Ming Chen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Ming Chen has a total of 32 co-authors. Here are the top co-authors by number of shared publications:
Chi He Chen
Department of Materials and Optoelectronic Science, National Sun Yat-Sen University, Kaohsiung 80424, Taiwan, Republic of China
6 shared publicationsHsin‐Ying Lu
Department of Materials and Optoelectronic Science, National Sun Yat-Sen University, Kaohsiung 80424, Taiwan, Republic of China
6 shared publicationsChia‐Jung Tsai
Department of Materials and Optoelectronic Science, National Sun Yat-Sen University, Kaohsiung 80424, Taiwan, Republic of China
4 shared publicationsShih‐Fu Lu
Department of Materials and Optoelectronic Science, National Sun Yat-Sen University, Kaohsiung 80424, Taiwan, Republic of China
4 shared publications- Chang-Mou Wu
Department of Materials Science and Engineering, National Taiwan University of Science and Technology, Taipei 10607, Taiwan
2 shared publications Chao‐Sen Yang
Institute of Materials Science and Engineering, National Sun Yat-Sen University, Kaohsiung 80424, Taiwan, Republic of China
2 shared publications
Latest Publications
- 21 September 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 123 (6) , 3610-3619
Mechanisms and kinetics of thermal degradation of poly(butylene succinate‐co‐propylene succinate)s
Poly(butylene succinate) (PBSu) and two PBSu‐rich poly(butylene succinate‐co‐propylene succinate)s were studied. Copolyesters were characterized as random copolymers, based on 13C‐NMR spectra. TGA‐FTIR was used to monitor the degradation products at a heating rate of 5°C/min under N2. FTIR spectra revealed that the major products were anhydrides, which were formed following two cyclic intramolecular degradation mechanisms by the breaking of the weak O‐CH2 bonds around succinate groups. Thermal stability at heating rates of 1, 3, 5, and 10°C/min under N2 was investigated using TGA. The model‐free methods of the Friedman and Ozawa equations are useful for studying the activation energy of degradation in each period of mass loss. The results reveal that the random incorporation of minor propylene succinate units into PBSu did not markedly affect their thermal resistance. Two model‐fitting mechanisms were used to determine the mass loss function f(α), the activation energy and the associated mechanism. The mechanism of autocatalysis nth‐order, with f(α) = αm(1 − α)n, fitted the experimental data much more closely than did the nth‐order mechanism given by f(α) = (1 − α)n. The obtained activation energy was used to estimate the failure temperature (Tf). The values of Tf for a mass loss of 5% and an endurance time of 60,000 h are 160.7, 155.5, and 159.3°C for PBSu and two the copolyesters, respectively. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012
- 21 September 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 123 (6) , 3610-3619
Mechanisms and kinetics of thermal degradation of poly(butylene succinate‐co‐propylene succinate)s
Poly(butylene succinate) (PBSu) and two PBSu‐rich poly(butylene succinate‐co‐propylene succinate)s were studied. Copolyesters were characterized as random copolymers, based on 13C‐NMR spectra. TGA‐FTIR was used to monitor the degradation products at a heating rate of 5°C/min under N2. FTIR spectra revealed that the major products were anhydrides, which were formed following two cyclic intramolecular degradation mechanisms by the breaking of the weak O‐CH2 bonds around succinate groups. Thermal stability at heating rates of 1, 3, 5, and 10°C/min under N2 was investigated using TGA. The model‐free methods of the Friedman and Ozawa equations are useful for studying the activation energy of degradation in each period of mass loss. The results reveal that the random incorporation of minor propylene succinate units into PBSu did not markedly affect their thermal resistance. Two model‐fitting mechanisms were used to determine the mass loss function f(α), the activation energy and the associated mechanism. The mechanism of autocatalysis nth‐order, with f(α) = αm(1 − α)n, fitted the experimental data much more closely than did the nth‐order mechanism given by f(α) = (1 − α)n. The obtained activation energy was used to estimate the failure temperature (Tf). The values of Tf for a mass loss of 5% and an endurance time of 60,000 h are 160.7, 155.5, and 159.3°C for PBSu and two the copolyesters, respectively. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012
- 8 January 2011
- Published by Springer Nature in Journal of Polymer Research
- Vol. 18 (6) , 1527-1537
Nonisothermal crystallization kinetics of novel biodegradable poly(butylene succinate-co-2-methyl-1,3-propylene succinate)s
- 8 January 2011
- Published by Springer Nature in Journal of Polymer Research
- Vol. 18 (6) , 1527-1537
