Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Xingping Fan has a total of 15 co-authors. Here are the top co-authors by number of shared publications:

  • Bo Feng

    School of Materials Science and Engineering Southwest Jiaotong University 610031 Chengdu Sichuan PR China

    1 shared publication
  • Dongbing Liu

    College of Mathematics and Computer, Panzhihua University, Panzhihua 617000, China

    1 shared publication
  • Haibo Wang

    Vanadium and Titanium Institute of Panzhihua University, Panzhihua, Sichuan, 617000, PR China

    1 shared publication
  • Hao Zhang

    National Engineering Research Center for Biomaterials, Sichuan University, Chengdu 610064, China

    1 shared publication
  • Jianxin Wang

    Key Laboratory of Advanced Technologies of Materials (Ministry of Education), Southwest Jiaotong University, Chengdu, Sichuan, PR China

    1 shared publication
  • Jie Weng

    Institute of Biomedical Engineering College of Medicine Southwest Jiaotong University Chengdu China

    1 shared publication

Latest Publications

  • Open Access

    Influence of Nano-ZrO2 Particles on the Microstructure and Properties of Micro-Arc Oxidation Coatings on TC4 Titanium Alloy

    by Xingping Fan, Xinzhu Xiao, Limin Zhang, Xi Lin, Ping Wang

    To enhance the surface hardness and wear resistance of TC4 titanium alloy, this paper systematically investigates the effects of voltage, time, and nano-ZrO2 particle concentration on the microstructure, phase composition, hardness, and wear resistance of ceramic coatings prepared by micro-arc oxidation (MAO) technology in silicate electrolyte systems. The results indicate that as the voltage increases, the pore size of the coating layer increases while the number decreases; as the time extends, the pore size first increases and then decreases. The addition of nano-ZrO2 particles can fill the micropores in the coating layer, significantly improving its compactness. XRD analysis reveals that the coating layer primarily consists of anatase TiO2, rutile TiO2, and SiO2. The addition of ZrO2 leads to the formation of monoclinic ZrO2 and ZrTiO4 phases. Hardness tests show that the highest hardness (449 ± 4 HV) is achieved at a voltage of 480 V and a duration of 3 min, and further increases to 547 ± 5 HV with the addition of 5 g/L ZrO2. Friction and wear experiments demonstrate that the friction coefficient decreases from 0.12 to 0.06 with the addition of ZrO2, significantly reducing the wear mass loss. The optimal process parameters are a voltage of 480 V, a duration of 3 min, and a ZrO2 concentration of 5 g/L, resulting in a composite coating with a dense surface, high hardness, and excellent wear resistance.

  • Open Access

    Effect of Voltage on the Structure and Biological Activity of Micro-Arc Oxidation Ti-13Nb-13Zr Alloy Coatings

    by Dongbing Liu, Xingping Fan

    Titanium alloys, particularly β-type Ti-13Nb-13Zr, are promising biomedical materials due to their low elastic modulus and excellent biocompatibility. However, their bioactivity needs improvement for better bone integration. In this study, a calcium-phosphate (Ca/P) coating was prepared on a Ti-13Nb-13Zr alloy via micro-arc oxidation (MAO) in an electrolyte containing calcium acetate and dipotassium hydrogen phosphate. The effect of applied voltage (300 V, 400 V, and 500 V) on the phase composition, surface morphology, and in vitro bioactivity of the coatings was investigated. Surface characterization was performed using scanning electron microscopy (SEM), X-ray diffraction (XRD), and energy-dispersive spectroscopy (EDS). The results show that increasing the voltage increased the surface roughness, average pore size, and rutile TiO2 content in the coating. The Ca/P ratio in the coating approached 1.67 at 500 V, similar to that of natural bone. After immersion in simulated body fluid (SBF) for 20 days, the coating formed at 500 V induced the highest deposition of hydroxyapatite (HA), completely covering the microporous surface. These findings indicate that MAO treatment at 500 V significantly enhances the bioactivity of the Ti-13Nb-13Zr alloy, making it a promising candidate for orthopedic implants.


