Geoff M. Scamans
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Geoff M. Scamans has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
- Jayesh Bhimji Patel
Brunel Centre for Advanced Solidification Technology (BCAST), Brunel University London, Uxbridge UB8 3PH, UK
6 shared publications - Kawther Al-Helal
Brunel Centre for Advanced Solidification Technology, Brunel University London, Uxbridge UB8 3PH, UK
6 shared publications - Zhongyun Fan
Brunel Centre for Advanced Solidification Technology (BCAST), Brunel University London, Uxbridge UB8 3PH, UK
5 shared publications - Jaime Lazaro-Nebreda
BCAST, Brunel University London, Uxbridge, UB8 3PH, UK
4 shared publications A. Hall
Alken, 21 Meadow View Holmewood Derbyshire S42 5UL UK
1 shared publicationC. Butler
Innoval Technology Ltd. Beaumont Close Banbury Oxon OX16 1TQ UK
1 shared publication
Latest Publications
- Open Access
Degassing of Aluminum Alloy Melts by High Shear Melt Conditioning Technology: An Overview
The search for more efficient methods for degassing aluminum alloy melts has always been of great interest for the metal industry because the presence of hydrogen and oxides in the melts’ prior casting was detrimental to the integrity and properties of the final products. In this work, we present an overview of the progress and key findings from the research and development of an innovative High Shear Melt Conditioning (HSMC) degassing technology during the Liquid Metal Engineering (LiME) Research Hub project. Compared to conventional rotary degassing, this novel technique was capable of working at higher rotor speeds to efficiently break and disperse the naturally occurring oxide bifilms in the melt and to capture and disperse each supplied inert gas bubble into many tiny bubbles throughout the whole melt. This resulted in the elimination of the need to degas fluxes to remove the oxides in the melt, the reduction in the gas flow required to reach the same level of hydrogen removal rate, and the minimization of the regassing effect after processing. The increased process efficiency allowed for reduced melt processing costs and, at the same time, improved the melt quality, which resulted in fewer defects and improved mechanical properties.
Open AccessDegassing of Aluminum Alloy Melts by High Shear Melt Conditioning Technology: An Overview
The search for more efficient methods for degassing aluminum alloy melts has always been of great interest for the metal industry because the presence of hydrogen and oxides in the melts’ prior casting was detrimental to the integrity and properties of the final products. In this work, we present an overview of the progress and key findings from the research and development of an innovative High Shear Melt Conditioning (HSMC) degassing technology during the Liquid Metal Engineering (LiME) Research Hub project. Compared to conventional rotary degassing, this novel technique was capable of working at higher rotor speeds to efficiently break and disperse the naturally occurring oxide bifilms in the melt and to capture and disperse each supplied inert gas bubble into many tiny bubbles throughout the whole melt. This resulted in the elimination of the need to degas fluxes to remove the oxides in the melt, the reduction in the gas flow required to reach the same level of hydrogen removal rate, and the minimization of the regassing effect after processing. The increased process efficiency allowed for reduced melt processing costs and, at the same time, improved the melt quality, which resulted in fewer defects and improved mechanical properties.
- Open Access
De-Ironing of Aluminium Alloy Melts by High Shear Melt Conditioning Technology: An Overview
The main problem of recycling aluminium scrap is the gradual accumulation of impurities, especially iron, which tend to form undesired intermetallic compounds that affect the integrity and the mechanical performance of the castings. In this paper, we aim to provide an overview on the topic of iron removal from aluminium melts through primary intermetallic precipitation and the progress made during the LiME Hub project to understand the process and to develop a more efficient procedure. We cover both thermodynamic analysis and experimental validation. We found that high shear melt conditioning technology enhances the typically slow nucleation and growth of the dense primary intermetallics, speeding up their sedimentation and allowing a faster removal of Fe from the melt by simple gravity sedimentation. It also promotes the formation of smaller and more compact Fe-rich intermetallics, allowing an increased volume fraction recovery and mitigating their effect of being present in the final castings. The technology is not limited to batch processing, with a 90% efficiency, but can also be applied to continuous melt treatment of aluminium scrap, with currently 60% efficiency, and could be combined with other solid–liquid separation techniques to increase the purification efficiency even more.
