Hiroki Ohno
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Hiroki Ohno has a total of 38 co-authors. Here are the top co-authors by number of shared publications:
- Kazuhiko Endo
Division of Biomaterials and Bioengineering, Department of Oral Rehabilitation, School of Dentistry, Health Sciences University of Hokkaido
10 shared publications Yuro Yamane
Department of Dental Materials Science, Health Sciences University of Hokkaido School of Dentistry, Kanazawa 1757, Ishikari-Tobetsu, Hokkaido 061-0293, Japan
4 shared publicationsKazuhiko Endo
Division of Biomaterials and Bioengineering, Department of Oral Rehabilitation, School of Dentistry, Health Sciences University of Hokkaido
3 shared publicationsIsao Kawashima
2 shared publicationsKazuhiro Hikita
Department of Dental Materials Science, School of Dentistry, Health Sciences University of Hokkaido
2 shared publicationsMasahiro Suzuki
2 shared publications
Latest Publications
- Open Access
- 1 January 2013
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 32 (6) , 920-927
Analysis of residual stress in the resin of metal-resin adhesion structures by scanning acoustic microscopy
The residual stress caused by polymerization shrinkage and thermal contraction of a heat-curing resin containing 4-META on a metal-resin structure was measured by a scanning acoustic microscope. The tensile residual stress in the resin occurred within 70 µm of the adhesion interface with a flat plate specimen. The maximum tensile stress was about 58 MPa at the interface. On a metal plate specimen with retention holes, ring-like cracks in the resin occurred around the retention holes with the adhesive specimen and many linear cracks occurred in the resin vertical to the longitudinal direction of the metal frame with the non-adhesive specimens. There was tensile residual stress on the resin surface at the center of the retention holes of the adhesion specimen, indicating that the stress in the specimen with surface treatment for adhesion was higher than in that without surface treatment.
- 1 January 2013
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 32 (6) , 920-927
Open AccessAnalysis of residual stress in the resin of metal-resin adhesion structures by scanning acoustic microscopy
The residual stress caused by polymerization shrinkage and thermal contraction of a heat-curing resin containing 4-META on a metal-resin structure was measured by a scanning acoustic microscope. The tensile residual stress in the resin occurred within 70 µm of the adhesion interface with a flat plate specimen. The maximum tensile stress was about 58 MPa at the interface. On a metal plate specimen with retention holes, ring-like cracks in the resin occurred around the retention holes with the adhesive specimen and many linear cracks occurred in the resin vertical to the longitudinal direction of the metal frame with the non-adhesive specimens. There was tensile residual stress on the resin surface at the center of the retention holes of the adhesion specimen, indicating that the stress in the specimen with surface treatment for adhesion was higher than in that without surface treatment.
- 1 July 2006
- Published by Wiley in The Angle Orthodontist
- Vol. 76 (4) , 705-11
Galvanic corrosion behavior of orthodontic archwire alloys coupled to bracket alloys.
The purpose of this study was to provide a quantitative assessment of galvanic corrosion behavior of orthodontic archwire alloys coupled to orthodontic bracket alloys in 0.9% NaCl solution and to study the effect of surface area ratios. Two common bracket alloys, stainless steels and titanium, and four common wire alloys, nickel-titanium (NiTi) alloy, beta-titanium (beta-Ti) alloy, stainless steel, and cobalt-chromium-nickel alloy, were used. Three different area ratios, 1:1, 1:2.35, and 1:3.64, were used; two of them assumed that the multibracket appliances consists of 14 brackets and 0.016 inch of round archwire or 0.016 x 0.022 inch of rectangular archwire. The galvanic current was measured for 3 successive days using zero-impedance ammeter. When the NiTi alloy was coupled with Ti (1:1, 1:2.35, and 1:3.64 of the surface area ratio) or beta-Ti alloy was coupled with Ti (1:2.35 and 1:3.64 of the surface area ratio), Ti initially was the anode and corroded. However, the polarity reversed in 1 hour, resulting in corrosion of the NiTi or beta-Ti. The NiTi alloy coupled with SUS 304 or Ti exhibited a relatively large galvanic current density even after 72 hours. It is suggested that coupling SUS 304-NiTi and Ti-NiTi may remarkably accelerate the corrosion of NiTi alloy, which serves as the anode. The different anode-cathode area ratios used in this study had little effect on galvanic corrosion behavior.
