Ashok Kumar Ray
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Ashok Kumar Ray has a total of 17 co-authors. Here are the top co-authors by number of shared publications:
Nilima Roy
2 shared publications- Arpan Das
Bhabha Atomic Research Centre, Mumbai, India
1 shared publication B. Ravi Kumar
National Metallurgical Laboratory (CSIR), Jamshedpur-831007, India
1 shared publicationBangsidhar Goswami
R.V.S. College of Engineering and Technology, Jamshedpur-831012, India
1 shared publicationByomkesh Dash
National Metallurgical Laboratory (CSIR), Jamshedpur-831007, India
1 shared publicationDeepak Kumar Das
Defence Metallurgical Research Laboratory, Hyderabad-500058, India
1 shared publication
Latest Publications
- 1 March 2018
- Published by Walter de Gruyter GmbH
Stress Analysis and Creep Behavior of Service Exposed Primary Superheater Tube in a Thermal Power Plant
The elastic, inelastic deformation and stress distribution pattern of a seventeen years service exposed primary superheater tube in a 120 MW boiler of a thermal power plant have been evaluated by using both analytical and numerical techniques. The commercial finite element computer code ANSYS was used for stress analysis. The methodology is a valuable design tool for development of new boiler tubes as well as for considering the effects of numerous operating variables on creep life. The health of the tube was also assessed based on microstructure, hardness and a few conventional creep tests carried out at 500°C at various stress levels (40–177 MPa). Results revealed that there was not much variation in the microstructure and hardness of the service exposed tubes compared to the virgin material. Creep deformation behavior of the service exposed and virgin tubes of the same material at 40 MPa reveal that deterioration of the creep properties fall within the 20% scatter band, which is well within the specified limits of ASTM standard. The service exposed primary superheater tube is thus in a good state of health.
- 1 March 2018
- Published by Walter de Gruyter GmbH
Stress Analysis and Creep Behavior of Service Exposed Primary Superheater Tube in a Thermal Power Plant
The elastic, inelastic deformation and stress distribution pattern of a seventeen years service exposed primary superheater tube in a 120 MW boiler of a thermal power plant have been evaluated by using both analytical and numerical techniques. The commercial finite element computer code ANSYS was used for stress analysis. The methodology is a valuable design tool for development of new boiler tubes as well as for considering the effects of numerous operating variables on creep life. The health of the tube was also assessed based on microstructure, hardness and a few conventional creep tests carried out at 500°C at various stress levels (40–177 MPa). Results revealed that there was not much variation in the microstructure and hardness of the service exposed tubes compared to the virgin material. Creep deformation behavior of the service exposed and virgin tubes of the same material at 40 MPa reveal that deterioration of the creep properties fall within the 20% scatter band, which is well within the specified limits of ASTM standard. The service exposed primary superheater tube is thus in a good state of health.
- 14 January 2012
- Published by Walter de Gruyter GmbH in High Temperature Materials and Processes
- Vol. 31 (6) , 691-699
High Cycle Fatigue and Cyclic Plastic Deformation Behaviour of High Temperature Oxidation Resistant Titanium Aluminide Coated IMI 834 Alloy at 873 K
High cycle and force-controlled (HCF) as well as low cycle fatigue (LCF) behaviour of titanium alloy IMI 834 was comparatively studied in bare condition and with titanium aluminide (Al2Ti) coating, at 873 K in air, for compressor disc of aero engines. HCF testing of bare and Al2Ti coated IMI 834 alloy at 873 K in air revealed that the coated materials has higher lifetime than the bare alloy. However, for low cycle, high stress lifetimes, the unprotected bare alloy is stronger, possibly due to early crack formation and growth in coated layer. In the case of LCF tests at higher values of total strain amplitudes Al2Ti coated IMI 834 alloy has longer fatigue life (Nf) as compared to the bare IMI 834 alloy which appears to be due to load shifting to the coat, but at lower values of total strain amplitude, Al2Ti coating on IMI 834 alloy seems to have no effect on Nf . Higher values of cyclic strength coefficient (K′) and cyclic hardening exponent (n′) for coated IMI 834 alloy indicate that coating offers resistance to cyclic plastic deformation at 873 K in air, and hence is beneficial. The coating adheres well to the substrate and is also fairly resistant to high temperature corrosion in sea water atmosphere at 873 K.
- 14 January 2012
- Published by Walter de Gruyter GmbH in High Temperature Materials and Processes
- Vol. 31 (6) , 691-699
High Cycle Fatigue and Cyclic Plastic Deformation Behaviour of High Temperature Oxidation Resistant Titanium Aluminide Coated IMI 834 Alloy at 873 K
High cycle and force-controlled (HCF) as well as low cycle fatigue (LCF) behaviour of titanium alloy IMI 834 was comparatively studied in bare condition and with titanium aluminide (Al2Ti) coating, at 873 K in air, for compressor disc of aero engines. HCF testing of bare and Al2Ti coated IMI 834 alloy at 873 K in air revealed that the coated materials has higher lifetime than the bare alloy. However, for low cycle, high stress lifetimes, the unprotected bare alloy is stronger, possibly due to early crack formation and growth in coated layer. In the case of LCF tests at higher values of total strain amplitudes Al2Ti coated IMI 834 alloy has longer fatigue life (Nf) as compared to the bare IMI 834 alloy which appears to be due to load shifting to the coat, but at lower values of total strain amplitude, Al2Ti coating on IMI 834 alloy seems to have no effect on Nf . Higher values of cyclic strength coefficient (K′) and cyclic hardening exponent (n′) for coated IMI 834 alloy indicate that coating offers resistance to cyclic plastic deformation at 873 K in air, and hence is beneficial. The coating adheres well to the substrate and is also fairly resistant to high temperature corrosion in sea water atmosphere at 873 K.
- 27 April 2006
- Published by Elsevier in Materials Characterization
- Vol. 57 (3) , 199-209
Characterization of bond coat in a thermal barrier coated superalloy used in combustor liners of aero engines
- 27 April 2006
- Published by Elsevier in Materials Characterization
- Vol. 57 (3) , 199-209
Characterization of bond coat in a thermal barrier coated superalloy used in combustor liners of aero engines