Jun Hwan Kim
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Jun Hwan Kim has a total of 27 co-authors. Here are the top co-authors by number of shared publications:
Byoung Oon Lee
Korea Atomic Energy Research Institute
2 shared publicationsChan Bock Lee
Korea Atomic Energy Research Institute
2 shared publications- Hyeong Min Heo
Gwangju center, Korea Basic Science Institute, 77 Yongbong-ro, Buk-gu, Gwangju 61186, Korea
2 shared publications - Jin-Sik Cheon
Korea Atomic Energy Research Institute
2 shared publications - Jongryoul Kim
Hanyang University
2 shared publications - Sung Ho Kim
Advanced Fuel Development Division, Korea Atomic Energy Research Institute, Daejeon, Republic of Korea
2 shared publications
Latest Publications
- Open Access
Applicability of Swaging as an Alternative for the Fabrication of Accident-Tolerant Fuel Cladding
We suggest an alternative to conventional coating methods for accident-tolerant fuel (ATF) cladding. A Zircaloy-4 tube was inserted into metal tubes of different materials and the inserted tubes were subjected to physical force at room temperature. The manufactured tube exhibited a pseudo-single tube (PST) structure and had higher thermal stability than a Zircaloy-4 tube. Optical microscopy and scanning electron microscopy images showed that the PST had a uniform and well-bonded interface structure, i.e., no gaps or voids were found at the interface between the inner and outer tubes. Energy-dispersive X-ray spectroscopy analysis confirmed that the metal components did not interdiffuse at the interface of the PST, even after being kept at 600 and 900 °C for 1 h and rapidly cooled to room temperature. Unlike pure Zircaloy-4 tubes, Zircaloy-4/stainless use steel (SUS) 316 PST did not show significant structural collapse, even after being stored at 1200 °C for 1 h. Based on these results, if a PST was fabricated using a Zircaloy-4 tube thinner than the Zircaloy-4 tube used in this study and an outer tube of micron-scale thickness, swaging may be a feasible alternative to Zircaloy-4-based ATF cladding.
Open AccessApplicability of Swaging as an Alternative for the Fabrication of Accident-Tolerant Fuel Cladding
We suggest an alternative to conventional coating methods for accident-tolerant fuel (ATF) cladding. A Zircaloy-4 tube was inserted into metal tubes of different materials and the inserted tubes were subjected to physical force at room temperature. The manufactured tube exhibited a pseudo-single tube (PST) structure and had higher thermal stability than a Zircaloy-4 tube. Optical microscopy and scanning electron microscopy images showed that the PST had a uniform and well-bonded interface structure, i.e., no gaps or voids were found at the interface between the inner and outer tubes. Energy-dispersive X-ray spectroscopy analysis confirmed that the metal components did not interdiffuse at the interface of the PST, even after being kept at 600 and 900 °C for 1 h and rapidly cooled to room temperature. Unlike pure Zircaloy-4 tubes, Zircaloy-4/stainless use steel (SUS) 316 PST did not show significant structural collapse, even after being stored at 1200 °C for 1 h. Based on these results, if a PST was fabricated using a Zircaloy-4 tube thinner than the Zircaloy-4 tube used in this study and an outer tube of micron-scale thickness, swaging may be a feasible alternative to Zircaloy-4-based ATF cladding.
- Open Access
Influence of Heat Treatment on the Workability of Modified 9Cr-2W Steel with Higher B Content
In this study, the effect of heat treatment on the fracture behavior of alloy B steel with boron (B) contents as high as 130 ppm was investigated. The Alloy B are derived from Gr.92 steel with outstanding creep characteristics. The amounts of minor alloying elements such as B, N, Nb, Ta, and C were optimized to achieve better mechanical properties at high temperatures. Hence, workability of the alloy B and Gr.92 were compared. An increase in the B content affected the phase transformation temperature and texture of the steel. The development of the {111} components in γ-fibers depended on the austenite fraction of the steel after the phase transformation. An increase in the B content of the steel increased its α-to-γ phase transformation temperature, thus preventing the occurrence of sufficient transformation under the normalizing condition. Cracks occurred at the point of the elastic-to-plastic deformation transition in the normal direction during the rolling process, thereby resulting in failure. Therefore, it is necessary to avoid intermediate heat treatment conditions, in which γ-fibers do not fully develop, i.e., to avoid an imperfect normalization.