- 1 July 2006
- Published by Wiley in The Angle Orthodontist
- Vol. 76 (4) , 705-11
Galvanic corrosion behavior of orthodontic archwire alloys coupled to bracket alloys.
The purpose of this study was to provide a quantitative assessment of galvanic corrosion behavior of orthodontic archwire alloys coupled to orthodontic bracket alloys in 0.9% NaCl solution and to study the effect of surface area ratios. Two common bracket alloys, stainless steels and titanium, and four common wire alloys, nickel-titanium (NiTi) alloy, beta-titanium (beta-Ti) alloy, stainless steel, and cobalt-chromium-nickel alloy, were used. Three different area ratios, 1:1, 1:2.35, and 1:3.64, were used; two of them assumed that the multibracket appliances consists of 14 brackets and 0.016 inch of round archwire or 0.016 x 0.022 inch of rectangular archwire. The galvanic current was measured for 3 successive days using zero-impedance ammeter. When the NiTi alloy was coupled with Ti (1:1, 1:2.35, and 1:3.64 of the surface area ratio) or beta-Ti alloy was coupled with Ti (1:2.35 and 1:3.64 of the surface area ratio), Ti initially was the anode and corroded. However, the polarity reversed in 1 hour, resulting in corrosion of the NiTi or beta-Ti. The NiTi alloy coupled with SUS 304 or Ti exhibited a relatively large galvanic current density even after 72 hours. It is suggested that coupling SUS 304-NiTi and Ti-NiTi may remarkably accelerate the corrosion of NiTi alloy, which serves as the anode. The different anode-cathode area ratios used in this study had little effect on galvanic corrosion behavior.
- Open Access
- 1 January 2005
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 24 (4) , 503-507
Mechanism by which Porous Structure is Formed on the Surface of Gold Alloy Containing Only Cu as Base Metal
Gold alloys with Cu contents of 10mass%, 20%, and 30% were used for morphological observation of porous surface structures after heating at 800°C in air followed by pickling with acid solution. With increasing Cu content in the gold alloy, the internal oxidation zone became well-developed in the alloy matrix. The mechanism by which a porous structure was formed on the surface of a gold alloy containing only Cu as a base metal was thought to be as follows: Cu2O which formed along the grain boundaries acted as a diffusion path, permitting the penetration of O2- into the inner alloy matrix, and thereby resulting in internal oxidation occurring predominantly along the grain boundaries.
- 1 January 2005
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 24 (4) , 503-507
Open AccessMechanism by which Porous Structure is Formed on the Surface of Gold Alloy Containing Only Cu as Base Metal
Gold alloys with Cu contents of 10mass%, 20%, and 30% were used for morphological observation of porous surface structures after heating at 800°C in air followed by pickling with acid solution. With increasing Cu content in the gold alloy, the internal oxidation zone became well-developed in the alloy matrix. The mechanism by which a porous structure was formed on the surface of a gold alloy containing only Cu as a base metal was thought to be as follows: Cu2O which formed along the grain boundaries acted as a diffusion path, permitting the penetration of O2- into the inner alloy matrix, and thereby resulting in internal oxidation occurring predominantly along the grain boundaries.
- 1 May 2004
- Published by Elsevier in Dental Materials
- Vol. 20 (4) , 330-337
New mechanical retention method for resin and gold alloy bonding
- 1 May 2004
- Published by Elsevier in Dental Materials
- Vol. 20 (4) , 330-337
New mechanical retention method for resin and gold alloy bonding
- 1 January 2002
- Published by Japan Prosthodontic Society in Nihon Hotetsu Shika Gakkai Zasshi
- Vol. 46 (5) , 685-692
Design of a CAD/CAM Crown Using Tooth Form Data from the Corresponding Tooth Located on the Contralateral Side. Investigation into the Condition of the Corresponding Tooth Located on the Contralateral Side.