  • Open Access

    Preparation and Photocatalytic Performance of Silver-Loaded Micro-Arc Oxidation TiO2 Coating

    by Xingping Fan, Ying Xia, Wei Fan, Yulong Li

    Using a Ti6Al4V (TC4) titanium alloy plate as a substrate, micro-arc oxidation technology was applied at an oxidation time of 3.5 min and a voltage of 480 V, 495 V, and 510 V. A TiO2–containing ceramic layer was prepared on the surface of the TC4 alloy, and the TiO2–containing coating was doped with silver ions. The surface microstructure, phase structure, and photocatalytic performance of ceramic coatings before and after doping with silver ions were analyzed using instruments such as X-ray diffraction (XRD), energy dispersive spectroscopy (EDS), and scanning electron microscopy (SEM). The results showed that as the oxidation voltage increased, the number of large pores first decreased and then increased. At a voltage of 495 V, the total area of various pores reached 45–50 μm2. After the voltage rose to 510 V, the maximum pore area decreased. TiO2 exists in the surface pores of the morphology in the form of rutile, and the loading of silver ions further enhances its photocatalytic performance. The degradation rate of methyl orange by undoped silver ion samples can reach 15.5%, and the degradation rate of methyl orange can reach about 31% when 4 g/L Ag2O is added to the electrolyte. Increasing the concentration of doped silver ions can enhance the degradation rate of methyl orange.

  • Open Access

    Preparation and biological activity study of Ti13Nb13Zr surface nanotubes

    by Xingping Fan, Wei Fan

    As a third‐generation titanium alloy, Ti13Nb13Zr is widely used in the field of biomedicine due to its advantages such as low elastic modulus, high strength, high toughness, high fatigue strength, corrosion resistance, and good biocompatibility. However, the biological inertness of Ti13Nb13Zr alloy limit their wide application as biomedical implant materials. In this study, the bioactive TiO 2 nanotubes was prepared on Ti13Nb13Zr alloy by anodisation and heat treatment method. The bioactivity of Ti13Nb13Zr was evaluated by immersing the samples into the simulated body fluid for 20 days. Results show that the Ti13Nb13Zr alloy coated with anatase nanotubes has the superior ability of hydroxyapatite formation.


  • Open Access

    Fabrication and Characterization of LaF3-Reinforced Porous HA/Ti Scaffolds

    by Xingping Fan, Hao Zhang

    To improve the performance of porous hydroxyapatite/titanium (HA/Ti) composites, LaF3 reinforced porous HA/Ti scaffolds with a porosity of approximately 60% were prepared via a powder metallurgical method, using NH4HCO3 as the pore-forming agent. The scaffolds induced HA formation and showed high bioactivity, and the compressive strength could be regulated by changing the LaF3 dosage. When the LaF3 dosage was 0.3%, the compressive strength of the porous scaffold was 65 MPa. Moreover, LaF3 reinforced porous HA/Ti scaffolds can further induce the deposition of calcium phosphate after immersion in simulated body fluid (SBF) for 7 days, indicating that the corresponding scaffold is an ideal choice for spongy bone repair.


  • Open Access

    Fabrication and properties of LaF3 reinforced porous HA/Ti scaffolds

    by Xingping Fan

    To improve the performance of porous hydroxyapatite/Titanium (HA/Ti) composites, LaF3 reinforced porous HA/Ti scaffolds with a porosity of approximately 60% were prepared via a powder metallurgical method using NH4HCO3 as the pore-forming agent. The scaffolds induced HA formation and showed high bioactivity, and the compressive strength could be regulated by changing the LaF3 dosage. When the LaF3 dosage was 0.3%, the compressive strength of the porous scaffold was 65 MPa. And LaF3 reinforced porous HA/Ti scaffolds can further induce the deposition of calcium phosphate after immersion in simulated body fluid (SBF) for 7 days,which indicating the corresponding scaffold was an ideal choice for spongy bone repair.