Open AccessDe-Ironing of Aluminium Alloy Melts by High Shear Melt Conditioning Technology: An Overview
The main problem of recycling aluminium scrap is the gradual accumulation of impurities, especially iron, which tend to form undesired intermetallic compounds that affect the integrity and the mechanical performance of the castings. In this paper, we aim to provide an overview on the topic of iron removal from aluminium melts through primary intermetallic precipitation and the progress made during the LiME Hub project to understand the process and to develop a more efficient procedure. We cover both thermodynamic analysis and experimental validation. We found that high shear melt conditioning technology enhances the typically slow nucleation and growth of the dense primary intermetallics, speeding up their sedimentation and allowing a faster removal of Fe from the melt by simple gravity sedimentation. It also promotes the formation of smaller and more compact Fe-rich intermetallics, allowing an increased volume fraction recovery and mitigating their effect of being present in the final castings. The technology is not limited to batch processing, with a 90% efficiency, but can also be applied to continuous melt treatment of aluminium scrap, with currently 60% efficiency, and could be combined with other solid–liquid separation techniques to increase the purification efficiency even more.
- Open Access
High-Shear De-Gassing and De-Ironing of an Aluminum Casting Alloy Made Directly from Aluminum End-of-Life Vehicle Scrap
High-shear melt conditioning (HSMC) technology was used for degassing and de-ironing of an aluminum alloy recovered from the Zorba cast fraction of the non-ferrous scrap from shredded end-of-life vehicles. The results showed that the recovery of aluminum alloys from the Zorba cast fraction was more than 80%. High-shear melt conditioning improved the degassing process during melt treatment in comparison with the adding of degassing tablets. The efficiency of the de-ironing process using HSMC increased by up to 24% after, increasing the Mn content to 0.8% in the melt. Adding Mn to Zorba melt enhanced the de-ironing process and eliminated the formation of β-AlFeSi intermetallic particles, which have a detrimental effect on both the mechanical and corrosion properties of the alloy.
Open AccessHigh-Shear De-Gassing and De-Ironing of an Aluminum Casting Alloy Made Directly from Aluminum End-of-Life Vehicle Scrap
High-shear melt conditioning (HSMC) technology was used for degassing and de-ironing of an aluminum alloy recovered from the Zorba cast fraction of the non-ferrous scrap from shredded end-of-life vehicles. The results showed that the recovery of aluminum alloys from the Zorba cast fraction was more than 80%. High-shear melt conditioning improved the degassing process during melt treatment in comparison with the adding of degassing tablets. The efficiency of the de-ironing process using HSMC increased by up to 24% after, increasing the Mn content to 0.8% in the melt. Adding Mn to Zorba melt enhanced the de-ironing process and eliminated the formation of β-AlFeSi intermetallic particles, which have a detrimental effect on both the mechanical and corrosion properties of the alloy.
- 12 April 2021
- Published by SAGE Publications in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
- Vol. 56 (5) , 495-496
Obituary
Professor George Thompson, OBE, DSc, FREng (1946–2020)It is with deep sadness that we share the news that our dear friend and colleague, Professor George Edward Thompson, passed away after a long i...
- 12 April 2021
- Published by SAGE Publications in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
- Vol. 56 (5) , 495-496
Obituary
Professor George Thompson, OBE, DSc, FREng (1946–2020)It is with deep sadness that we share the news that our dear friend and colleague, Professor George Edward Thompson, passed away after a long i...
- Open Access
Direct Chill Casting and Extrusion of AA6111 Aluminum Alloy Formulated from Taint Tabor Scrap
AA6111 aluminum automotive body-sheet alloy has been formulated from 100% Taint Tabor scrap aluminum. Direct chill casting with and without high shear melt conditioning (HSMC) was used to produce the AA6111 alloy billets. Both homogenized and non-homogenized billets were extruded into sheets. The optical micrographs of the melt conditioned direct chill (MC-DC) samples showed refined equiaxed grains in comparison to direct chill (DC) cast and direct chill grain refined (DC-GR) samples. Optical metallography showed extensive peripheral coarse grain (PCG) for the DC, DC-GR and MC-DC planks extruded from the homogenized standard AA6111 billets while planks extruded from modified AA6111 billets (with recrystallization inhibitors) showed thin PCG band. The co-addition of recrystallization inhibitors Mn, Zr, and Cr with elimination of the billet homogenization step had a favorable impact on the microstructure of the AA6111 alloy following the extrusion process where a fibrous grain structure was retained across the whole section of the planks. The mechanical properties of as-cast planks extruded from non-homogenized billets were similar to those extruded from homogenized billets. Eliminating the homogenization heat treatment step prior to extrusion has important ramifications in terms of processing cost reduction.