- 1 January 2002
- Published by Japan Prosthodontic Society in Nihon Hotetsu Shika Gakkai Zasshi
- Vol. 46 (5) , 685-692
Design of a CAD/CAM Crown Using Tooth Form Data from the Corresponding Tooth Located on the Contralateral Side. Investigation into the Condition of the Corresponding Tooth Located on the Contralateral Side.
- Open Access
- 1 January 2001
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 20 (1) , 90-102
XPS Study on the Weakest Zone in the Adhesion Structure between Resin Containing 4-META and Precious Metal Alloys Treated with Different Surface Modification Methods.
Three precious metal alloys, Type IV gold alloy, 14 K gold alloy, and silver-based alloy, were treated with different surface modifications including a metal primer (VBATDT) application, a SiOx coating method, high-temperature oxidation, modification method with a liquid Ga-Sn alloy, and tin electroplating. Then thin PMMA films were bonded with a resin containing 4-META. Water durability at the adhesion interface was evaluated after water immersion, followed by thermal cycling used liquid nitrogen. The weakest zone at the interface was investigated using XPS only for the Ag-Pd alloy specimens that had been surface-treated with as-polishing, adhesive primer, and the SiOx coating method, since peeling of the PMMA film on the surface of specimens surface-treated by other methods was not observed. Metal elements were detected from the resin side at the adhesion interface. The chemical states of Cu in the resin before argon ion etching were characterized as metal oxides and/or states of chemical interaction with 4-META, VBATDT, or SiOx.
- 1 January 2001
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 20 (1) , 90-102
Open AccessXPS Study on the Weakest Zone in the Adhesion Structure between Resin Containing 4-META and Precious Metal Alloys Treated with Different Surface Modification Methods.
Three precious metal alloys, Type IV gold alloy, 14 K gold alloy, and silver-based alloy, were treated with different surface modifications including a metal primer (VBATDT) application, a SiOx coating method, high-temperature oxidation, modification method with a liquid Ga-Sn alloy, and tin electroplating. Then thin PMMA films were bonded with a resin containing 4-META. Water durability at the adhesion interface was evaluated after water immersion, followed by thermal cycling used liquid nitrogen. The weakest zone at the interface was investigated using XPS only for the Ag-Pd alloy specimens that had been surface-treated with as-polishing, adhesive primer, and the SiOx coating method, since peeling of the PMMA film on the surface of specimens surface-treated by other methods was not observed. Metal elements were detected from the resin side at the adhesion interface. The chemical states of Cu in the resin before argon ion etching were characterized as metal oxides and/or states of chemical interaction with 4-META, VBATDT, or SiOx.
- 1 January 2001
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 20 (1) , 63-74
Mechanism of Adhesion between 4-META Resin and Alloys Based on Bolger's Acid-base Interaction.
The water durability at adhesion interfaces between 4-META resin and Au-In or Au-Si alloys was investigated by the peeling test and by surface analysis using X-ray photoelectron spectroscopy (XPS) as well as theoretical consideration based on Bolger's acid-base theory. XPS spectra demonstrated that several-nm thick layers of In2O3 and SiO2 were formed on the Au-In and Au-Si alloys. The water durability of the Au-In alloys increased with increases in In content. The Au-Si alloy and quartz glass specimens showed a total absence of water durability. Bolger's theory suggested that the interaction of 4-MET with In2O3 was considered to be ionic and stable in the presence of water while that of 4-MET with SiO2 was due to hydrogen bonds, which can easily be dissociated in the presence of water. These findings suggest that Bolger's theory is useful for evaluating chemical interactions between an adhesive monomer and oxides on a precious metal alloy.
- 1 January 2001
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 20 (1) , 63-74
Mechanism of Adhesion between 4-META Resin and Alloys Based on Bolger's Acid-base Interaction.
