showed a superior copper diffusion barrier property to TiN or Ru itself, which had a polycrystalline structure. Moreover, Ru–TiN films showed a good adhesion to both chemical vapor deposition copper and an underlayer of SiO2SiO2 .
- 1 January 2006
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 153 (6) , G578-G581
Plasma-Enhanced Atomic Layer Deposition of Ru–TiN Thin Films for Copper Diffusion Barrier Metals
Ruthenium-titanium nitride (Ru–TiN) thin films were grown by plasma-enhanced atomic layer deposition (PEALD) at a growth temperature of 200°C200°C . For the Ru–TiN PEALD, Ru and TiN were sequentially deposited to intermix TiN with Ru. The composition of Ru–TiN films was controlled by changing the number of deposition cycles allocated to Ru, while the number of deposition cycles for TiN was fixed to one cycle. The microstructures of Ru–TiN films changed from polycrystalline to amorphous, as the intermixing ratio of Ru increased in the deposited Ru–TiN films. The resistivity of the Ru–TiN film was abruptly increased by adding Ru at the first stage, but after showing a peak resistivity, it decreased with the intermixing ratio of Ru in the films. Especially, the film of Ru0.67–(TiN)0.33Ru0.67–(TiN)0.33 showed an electrical resistivity of 190μΩcm190μΩcm . As a Cu diffusion barrier layer, amorphous Ru–TiN films showed a superior copper diffusion barrier property to TiN or Ru itself, which had a polycrystalline structure. Moreover, Ru–TiN films showed a good adhesion to both chemical vapor deposition copper and an underlayer of SiO2SiO2 .