Open AccessDirect Chill Casting and Extrusion of AA6111 Aluminum Alloy Formulated from Taint Tabor Scrap
AA6111 aluminum automotive body-sheet alloy has been formulated from 100% Taint Tabor scrap aluminum. Direct chill casting with and without high shear melt conditioning (HSMC) was used to produce the AA6111 alloy billets. Both homogenized and non-homogenized billets were extruded into sheets. The optical micrographs of the melt conditioned direct chill (MC-DC) samples showed refined equiaxed grains in comparison to direct chill (DC) cast and direct chill grain refined (DC-GR) samples. Optical metallography showed extensive peripheral coarse grain (PCG) for the DC, DC-GR and MC-DC planks extruded from the homogenized standard AA6111 billets while planks extruded from modified AA6111 billets (with recrystallization inhibitors) showed thin PCG band. The co-addition of recrystallization inhibitors Mn, Zr, and Cr with elimination of the billet homogenization step had a favorable impact on the microstructure of the AA6111 alloy following the extrusion process where a fibrous grain structure was retained across the whole section of the planks. The mechanical properties of as-cast planks extruded from non-homogenized billets were similar to those extruded from homogenized billets. Eliminating the homogenization heat treatment step prior to extrusion has important ramifications in terms of processing cost reduction.
- Open Access
Melt Conditioned Direct Chill (MC-DC) Casting and Extrusion of AA5754 Aluminium Alloy Formulated from Recycled Taint Tabor Scrap
The melt conditioned direct chill (MC-DC) casting process has been used to produce billets and extruded planks of AA5754 alloy formulated from 100% recycled Taint Tabor scrap aluminum. The billets were homogenized and then extruded into flat planks. Optical metallography of the MC-DC cast billets showed equiaxed refined grains in comparison to conventional direct chill (DC) cast and direct chill grain refined (DC-GR) cast billets formulated from the same Taint Tabor scrap. Microstructural evaluation of the extruded planks showed extensive peripheral coarse grain (PCG) for the DC, DC-GR and MC-DC cast planks. The 2 mm and 1 mm MC-DC cast planks produced after cold rolling and heat treatment showed a fully recrystallized microstructure at 380 °C and 300 °C for 10 min respectively with an improvement in mechanical properties over DC-GR cast and similarly processed planks. The as-extruded MC-DC cast planks tensile tested in the transverse direction showed 34% elongation and 213 MPa ultimate tensile strength. These tensile results showed 5.8% higher elongation and 1.2% higher ultimate tensile strength compared with the DC-GR planks after applying high shear melt conditioning.
Open AccessMelt Conditioned Direct Chill (MC-DC) Casting and Extrusion of AA5754 Aluminium Alloy Formulated from Recycled Taint Tabor Scrap
The melt conditioned direct chill (MC-DC) casting process has been used to produce billets and extruded planks of AA5754 alloy formulated from 100% recycled Taint Tabor scrap aluminum. The billets were homogenized and then extruded into flat planks. Optical metallography of the MC-DC cast billets showed equiaxed refined grains in comparison to conventional direct chill (DC) cast and direct chill grain refined (DC-GR) cast billets formulated from the same Taint Tabor scrap. Microstructural evaluation of the extruded planks showed extensive peripheral coarse grain (PCG) for the DC, DC-GR and MC-DC cast planks. The 2 mm and 1 mm MC-DC cast planks produced after cold rolling and heat treatment showed a fully recrystallized microstructure at 380 °C and 300 °C for 10 min respectively with an improvement in mechanical properties over DC-GR cast and similarly processed planks. The as-extruded MC-DC cast planks tensile tested in the transverse direction showed 34% elongation and 213 MPa ultimate tensile strength. These tensile results showed 5.8% higher elongation and 1.2% higher ultimate tensile strength compared with the DC-GR planks after applying high shear melt conditioning.
