SOSung-Tag Oh

Sung-Tag Oh

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Sung-Tag Oh has a total of 72 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Non-Isothermal Reduction Behavior and Microstructural Characteristics of MoO3 Powder in Pure Hydrogen Atmosphere

    by Wonyong Kwon, Youngmin Kim, MinJu Son, Eui Seon Lee, Sung-Tag Oh

    The reduction behavior and microstructure of both raw and ball-milled MoO3 powders have been investigated. The raw powder consisted of coarse plate-shaped particles, whereas the powder ball-milled for 5 h showed agglomerates composed of fine equiaxed particles. XRD analysis of the hydrogen-reduced powders indicated that only the diffraction lines for Mo are observed. In contrast, the milled powder exhibited the main peak of Mo and carbides peak as minor phases. The reduction kinetics of MoO3 powders were evaluated by analyzing the extent of peak shift at various heating rates using thermogravimetric analysis. The activation energies for the raw powder were determined to range from 97.5 to 104.4 kJ/mol, which are approximately consistent with the values reported for the isothermal reduction of MoO3 in a hydrogen atmosphere. For the ball-milled powders, the activation energy was measured to be 148.8–167.1 kJ/mol, which was interpreted to be related to the carbides formed by the reaction of Fe and C impurities with Mo.

  • Open Access

    Enhancing Filtration Performance of Sintered Metal Filters Through Pore Structure Modification using Fine Flake-Shaped Particles

    by Dong Hoon Lee, Kyung-Shik Yoon, Hee Yeon Jeon, Jeong Hyun Kim, Jung-Yeul Yun, Sung-Tag Oh, Young-In Lee

    Sintered metal gas filters commonly suffer from a trade-off between filtration efficiency and gas permeability due to limited control over pore structure. In this study, fine flake-shaped stainless steel 316L powders were introduced into a sintered filter matrix to modify pore geometry without significantly reducing porosity. Microstructural and pore analyses showed that flake addition subdivided interparticle voids, leading to reduced pore size while maintaining high open porosity at low flake contents. Notably, the filter containing 1 wt.% flake-shaped powder exhibited a clear improvement in filtration efficiency without a pronounced increase in pressure drop. At higher flake contents, further gains in filtration efficiency were accompanied by a rapid increase in flow resistance. This work demonstrates that the controlled incorporation of fine flake-shaped powders provides a simple and scalable approach to pore-structure engineering for high-performance metal gas filters.

  • Open Access

    Effect of Powder Preparation Method on the Microstructural Characteristics of Sintered W-7Ni-3Cu Heavy Alloy

    by Youngmin Kim, Ji Young Kim, Minju Son, Wonyong Kwon, Eui Seon Lee, Sung-Tag Oh

    The effect of powder characteristics and sintering temperature on the properties of W-7Ni-3Cu is investigated. The heavy alloy powders were prepared by ball milling and hydrogen reduction of elemental metal or metal oxide powders. Microstructural analysis revealed that the powder mixtures reduced by hydrogen at 800oC consist of a trace amount of Ni4W phase along with the metal W phase and Ni-Cu solid solution. Additionally, compared to metal powder, the powder mixture using oxide as raw material exhibited a relatively fine particle size. The W-7Ni-3Cu alloys sintered using oxide powders had relative density of over 99%, whereas the specimens using metal powders as a raw material showed relatively low values of 87.8~98.2%. The Vickers hardness of the sintered specimens using oxide powder was 3.34–3.92 GPa, which was higher than that of 2.39–3.22 GPa measured when using metal powders. The observed results can be attributed to the relatively high density and the reduced grain size.

  • Open Access

    Preparation of Porous W-Cu by Freeze Casting of Tert-butyl Alcohol Slurry Mixed with WO3-CuO Powder

    by Youngmin Kim, Ji Young Kim, Minju Son, Wonyong Kwon, Eui Seon Lee, Sung-Tag Oh

    The influence of process conditions on the microstructure of porous W-Cu, fabricated by freeze casting using tert-butyl alcohol as the freezing agent, was investigated. The slurries containing 10 vol% of WO3-CuO powder were prepared by milling with a small amount of citric acid and polyethylene glycol as dispersants. The slurries with dispersion stability were frozen in a mold with the lower part cooled to -25°C, followed by sublimation in a vacuum to remove the freezing agent. The sintered W-1 vol% Cu in a hydrogen atmosphere exhibited aligned pores with the size of 50 μm, which were generated by sublimation of directionally solidified tert-butyl alcohol crystals. In the cross-section of the specimen, hexagonal pores corresponding to the crystal structure of tert-butyl alcohol was observed. Microstructure analysis of the struts revealed that Cu was distributed non-uniformly due to the mutual insolubility and low wettability of the W-Cu system.

  • Preparation of W-Cu Composite Powders by Hydrogen Reduction of WO3 And Copper Nitrate Mixture

    by Ji Won Choi, Ji Young Kim, Youngmin Kim, Eui Seon Lee, Sung-Tag Oh

    The synthesis of fine W composite powder with homogeneously dispersed Cu particles was investigated. Commercial or ultrasonic spray pyrolysis WO3 powders were used as source materials of W, and copper nitrate was added and hydrogen-reduced to finally fabricate W-Cu composite powder. The reduced powder prepared using ultrasonic spray pyrolysis WO3 powder exhibited a spherical agglomerate composed of fine particles and pores, whereas that using commercial WO3 showed relatively fine particles with a size of about 200 nm. TEM analysis revealed that Cu elements were uniformly distributed in the composite powder. These results help to optimize the synthesis process of homogeneous W-Cu nanocomposite powders.