Nonisothermal crystallization kinetics of novel biodegradable poly(butylene succinate-co-2-methyl-1,3-propylene succinate)s
- 14 May 2010
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 48 (12) , 1299-1308
Nonisothermal crystallization kinetics of biodegradable poly(butylene succinate‐co‐propylene succinate)s
Poly(butylene succinate) (PBSu) and two poly(butylene succinate‐co‐propylene succinate)s were synthesized via the direct polycondensation reaction. The copolyesters were characterized as having 7.0.and 11.5 mol % propylene succinate (PS) units, respectively, by 1H NMR. A differential scanning calorimeter (DSC) and a polarized light microscope (PLM) adopted to study the nonisothermal crystallization of these polyesters at a cooling rate of 1, 2, 3, 5, 6, and 10 °C/min. Morphology and the isothermal growth rates of spherulites under PLM experiments were monitored and obtained by curve‐fitting. These continuous rate data were analyzed with the Lauritzen−Hoffman equation. A transition of regime II → III was found at 95.6, 84.4, and 77.3 °C for PBSu, PBPSu 95/5, and PBPSu 90/10, respectively. DSC exothermic curves show that all of the nonisothermal crystallization occurred in regime III. DSC data were analyzed using modified Avrami, Ozawa, Mo, Friedman, and Vyazovkin equations. All the results of PLM and DSC measurements indicate that incorporation of minor PS units into PBSu markedly inhibits the crystallization of the resulting polymer. © 2010 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 48: 1299–1308, 2010
- 14 May 2010
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 48 (12) , 1299-1308
Nonisothermal crystallization kinetics of biodegradable poly(butylene succinate‐co‐propylene succinate)s
Poly(butylene succinate) (PBSu) and two poly(butylene succinate‐co‐propylene succinate)s were synthesized via the direct polycondensation reaction. The copolyesters were characterized as having 7.0.and 11.5 mol % propylene succinate (PS) units, respectively, by 1H NMR. A differential scanning calorimeter (DSC) and a polarized light microscope (PLM) adopted to study the nonisothermal crystallization of these polyesters at a cooling rate of 1, 2, 3, 5, 6, and 10 °C/min. Morphology and the isothermal growth rates of spherulites under PLM experiments were monitored and obtained by curve‐fitting. These continuous rate data were analyzed with the Lauritzen−Hoffman equation. A transition of regime II → III was found at 95.6, 84.4, and 77.3 °C for PBSu, PBPSu 95/5, and PBPSu 90/10, respectively. DSC exothermic curves show that all of the nonisothermal crystallization occurred in regime III. DSC data were analyzed using modified Avrami, Ozawa, Mo, Friedman, and Vyazovkin equations. All the results of PLM and DSC measurements indicate that incorporation of minor PS units into PBSu markedly inhibits the crystallization of the resulting polymer. © 2010 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 48: 1299–1308, 2010
- 22 March 2010
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 48 (9) , 932-939
Crystal growth rates and master curves of poly(ethylene succinate) and its copolyesters using a nonisothermal method
The spherulitic growth of poly(ethylene succinate) (PES) and two PES‐rich copolyesters at constant cooling rate was monitored and recorded using a system of polarized light microscope. Individual experiment of these polyesters lasted 40, 60, and 120 min, respectively. A continuous curve of isothermal growth rates between the melting and glass transition temperatures can be obtained after curve fitting procedures. These curves fit very well with those data points determined in the isothermal experiments, which are time consuming. The continuous data of PES was analyzed with the Hoffman (Lauritzen equation. A transition of regime II → III was found at 70.7 °C, which is very close to the literature values. The maximum growth rate was formulated in the Arrhenius and WLF expressions for the molecular transport term. A master curve of crystal growth rate for PES was constructed based on the continuous data of PES. When the reduced growth rates after normalization were plotted against the reduced temperatures, a universal master curve was observed for PES and two PES‐rich copolyesters. This nonisothermal method provides an efficient and reliable way for studying the crystallization kinetics of polymer and for constructing a universal master curve of crystal growth rate of PES. © 2010 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 48: 932–939, 2010
- 22 March 2010
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 48 (9) , 932-939
Crystal growth rates and master curves of poly(ethylene succinate) and its copolyesters using a nonisothermal method