Open AccessInfluence of Heat Treatment on the Workability of Modified 9Cr-2W Steel with Higher B Content
In this study, the effect of heat treatment on the fracture behavior of alloy B steel with boron (B) contents as high as 130 ppm was investigated. The Alloy B are derived from Gr.92 steel with outstanding creep characteristics. The amounts of minor alloying elements such as B, N, Nb, Ta, and C were optimized to achieve better mechanical properties at high temperatures. Hence, workability of the alloy B and Gr.92 were compared. An increase in the B content affected the phase transformation temperature and texture of the steel. The development of the {111} components in γ-fibers depended on the austenite fraction of the steel after the phase transformation. An increase in the B content of the steel increased its α-to-γ phase transformation temperature, thus preventing the occurrence of sufficient transformation under the normalizing condition. Cracks occurred at the point of the elastic-to-plastic deformation transition in the normal direction during the rolling process, thereby resulting in failure. Therefore, it is necessary to avoid intermediate heat treatment conditions, in which γ-fibers do not fully develop, i.e., to avoid an imperfect normalization.
- Open Access
Evaluation of Workability on the Microstructure and Mechanical Property of Modified 9Cr-2W Steel for Fuel Cladding by Cold Drawing Process and Intermediate Heat Treatment Condition
In this study, we evaluated the cold drawing workability of two kinds of modified 9Cr-2W steel containing different contents of boron and nitrogen depending on the temperature and time of normalizing and tempering treatments. Using ring compression tests at room temperature, the effect of intermediate heat treatment condition on workability was investigated. It was found that the prior austenite grain size can be changed by the austenite transformation and that the grain size increases with increasing temperature during normalizing heat treatment. Alloy B and Alloy N showed different patterns after normalizing heat treatment. Alloy N had higher stress than Alloy B, and the reduction in alloy N increased while the reduction in alloy B decreased. Alloy B showed a larger number of initially formed cracks and a larger average crack length than Alloy N. Crack length and number increased proportionally in Alloy B as the stress increased. Alloy B had lower crack resistance than Alloy N due to boron segregation.
Open AccessEvaluation of Workability on the Microstructure and Mechanical Property of Modified 9Cr-2W Steel for Fuel Cladding by Cold Drawing Process and Intermediate Heat Treatment Condition
In this study, we evaluated the cold drawing workability of two kinds of modified 9Cr-2W steel containing different contents of boron and nitrogen depending on the temperature and time of normalizing and tempering treatments. Using ring compression tests at room temperature, the effect of intermediate heat treatment condition on workability was investigated. It was found that the prior austenite grain size can be changed by the austenite transformation and that the grain size increases with increasing temperature during normalizing heat treatment. Alloy B and Alloy N showed different patterns after normalizing heat treatment. Alloy N had higher stress than Alloy B, and the reduction in alloy N increased while the reduction in alloy B decreased. Alloy B showed a larger number of initially formed cracks and a larger average crack length than Alloy N. Crack length and number increased proportionally in Alloy B as the stress increased. Alloy B had lower crack resistance than Alloy N due to boron segregation.
- Open Access
Results of High-Temperature Heating Test for Irradiated U-10Zr(-5Ce) with T92 Cladding Fuel
A microstructure observation using an optical microscope, SEM and EPMA was performed for the irradiated U-10Zr and U-10Zr-5Ce fuel slugs with a T92 cladding specimen after a high-temperature heating test. Also, the measured eutectic penetration rate was compared with the value predicted by the existing eutectic penetration correlation being used for design and modeling purposes. The heating temperature and duration time for the U-10Zr/T92 specimen were 750 °C and 1 h, and those for the U-10Zr-5Ce/T92 specimen were 800 °C and 1 h. In the case of the U-10Zr/T92 specimen, the migration phenomena of U, Zr, Fe, and Cr as well as the Nd lanthanide fission product were observed at the eutectic melting region. The measured penetration rate was similar to the value predicted by the existing eutectic penetration rate correlation. In addition, when comparing with measured eutectic penetration rates for the unirradiated U-10Zr fuel slug with FMS (ferritic martensitic steel, HT9 or Gr.91) cladding specimens which had been reported in the literature, the measured eutectic penetration rate for the irradiated fuel specimen was higher than that for the unirradiated U-10Zr specimen. In the case of the U-10Zr-5Ce/T92 specimen in which there had been a gap between the fuel slug and cladding after the irradiation test, the eutectic melting region was not found because contact between the fuel slug and cladding did not take place during the heating test.