  • Open Access

    Controllable preparation of TiO2 nanotubes and their photocatalytic performance

    by Fan Xing-Ping

    Ethylene glycol aqueous solution containing 0.5% NH4F was used as the electrolyte and the Ti foil was oxidized at 40 V for 30 min to obtain TiO2 nanotube arrays with an inner diameter of about 85 nm. After heat treatment at 450 °C for 2 h, the TiO2 nanotubes transformed from an amorphous phase to anatase, and a small percentage of the nanotubes collapsed. The Pt loaded by electrodeposition appeared at the nozzle of the nanotubes in a flake morphology.The best catalytic effect on methylene blue degradation was achieved by Pt loading with electrodeposition for 120 s.The methylene blue degradation rate reached 50% after 10 h of ultraviolet irradiation.


  • Construction and Biological Performance of Surface Treated Porous Titanium Scaffold Using Nanotube Arrays of Anatase

    by Haibo Wang, Xingping Fan

    TiO2 nanotube in diameter of ~ 100 nm array films were prepared on a porous titanium scaffold with a porosity of 70% via anodic oxidation. The morphology and phases of the films were characterized, and the thermal stability of the films were also studied. In-vitro, the bioactivity of the modified scaffolds was evaluated by simulated body fluid immersion test. In vivo, the scaffolds were implanted into the back muscles of the dog for 6 months. Results show that the anatase nanotubues give better bioactivity than the amorphous. The scaffold after anodic oxidation and annealing at 500 °C for 5 hours not only can induce the formation of hydroxyapatite, but also can induce blood vessel formation and promote the expressions of bone morphogenetic protein BMP-2. The BMP-2 concentrations is 5.57±0.20 μ/L for the scaffold been anodically oxidated and heat-preserved, the value is much higher than that of untreated scaffold(2.78±0.16 μg/L)or only been anodically oxidated(2.86±0.17 μg/L). It shows that the anatase TiO2 nanotubes can contribute to the potential osteoinductivity. This study will promote the development of novel functional porous supports.

  • Open Access

    Study on the surface packing cementation aluminizing processes of Q345 steel in an air environment

    by Fan Xingping

    To address the requirement of a vacuum environment or a protective atmosphere in the process of aluminizing, pack cementation was used to aluminize the surface of Q345 steel in an air environment. The aluminized coating with a large hardness and corrosion resistance was prepared on the surface of Q345 steel. The influence of the aluminizing temperature and the holding time on the surface quality and thickness of the aluminized coating was studied to determine the optimum conditions for aluminizing. The surface quality of the coating was observed by an electron microscope and the thickness of the aluminized coating was measured. The main elemental distribution of the coating was also analyzed by an energy spectrometer. The phase composition of the aluminized coating was analyzed by an x-ray diffractometer and the change in coating hardness was measured by a microhardness tester. The results showed that when the holding time was 3 h and the heating temperature was 800 °C, the obtained thickness of the aluminized coating was 180 μm, with good quality, excellent hardness, and corrosion resistance.


  • Effects of High-Concentration Alkali Treatment on Surface Bioactivity of Porous Titanium

    by Xingping Fan

    Various surface treatment methods have been used to modify the surface activation of dense titanium. In this study, a high concentration of sodium hydroxide solution was used to treat porous titanium prepared by adding porous agent at different times. The results of the study showed that after alkali treatment, porous titanium was implanted into the back muscle of the dog and the implanted sample was taken out for bone formation protein-2 enzymatic immunoassay after 6 months. The porous titanium inner wall has been covered. The microstructures vary with the treatment time. The treated surface can induce the formation of hydroxyapatite deposition and promote the expression of BMP-2, which shows good bone induction. High concentration alkali treatment of porous titanium, the method is simple, can shorten the HA formation time, can effectively activate porous titanium inner and outer surfaces, is an effective method to prepare bioactive porous titanium.