The spherulitic growth of poly(ethylene succinate) (PES) and two PES‐rich copolyesters at constant cooling rate was monitored and recorded using a system of polarized light microscope. Individual experiment of these polyesters lasted 40, 60, and 120 min, respectively. A continuous curve of isothermal growth rates between the melting and glass transition temperatures can be obtained after curve fitting procedures. These curves fit very well with those data points determined in the isothermal experiments, which are time consuming. The continuous data of PES was analyzed with the Hoffman (Lauritzen equation. A transition of regime II → III was found at 70.7 °C, which is very close to the literature values. The maximum growth rate was formulated in the Arrhenius and WLF expressions for the molecular transport term. A master curve of crystal growth rate for PES was constructed based on the continuous data of PES. When the reduced growth rates after normalization were plotted against the reduced temperatures, a universal master curve was observed for PES and two PES‐rich copolyesters. This nonisothermal method provides an efficient and reliable way for studying the crystallization kinetics of polymer and for constructing a universal master curve of crystal growth rate of PES. © 2010 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 48: 932–939, 2010
- 22 February 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 116 (6) , 3693-3701
Biodegradable poly(ethylene succinate) blends and copolymers containing minor amounts of poly(butylene succinate)
Poly(ethylene succinate) (PES), poly(butylene succinate) (PBS), and PES‐rich copolyesters were synthesized using an effective catalyst, titanium tetraisopropoxide. PES was blended with minor amounts of PBS for the comparison. The compositions of the copolyesters and the blends were determined from NMR spectra. Their thermal properties were studied using a differential scanning calorimeter (DSC), a temperature modulated DSC (TMDSC), and a thermogravimetric analyzer. No significant difference exists among the thermal stabilities of these polyesters and blends. For the blends, the reversible curves of TMDSC showed a distinct glass‐rubber transition temperature (Tg), however, the variation of the Tg values with the blend compositions was small. Isothermal crystallization kinetics and the melting behavior after crystallization were examined using DSC. Wide‐angle X‐ray diffractograms (WAXD) were obtained for the isothermally crystallized specimens. The results of DSC and WAXD indicate that the blends have a higher degree of crystallinity and a higher melting temperature than those of the corresponding copolymers. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 22 February 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 116 (6) , 3693-3701
Biodegradable poly(ethylene succinate) blends and copolymers containing minor amounts of poly(butylene succinate)
Poly(ethylene succinate) (PES), poly(butylene succinate) (PBS), and PES‐rich copolyesters were synthesized using an effective catalyst, titanium tetraisopropoxide. PES was blended with minor amounts of PBS for the comparison. The compositions of the copolyesters and the blends were determined from NMR spectra. Their thermal properties were studied using a differential scanning calorimeter (DSC), a temperature modulated DSC (TMDSC), and a thermogravimetric analyzer. No significant difference exists among the thermal stabilities of these polyesters and blends. For the blends, the reversible curves of TMDSC showed a distinct glass‐rubber transition temperature (Tg), however, the variation of the Tg values with the blend compositions was small. Isothermal crystallization kinetics and the melting behavior after crystallization were examined using DSC. Wide‐angle X‐ray diffractograms (WAXD) were obtained for the isothermally crystallized specimens. The results of DSC and WAXD indicate that the blends have a higher degree of crystallinity and a higher melting temperature than those of the corresponding copolymers. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 20 February 2010
- Published by Springer Nature in Colloid and Polymer Science
- Vol. 288 (7) , 731-738
Synthesis and characterization of poly(butylene succinate) and its copolyesters containing minor amounts of propylene succinate
- 20 February 2010
- Published by Springer Nature in Colloid and Polymer Science
- Vol. 288 (7) , 731-738
Synthesis and characterization of poly(butylene succinate) and its copolyesters containing minor amounts of propylene succinate
- 30 March 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 113 (2) , 876-886
Characterization, crystallization kinetics, and melting behavior of poly(ethylene succinate) copolyester containing 7 mol % butylene succinate