The water durability at adhesion interfaces between 4-META resin and Au-In or Au-Si alloys was investigated by the peeling test and by surface analysis using X-ray photoelectron spectroscopy (XPS) as well as theoretical consideration based on Bolger's acid-base theory. XPS spectra demonstrated that several-nm thick layers of In2O3 and SiO2 were formed on the Au-In and Au-Si alloys. The water durability of the Au-In alloys increased with increases in In content. The Au-Si alloy and quartz glass specimens showed a total absence of water durability. Bolger's theory suggested that the interaction of 4-MET with In2O3 was considered to be ionic and stable in the presence of water while that of 4-MET with SiO2 was due to hydrogen bonds, which can easily be dissociated in the presence of water. These findings suggest that Bolger's theory is useful for evaluating chemical interactions between an adhesive monomer and oxides on a precious metal alloy.
- Open Access
- 1 January 2000
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 19 (1) , 34-49
Corrosion Characteristics of Ferric and Austenitic Stainless Steels for Dental Magnetic Attachment.
The corrosion behaviors of four ferric stainless steels and two austenitic stainless steels were examined in a simulated physiological environment (0.9% NaCl solution) to obtain basic data for evaluating the appropriate composition of stainless steels for dental magnetic attachments. The corrosion resistance was evaluated by electrochemical techniques and the analysis of released metal ions by atomic absorption spectrophotometry. The surface of the stainless steels was analyzed by X-ray photoelectron spectroscopy (XPS). The breakdown potential of ferric stainless steels increased and the total amount of released metal ions decreased linearly with increases in the sum of the Cr and Mo contents. The corrosion rate of the ferric stainless steels increased 2 to 6 times when they were galvanically coupled with noble metal alloys but decreased when coupled with commercially pure Ti. For austenitic stainless steels, the breakdown potential of high N-bearing stainless steel was approximately 500 mV higher than that of SUS316L, which is currently used as a component in dental magnetic attachments. The enriched nitrogen at the alloy/passive film interface may be effective in improving the localized corrosion resistance.
- 1 January 2000
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 19 (1) , 34-49
Open AccessCorrosion Characteristics of Ferric and Austenitic Stainless Steels for Dental Magnetic Attachment.
The corrosion behaviors of four ferric stainless steels and two austenitic stainless steels were examined in a simulated physiological environment (0.9% NaCl solution) to obtain basic data for evaluating the appropriate composition of stainless steels for dental magnetic attachments. The corrosion resistance was evaluated by electrochemical techniques and the analysis of released metal ions by atomic absorption spectrophotometry. The surface of the stainless steels was analyzed by X-ray photoelectron spectroscopy (XPS). The breakdown potential of ferric stainless steels increased and the total amount of released metal ions decreased linearly with increases in the sum of the Cr and Mo contents. The corrosion rate of the ferric stainless steels increased 2 to 6 times when they were galvanically coupled with noble metal alloys but decreased when coupled with commercially pure Ti. For austenitic stainless steels, the breakdown potential of high N-bearing stainless steel was approximately 500 mV higher than that of SUS316L, which is currently used as a component in dental magnetic attachments. The enriched nitrogen at the alloy/passive film interface may be effective in improving the localized corrosion resistance.
- 1 January 1998
- Published by Japan Society of Corrosion Engineering in Corrosion Engineering
- Vol. 47 (9) , 570-576
Corrosion Resistance and Biocompatibility of High Nitrogen-bearing Stainless Steels
- 1 January 1998
- Published by Japan Society of Corrosion Engineering in Corrosion Engineering
- Vol. 47 (9) , 570-576
Corrosion Resistance and Biocompatibility of High Nitrogen-bearing Stainless Steels
- 1 January 1998
- Published by Japan Prosthodontic Society in Nihon Hotetsu Shika Gakkai Zasshi
- Vol. 42 (4) , 617-624
A Clinical Report of Prosthodontic Treatment Using Titanium for a Patient with Allergic Reaction to Sn, Cu, Cr, Au and Pd.
- 1 January 1998
- Published by Japan Prosthodontic Society in Nihon Hotetsu Shika Gakkai Zasshi
- Vol. 42 (4) , 617-624
A Clinical Report of Prosthodontic Treatment Using Titanium for a Patient with Allergic Reaction to Sn, Cu, Cr, Au and Pd.