- Open Access
Melt Conditioned Direct Chill (MC-DC) Casting of AA-6111 Aluminium Alloy Formulated from Incinerator Bottom Ash (IBA)
The melt conditioned direct chill (MC-DC) casting process has been used for the production of billets of AA-6111 alloy formulated from recycled aluminium derived from incinerator bottom ash (IBA). The billets were homogenised and then extruded into planks. Optical metallography of the MC-DC billets showed equiaxed refined grains in comparison to DC and grain refined (DC-GR) billets formulated from the same scrap source. Microstructure evaluation for the extruded planks showed a less extensive peripheral coarse grain (PCG) for the MC-DC sample.
Open AccessMelt Conditioned Direct Chill (MC-DC) Casting of AA-6111 Aluminium Alloy Formulated from Incinerator Bottom Ash (IBA)
The melt conditioned direct chill (MC-DC) casting process has been used for the production of billets of AA-6111 alloy formulated from recycled aluminium derived from incinerator bottom ash (IBA). The billets were homogenised and then extruded into planks. Optical metallography of the MC-DC billets showed equiaxed refined grains in comparison to DC and grain refined (DC-GR) billets formulated from the same scrap source. Microstructure evaluation for the extruded planks showed a less extensive peripheral coarse grain (PCG) for the MC-DC sample.
- 3 May 2013
- Published by Wiley in Surface and Interface Analysis
- Vol. 45 (10) , 1430-1434
Surface treatment of aluminium automotive sheet: Mythology and technology
The use of aluminium automotive sheet to save weight, fuel and carbon emissions is increasing as EU OEMS strive to reach progressively tougher targets and from the need to avoid fleet average penalty payments. Surface finishing of structural sheet for alloys like AA5754 generally involves cleaning and pretreatment followed by roll coating with a lubricant. For alloys supplied for body panels like AA6016 and its variants, surface treatments can include a mechanical texturing treatment followed by cleaning and pretreatment with a stabilising treatment and then spray coating with a dry film lubricant. Surface finishing capacity in the EU is now available on six finishing lines with an estimated total capacity of about 350 kt/year. This is just about in balance with present demand, but the capacity of the existing lines will soon be exceeded by the rapidly increasing demand. Further finishing lines will be required to keep pace with the increasing demand. There is a difficult balance to achieve between cost and finishing process complexity and the demanding requirements of formability, adhesive bond durability and surface appearance specified by the automotive companies in the EU. It is important to understand the need and value of each of the finishing treatments considered to be essential for automotive sheet supply in the EU compared to the less stringent requirements applied in North America and Japan. The complex microstructural and technological issues surrounding surface finishing and sheet performance will be analysed and discussed in detail and opportunities identified. Copyright © 2013 John Wiley & Sons, Ltd.
- 3 May 2013
- Published by Wiley in Surface and Interface Analysis
- Vol. 45 (10) , 1430-1434
Surface treatment of aluminium automotive sheet: Mythology and technology
The use of aluminium automotive sheet to save weight, fuel and carbon emissions is increasing as EU OEMS strive to reach progressively tougher targets and from the need to avoid fleet average penalty payments. Surface finishing of structural sheet for alloys like AA5754 generally involves cleaning and pretreatment followed by roll coating with a lubricant. For alloys supplied for body panels like AA6016 and its variants, surface treatments can include a mechanical texturing treatment followed by cleaning and pretreatment with a stabilising treatment and then spray coating with a dry film lubricant. Surface finishing capacity in the EU is now available on six finishing lines with an estimated total capacity of about 350 kt/year. This is just about in balance with present demand, but the capacity of the existing lines will soon be exceeded by the rapidly increasing demand. Further finishing lines will be required to keep pace with the increasing demand. There is a difficult balance to achieve between cost and finishing process complexity and the demanding requirements of formability, adhesive bond durability and surface appearance specified by the automotive companies in the EU. It is important to understand the need and value of each of the finishing treatments considered to be essential for automotive sheet supply in the EU compared to the less stringent requirements applied in North America and Japan. The complex microstructural and technological issues surrounding surface finishing and sheet performance will be analysed and discussed in detail and opportunities identified. Copyright © 2013 John Wiley & Sons, Ltd.