The copolyester was synthesized and characterized as having 92.7 mol % ethylene succinate units and 7.3 mol % butylene succinate (BS) units in a random sequence, as determined by the use of nuclear magnetic resonance. Isothermal crystallization kinetics of this copolyester was examined in the temperature range (Tc) from 30 to 80°C with the use of differential scanning calorimetry (DSC). The melting behavior after isothermal crystallization was studied with DSC by varying the Tc, the heating rate, and the crystallization time. The complex melting behavior involves both mechanisms of various lamellar crystals and melting–recrystallization–remelting. As the Tc increases, the contribution of recrystallization gradually decreases and finally disappears. The Hoffman–Weeks linear plot yielded an equilibrium melting temperature of 111.1°C, which is 1.6°C less than that of poly(ethylene succinate) (PES). The kinetic analysis of the spherulitic growth rates (G) indicated that a regime II→III transition occurred at ∼59°C (TII→III), which is ∼ 11°C less than that of PES. The overall crystallization rate, TII→III and G indicate that the random incorporation of only 7.3 mol % BS units into PES significantly inhibits the crystallization rate of PES. Finally, the morphology of melt‐crystallized samples was examined using polarized light microscopy and scanning electron microscopy. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009
- 30 March 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 113 (2) , 876-886
Characterization, crystallization kinetics, and melting behavior of poly(ethylene succinate) copolyester containing 7 mol % butylene succinate
The copolyester was synthesized and characterized as having 92.7 mol % ethylene succinate units and 7.3 mol % butylene succinate (BS) units in a random sequence, as determined by the use of nuclear magnetic resonance. Isothermal crystallization kinetics of this copolyester was examined in the temperature range (Tc) from 30 to 80°C with the use of differential scanning calorimetry (DSC). The melting behavior after isothermal crystallization was studied with DSC by varying the Tc, the heating rate, and the crystallization time. The complex melting behavior involves both mechanisms of various lamellar crystals and melting–recrystallization–remelting. As the Tc increases, the contribution of recrystallization gradually decreases and finally disappears. The Hoffman–Weeks linear plot yielded an equilibrium melting temperature of 111.1°C, which is 1.6°C less than that of poly(ethylene succinate) (PES). The kinetic analysis of the spherulitic growth rates (G) indicated that a regime II→III transition occurred at ∼59°C (TII→III), which is ∼ 11°C less than that of PES. The overall crystallization rate, TII→III and G indicate that the random incorporation of only 7.3 mol % BS units into PES significantly inhibits the crystallization rate of PES. Finally, the morphology of melt‐crystallized samples was examined using polarized light microscopy and scanning electron microscopy. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009
- 17 February 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 112 (4) , 2305-2314
Crystallization kinetics and melting behavior of poly[(trimethylene terephthalate)‐co‐(29 mol % ethylene terephthalate)] copolyester
- 17 February 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 112 (4) , 2305-2314
Crystallization kinetics and melting behavior of poly[(trimethylene terephthalate)‐co‐(29 mol % ethylene terephthalate)] copolyester
- 30 October 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 111 (3) , 1433-1439
Synthesis and characterization of poly(ethylene succinate) and its copolyesters containing minor amounts of butylene succinate
Poly(ethylene succinate) (PES) and its copolyesters that contain 7, 10, or 48 mol % butylene succinate (BS) were synthesized through a direct polycondensation reaction with titanium tetraisopropoxide as the catalyst. Measurements of intrinsic viscosity (1.08–1.27 dL/g) proved the success of the preparation of polyesters with high molecular weights. The compositions and the sequence distributions of the copolyesters were determined from 1H and 13C NMR spectra. The distributions of ethylene succinate and BS units were found to be random. Their thermal properties were elucidated using a differential scanning calorimeter (DSC) and a thermogravimetric analyzer. No significant difference exists among the thermal stabilities of these polyesters. All of the copolymers exhibit a single glass transition temperature. Wide‐angle X‐ray diffractograms (WAXD) were obtained from polyesters that were crystallized isothermally. The DSC thermograms and WAXD patterns indicate that the incorporation of BS units into PES significantly inhibits the crystallization behavior of PES. The heat of fusion of ideal PES crystals is 163 J/g, as determined by the depression of the melting point of PES crystals in acetophenone. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2009