  • Morphology Modification of MoO3 Powders by Hydrogen Reduction and Re-Oxidation Process

    by Youngmin Kim, Ji Young Kim, Ji Won Choi, Eui Seon Lee, Sung-Tag Oh

    An optimum route to fabricate the MoO3 nanoparticles with modified morphology was investigated. Microstructure analysis for the MoO3 powder prepared by high-energy ball milling process for 25 h showed that the plate-shaped raw powders are mostly converted into equiaxed fine particles, but exist as large agglomerates. However, the powder fabricated by the hydrogen reduction at 775℃ of raw powder and re-oxidation at 450℃ exhibits equiaxed fine particles with a size of about 260 nm and relatively small agglomerates. Additionally, the re-oxidized particles show a unimodal particle size distribution with measured values ranging from 0.18 to 0.42 μm. These results indicated that the reduction and re-oxidation process can significantly decrease the particle size and modify the powder morphology into an equiaxed shape.

  • Preparation and characterisation of W–7Ni–3Cu alloy powder by hydrogen reduction of metal oxides

    by Youn Ji Heo, Eui Seon Lee, Jongmin Byun, Sung-Tag Oh

    The microstructural characteristics and hydrogen reduction behaviour of W–7Ni–3Cu heavy alloy powders synthesised from WO 3 –NiO–CuO powder mixtures have been investigated. The fine and homogeneous oxide powder mixture is prepared by ball milling using stearic acid as a process control agent. The reduction behaviour of oxide powders is interpreted by thermogravimetric analysis in an N 2 –10% H 2 atmosphere. After milling for 5 h and hydrogen reduction at 800 °C, the oxide powders were completely converted to W, NiCu, and Ni 4 W phases without residual oxides and showed an average particle size of about 200 nm. The reduction kinetics is evaluated by the amount of peak shift in the thermogravimetric curves depending on the heating rates. The apparent activation energies for the reduction of CuO, NiO and WO 3 , estimated by the slope of the Kissinger plot, are measured as 96.9 kJ/mol, 122.0 kJ/mol and 114.6–124.3 kJ/mol, respectively. The measured activation energy is considered meaningful for quantitatively analysing the reduction kinetics in the non-isothermal reduction process of oxide composite powders.


  • Fabrication of porous W by freeze-casting and hydrogen reduction of camphene-based WO 3 suspension

    by Ji Won Choi, Youngmin Kim, Ji Young Kim, Eui Seon Lee, Sung-Tag Oh

    In this research, freeze-casting and sintering processes were applied to fabricate porous W with macroscopically aligned pores. Initially, the raw WO 3 powder was ball-milled for 5 h to remove large agglomerates, resulting in an unimodal distribution with an average size of 250 nm. The homogeneous suspension with dispersion stability can be prepared by adding oligomeric polyester as a dispersant. After unidirectional freeze-casting of camphene suspension and sintering in a hydrogen atmosphere, the green body was completely converted to porous W. The sintered W showed that aligned large pores were generated by sublimation of directionally solidified camphene crystals. The pore size of the sintered W decreased with increasing content of solid particles, and larger pore sizes were observed in the upper region than at the bottom of all specimens. Changes in pore size have been interpreted as differences in the solidification behavior of the suspension, such as the degree of redistribution of solid particles and the solidification velocity at the freezing front.

  • Open Access

    Fabrication of Porous TiO2 with Aligned Pores Using Tert-Butyl Alcohol Based Freeze Casting

    by Eui Seon Lee, Sung-Tag Oh

    The effect of freezing conditions on the pore structure of porous TiO2 fabricated using a freeze casting process with tert-butyl alcohol slurry was investigated. The raw powder was heat treated to manufacture a porous body with stable shape by suppressing volume change induced by the phase transformation of TiO2 powder. The XRD analysis result indicated that the anatase phase fraction in the raw powder could be converted to 98.6% rutile phase by heating it at 800°C for 30 min. Porous TiO2 ceramics with unidirectionally aligned pore channels were prepared by freezing tert-butyl alcohol slurry containing 10 vol% TiO2 powder under different freezing temperatures of -20, -30 and -40°C, respectively. After removing the frozen tert-butyl alcohol by sublimation in vacuum, the green samples were sintered at 1100°C for 4 h in air. The porous body contains directional pores with a size of approximately 30 µm, and a hexagonal pore shape corresponding to the crystal structure of tert-butyl alcohol was observed in the cross-section of the pores. Small pores were observed at the bottom part of the porous body near the Cu plate where the solidification heat was released, but relatively large pores were present at the upper part. Both microstructure observation and pore size distribution indicated that the pore size and the strut thickness increased significantly with increasing freezing temperature. The change in pore characteristics was explained as being mainly due to the difference in the solidification behavior of the slurry and the rearrangement of the solid powder.