E. McCafferty
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Latest Publications
- 1 January 2010
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 157 (11) , C382-C387
Pit Initiation on Aluminum as a Queueing Process
The pitting corrosion of aluminum is modeled as a queueing process in which chloride ions (customers or units) enter the passive film and are serviced (form an emerging pit) at certain sites (servers) at the oxide/metal interface. X-ray photoelectron spectroscopy (XPS) data show that chloride ions penetrate the passive film on aluminum and are considered to lie in a queue. The servicing (or processing) stage includes chloride-assisted localized dissolution of aluminum, development of local acidity within the emerging pit, and buildup of chloride ions within the developing pit. The arrival rate of chloride ions is determined from quantitative XPS intensity data. The servicing rate has been determined from anodic polarization curves and also from Scully's criterion for stable pit growth. The following queueing characteristic parameters have been calculated: the number of units in the queue, the number of units in the system (queue plus server), the average time a unit spends in the queue, and the average time a unit spends in the system (queue and server). This is done for the following queueing systems: single queue with a single server, single queue with multiple servers, and multiple queues with single or multiple servers. A long time in the system corresponds to a low rate for the ongoing corrosion reaction. The time that a unit spends in the system is maximized for (i) a decrease in the number of servers, (ii) a decrease in the servicing rate μ, (iii) a decrease in the number of queues, or (iv) an increase in the arrival rate (up to ).
- 1 January 2010
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 157 (11) , C382-C387
Pit Initiation on Aluminum as a Queueing Process
The pitting corrosion of aluminum is modeled as a queueing process in which chloride ions (customers or units) enter the passive film and are serviced (form an emerging pit) at certain sites (servers) at the oxide/metal interface. X-ray photoelectron spectroscopy (XPS) data show that chloride ions penetrate the passive film on aluminum and are considered to lie in a queue. The servicing (or processing) stage includes chloride-assisted localized dissolution of aluminum, development of local acidity within the emerging pit, and buildup of chloride ions within the developing pit. The arrival rate of chloride ions is determined from quantitative XPS intensity data. The servicing rate has been determined from anodic polarization curves and also from Scully's criterion for stable pit growth. The following queueing characteristic parameters have been calculated: the number of units in the queue, the number of units in the system (queue plus server), the average time a unit spends in the queue, and the average time a unit spends in the system (queue and server). This is done for the following queueing systems: single queue with a single server, single queue with multiple servers, and multiple queues with single or multiple servers. A long time in the system corresponds to a low rate for the ongoing corrosion reaction. The time that a unit spends in the system is maximized for (i) a decrease in the number of servers, (ii) a decrease in the servicing rate μ, (iii) a decrease in the number of queues, or (iv) an increase in the arrival rate (up to ).
- 10 October 2009
- Published by Springer Nature in Journal of Applied Electrochemistry
- Vol. 40 (3) , 543-549
Thermodynamics of chromate replacements by various homologous transition metal oxyanions
- 10 October 2009
- Published by Springer Nature in Journal of Applied Electrochemistry
- Vol. 40 (3) , 543-549
Thermodynamics of chromate replacements by various homologous transition metal oxyanions
- Open Access
- 1 January 2003
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 150 (5) , B238-B247
General Relations Regarding Graph Theory and the Passivity of Binary Alloys
The passivity of a binary alloy is considered in terms of a network of -M-O-M- bridges in the oxide film, where M is the component of the binary alloy which produces passivity. The structure of the oxide is represented by a mathematical graph, and graph theory is used to calculate the connectivity of the oxide, given by the product of the number of edges in the graph and the Randic index. A stochastic calculation is employed to insert ions of the second metal into the oxide film so as to disrupt the connectivity of the -M-O-M- network. This disruption occurs at a critical ionic concentration of the oxide film. Mathematical relationships are developed for the introduction of a general ion B+nB+n into oxides where passivity is due to the existence of continuous networks of -Cr-O-Cr-, -Si-O-Si-, or -Mo-O-Mo-. Thus, critical ionic compositions are calculated for oxide films on the binary alloys B-Cr, B-Si, or B-Mo where passivity is provided in turn by the presence of Cr, Si, or Mo, respectively, in the binary alloy. In each case, B refers to any metal B which produces B+nB+n ions in the oxide film, where +n+n is the oxidation number of the ion. © 2003 The Electrochemical Society. All rights reserved.
- 1 January 2003
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 150 (5) , B238-B247
Open AccessGeneral Relations Regarding Graph Theory and the Passivity of Binary Alloys
The passivity of a binary alloy is considered in terms of a network of -M-O-M- bridges in the oxide film, where M is the component of the binary alloy which produces passivity. The structure of the oxide is represented by a mathematical graph, and graph theory is used to calculate the connectivity of the oxide, given by the product of the number of edges in the graph and the Randic index. A stochastic calculation is employed to insert ions of the second metal into the oxide film so as to disrupt the connectivity of the -M-O-M- network. This disruption occurs at a critical ionic concentration of the oxide film. Mathematical relationships are developed for the introduction of a general ion B+nB+n into oxides where passivity is due to the existence of continuous networks of -Cr-O-Cr-, -Si-O-Si-, or -Mo-O-Mo-. Thus, critical ionic compositions are calculated for oxide films on the binary alloys B-Cr, B-Si, or B-Mo where passivity is provided in turn by the presence of Cr, Si, or Mo, respectively, in the binary alloy. In each case, B refers to any metal B which produces B+nB+n ions in the oxide film, where +n+n is the oxidation number of the ion. © 2003 The Electrochemical Society. All rights reserved.
- 1 January 1999
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 3 (1) , 28-30
Graph Theory and the Passivity of Iron-Chromium Binary Alloys
Using graph theory, it is shown that the introduction of 70 atom % of into a ‐Cr‐O‐Cr‐ oxide network serves to disjoin the network, or conversely, introduction of 30% atomic concentration of serves to provide a connected ‐Cr‐O‐Cr‐ network. The results of surface analysis show that this concentration of 30 atom % in the oxide film corresponds to 13 atom % chromium in the Fe‐Cr alloy, i.e., the critical concentration of Cr required for passivity in Fe‐Cr binary alloys. © 2000 The Electrochemical Society
- 1 January 1999
- Published by The Electrochemical Society in Electrochemical and Solid-State Letters
- Vol. 3 (1) , 28-30
Graph Theory and the Passivity of Iron-Chromium Binary Alloys
Using graph theory, it is shown that the introduction of 70 atom % of into a ‐Cr‐O‐Cr‐ oxide network serves to disjoin the network, or conversely, introduction of 30% atomic concentration of serves to provide a connected ‐Cr‐O‐Cr‐ network. The results of surface analysis show that this concentration of 30 atom % in the oxide film corresponds to 13 atom % chromium in the Fe‐Cr alloy, i.e., the critical concentration of Cr required for passivity in Fe‐Cr binary alloys. © 2000 The Electrochemical Society