Open AccessResults of High-Temperature Heating Test for Irradiated U-10Zr(-5Ce) with T92 Cladding Fuel
A microstructure observation using an optical microscope, SEM and EPMA was performed for the irradiated U-10Zr and U-10Zr-5Ce fuel slugs with a T92 cladding specimen after a high-temperature heating test. Also, the measured eutectic penetration rate was compared with the value predicted by the existing eutectic penetration correlation being used for design and modeling purposes. The heating temperature and duration time for the U-10Zr/T92 specimen were 750 °C and 1 h, and those for the U-10Zr-5Ce/T92 specimen were 800 °C and 1 h. In the case of the U-10Zr/T92 specimen, the migration phenomena of U, Zr, Fe, and Cr as well as the Nd lanthanide fission product were observed at the eutectic melting region. The measured penetration rate was similar to the value predicted by the existing eutectic penetration rate correlation. In addition, when comparing with measured eutectic penetration rates for the unirradiated U-10Zr fuel slug with FMS (ferritic martensitic steel, HT9 or Gr.91) cladding specimens which had been reported in the literature, the measured eutectic penetration rate for the irradiated fuel specimen was higher than that for the unirradiated U-10Zr specimen. In the case of the U-10Zr-5Ce/T92 specimen in which there had been a gap between the fuel slug and cladding after the irradiation test, the eutectic melting region was not found because contact between the fuel slug and cladding did not take place during the heating test.
- 19 September 2014
- Published by Springer Nature in Metals and Materials International
- Vol. 20 (5) , 819-824
Interaction between multi-component lanthanide alloy and ferritic-martensitic steel
- 19 September 2014
- Published by Springer Nature in Metals and Materials International
- Vol. 20 (5) , 819-824
Interaction between multi-component lanthanide alloy and ferritic-martensitic steel
- 8 July 2013
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 443 (1-3) , 112-119
Microstructure and mechanical property of ferritic–martensitic steel cladding under a 650°C liquid sodium environment
- 8 July 2013
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 443 (1-3) , 112-119
Microstructure and mechanical property of ferritic–martensitic steel cladding under a 650°C liquid sodium environment
- Open Access
- 30 March 2012
- Published by The Korean Radioactive Waste Society in Journal of Nuclear Fuel Cycle and Waste Technology
- Vol. 10 (1) , 21-26
Evaluation of Microstructural and Mechanical Property of Medium-sized HT9 Cladding Forged Material for Sodium-cooled Fast Reactor
- 30 March 2012
- Published by The Korean Radioactive Waste Society in Journal of Nuclear Fuel Cycle and Waste Technology
- Vol. 10 (1) , 21-26
Open AccessEvaluation of Microstructural and Mechanical Property of Medium-sized HT9 Cladding Forged Material for Sodium-cooled Fast Reactor
- 25 July 2011
- Published by The Korean Institute of Metals and Materials in Korean Journal of Metals and Materials
- Vol. 49 (7) , 549-556
Effect of Vapor Deposition on the Interdiffusion Behavior between the Metallic Fuel and Clad Material
- 25 July 2011
- Published by The Korean Institute of Metals and Materials in Korean Journal of Metals and Materials
- Vol. 49 (7) , 549-556
Effect of Vapor Deposition on the Interdiffusion Behavior between the Metallic Fuel and Clad Material
- 28 January 2011
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 528 (10-11) , 3771-3776
Microstructure and hydride embrittlement of zirconium model alloys containing niobium and tin
- 28 January 2011
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 528 (10-11) , 3771-3776
Microstructure and hydride embrittlement of zirconium model alloys containing niobium and tin