- 30 October 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 111 (3) , 1433-1439
Synthesis and characterization of poly(ethylene succinate) and its copolyesters containing minor amounts of butylene succinate
Poly(ethylene succinate) (PES) and its copolyesters that contain 7, 10, or 48 mol % butylene succinate (BS) were synthesized through a direct polycondensation reaction with titanium tetraisopropoxide as the catalyst. Measurements of intrinsic viscosity (1.08–1.27 dL/g) proved the success of the preparation of polyesters with high molecular weights. The compositions and the sequence distributions of the copolyesters were determined from 1H and 13C NMR spectra. The distributions of ethylene succinate and BS units were found to be random. Their thermal properties were elucidated using a differential scanning calorimeter (DSC) and a thermogravimetric analyzer. No significant difference exists among the thermal stabilities of these polyesters. All of the copolymers exhibit a single glass transition temperature. Wide‐angle X‐ray diffractograms (WAXD) were obtained from polyesters that were crystallized isothermally. The DSC thermograms and WAXD patterns indicate that the incorporation of BS units into PES significantly inhibits the crystallization behavior of PES. The heat of fusion of ideal PES crystals is 163 J/g, as determined by the depression of the melting point of PES crystals in acetophenone. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2009
- 9 October 2008
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 46 (22) , 2431-2442
Characterization, crystallization kinetics, and melting behavior of poly(ethylene succinate) copolyester containing 10 mol % butylene succinate
Copolyester was synthesized and characterized as having 89.9 mol % ethylene succinate units and 10.1 mol % butylene succinate units in a random sequence, as revealed by NMR. Isothermal crystallization kinetics was studied in the temperature range (Tc) from 30 to 73 °C using differential scanning calorimetry (DSC). The melting behavior after isothermal crystallization was investigated using DSC by varying the Tc, the heating rate and the crystallization time. DSC curves showed triple melting peaks. The melting behavior indicates that the upper melting peaks are associated primarily with the melting of lamellar crystals with various stabilities. As the Tc increases, the contribution of recrystallization slowly decreases and finally disappears. A Hoffman‐Weeks linear plot gives an equilibrium melting temperature of 107.0 °C. The spherulite growth of this copolyester from 80 to 20 °C at a cooling rate of 2 or 4 °C/min was monitored and recorded using an optical microscope equipped with a CCD camera. Continuous growth rates between melting and glass transition temperatures can be obtained after curve‐fitting procedures. These data fit well with those data points measured in the isothermal experiments. These data were analyzed with the Hoffman and Lauritzen theory. A regime II → III transition was detected at around 52 °C. © 2008 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 46: 2431–2442, 2008
- 9 October 2008
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 46 (22) , 2431-2442
Characterization, crystallization kinetics, and melting behavior of poly(ethylene succinate) copolyester containing 10 mol % butylene succinate
Copolyester was synthesized and characterized as having 89.9 mol % ethylene succinate units and 10.1 mol % butylene succinate units in a random sequence, as revealed by NMR. Isothermal crystallization kinetics was studied in the temperature range (Tc) from 30 to 73 °C using differential scanning calorimetry (DSC). The melting behavior after isothermal crystallization was investigated using DSC by varying the Tc, the heating rate and the crystallization time. DSC curves showed triple melting peaks. The melting behavior indicates that the upper melting peaks are associated primarily with the melting of lamellar crystals with various stabilities. As the Tc increases, the contribution of recrystallization slowly decreases and finally disappears. A Hoffman‐Weeks linear plot gives an equilibrium melting temperature of 107.0 °C. The spherulite growth of this copolyester from 80 to 20 °C at a cooling rate of 2 or 4 °C/min was monitored and recorded using an optical microscope equipped with a CCD camera. Continuous growth rates between melting and glass transition temperatures can be obtained after curve‐fitting procedures. These data fit well with those data points measured in the isothermal experiments. These data were analyzed with the Hoffman and Lauritzen theory. A regime II → III transition was detected at around 52 °C. © 2008 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 46: 2431–2442, 2008