Douglas E. Hirt
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Douglas E. Hirt has a total of 31 co-authors. Here are the top co-authors by number of shared publications:
Amol V. Janorkar
Department of Chemical Engineering and Center for Advanced Engineering Fibers & Films, Clemson University, Clemson, South Carolina 29634-0909
7 shared publicationsRahul M. Rasal
Department of Chemical and Biomolecular Engineering and Center for Advanced Engineering Fibers and Films, Clemson University, Clemson, SC 29634
5 shared publicationsNing Luo
Department of Chemical and Biomolecular Engineering, Center for Advanced Engineering Fibers and Films, Clemson University, Clemson, SC 29634-0909, USA
4 shared publicationsAndrew T. Metters
Department of Chemical Engineering and Center for Advanced Engineering Fibers & Films, Clemson University, Clemson, South Carolina 29634-0909
3 shared publicationsChun Zhang
Department of Chemical and Biomolecular Engineering, Center for Advanced Engineering Fibers and Films, Clemson University, Clemson, South Carolina 29634-0909, United States
3 shared publicationsDwight W. Schwark
Cryovac Division of Sealed Air Corporation, Duncan, South Carolina 29334 USA
3 shared publications
Latest Publications
- 8 September 2014
- Published by Wiley in Polymer Engineering & Science
- Vol. 55 (7) , 1652-1660
Degradation of PLA fibers at elevated temperature and humidity
The hydrolytic degradation of poly(lactic acid) (PLA) devices has previously been reported as size dependent for devices such as plates, microspheres, and films between 2 and 0.3 mm in thickness or diameter. In this study, the effect of fiber diameter on the degradation characteristics of PLA fiber of two diameters, 32 µm (PLA32) and 118 µm (PLA118), aged at 40, 60, and 80°C with 100% relative humidity, was investigated. Additionally, both PLA32 and PLA118 were aged at 40 and 60°C under nitrogen purge. The degradation of the fibers was evaluated based on changes in the total weight, crystallinity, and molecular weight of the samples. Both diameters exhibited similar total weight loss, crystallinity, and molecular weight loss profiles under each set of degradation conditions. Two models for the change in molecular weight were compared: a first order model and an autocatalytic model. For the obtained data, both models provided a reasonable fit of the molecular weight data. Based on the rate constants obtained for each model, the activation energy for PLA degradation was calculated (26.3 kcal mol−1 for the first order model and 22.4 kcal mol−1 for the autocatalytic model). The activation energies obtained were close to other values reported in the literature for PLA hydrolysis. POLYM. ENG. SCI., 55:1652–1660, 2015. © 2014 Society of Plastics Engineers
- 8 September 2014
- Published by Wiley in Polymer Engineering & Science
- Vol. 55 (7) , 1652-1660
Degradation of PLA fibers at elevated temperature and humidity
The hydrolytic degradation of poly(lactic acid) (PLA) devices has previously been reported as size dependent for devices such as plates, microspheres, and films between 2 and 0.3 mm in thickness or diameter. In this study, the effect of fiber diameter on the degradation characteristics of PLA fiber of two diameters, 32 µm (PLA32) and 118 µm (PLA118), aged at 40, 60, and 80°C with 100% relative humidity, was investigated. Additionally, both PLA32 and PLA118 were aged at 40 and 60°C under nitrogen purge. The degradation of the fibers was evaluated based on changes in the total weight, crystallinity, and molecular weight of the samples. Both diameters exhibited similar total weight loss, crystallinity, and molecular weight loss profiles under each set of degradation conditions. Two models for the change in molecular weight were compared: a first order model and an autocatalytic model. For the obtained data, both models provided a reasonable fit of the molecular weight data. Based on the rate constants obtained for each model, the activation energy for PLA degradation was calculated (26.3 kcal mol−1 for the first order model and 22.4 kcal mol−1 for the autocatalytic model). The activation energies obtained were close to other values reported in the literature for PLA hydrolysis. POLYM. ENG. SCI., 55:1652–1660, 2015. © 2014 Society of Plastics Engineers
- 12 March 2010
- Published by Wiley in Macromolecular Materials and Engineering
- Vol. 295 (3) , 204-209
Poly(lactic acid) Toughening with a Better Balance of Properties
Poly(lactic acid) (PLA) toughening is often associated with significant modulus and/or strength losses making it unsuitable for many consumer and biomedical applications. The major objective of this research was to toughen PLA without significant loss in modulus and strength and to introduce reactive acid groups using reactive blending of PLA with a combination of polymers. PLA was reactive blended with poly(acrylic acid) (PAA) followed by physical blending with poly(ethylene glycol) (PEG) in solution. The modified PLA was extruded into films using a co‐rotating twin‐screw extruder and characterized using tensile testing, differential scanning calorimetry (DSC), and dynamic mechanical analyses (DMA). This technology resulted in films with a ten‐fold increase in toughness compared to neat PLA with little or no decrease in strength and modulus. magnified image
- 12 March 2010
- Published by Wiley in Macromolecular Materials and Engineering
- Vol. 295 (3) , 204-209
Poly(lactic acid) Toughening with a Better Balance of Properties
Poly(lactic acid) (PLA) toughening is often associated with significant modulus and/or strength losses making it unsuitable for many consumer and biomedical applications. The major objective of this research was to toughen PLA without significant loss in modulus and strength and to introduce reactive acid groups using reactive blending of PLA with a combination of polymers. PLA was reactive blended with poly(acrylic acid) (PAA) followed by physical blending with poly(ethylene glycol) (PEG) in solution. The modified PLA was extruded into films using a co‐rotating twin‐screw extruder and characterized using tensile testing, differential scanning calorimetry (DSC), and dynamic mechanical analyses (DMA). This technology resulted in films with a ten‐fold increase in toughness compared to neat PLA with little or no decrease in strength and modulus. magnified image
- Open Access
- 1 October 2009
- Published by Wiley in Macromolecular Bioscience
- Vol. 9 (10)
Macromol. Biosci. 10/2009
- 1 October 2009
- Published by Wiley in Macromolecular Bioscience
- Vol. 9 (10)
Open AccessMacromol. Biosci. 10/2009
- 30 September 2009
- Published by Wiley in Macromolecular Bioscience
- Vol. 9 (10) , 989-996
Micropatterning of Covalently Attached Biotin on Poly(lactic acid) Film Surfaces
A two‐step approach was used to micropattern covalently attached biotin on the surface of poly(lactic acid) (PLA) film. Poly(acrylic acid) (PAA) was micropatterned on PLA using photolithography in step 1, followed by carbodiimide wet chemistry to covalently attach biotin to acid groups in step 2. The PAA micropatterning reaction progression was monitored using attenuated total reflectance‐Fourier transform infrared (ATR‐FT‐IR) spectroscopy, water contact angle goniometry, and atomic force microscopy (AFM). The PAA‐biotin conjugation reaction characterization using XPS confirmed the carbodiimide mediated amidation reaction. The resultant PLA film was then immersed into a solution of fluorescence‐conjugated streptavidin and examined under fluorescence microscopy to reveal various micropatterns magnified image
- 30 September 2009
- Published by Wiley in Macromolecular Bioscience
- Vol. 9 (10) , 989-996
Micropatterning of Covalently Attached Biotin on Poly(lactic acid) Film Surfaces
A two‐step approach was used to micropattern covalently attached biotin on the surface of poly(lactic acid) (PLA) film. Poly(acrylic acid) (PAA) was micropatterned on PLA using photolithography in step 1, followed by carbodiimide wet chemistry to covalently attach biotin to acid groups in step 2. The PAA micropatterning reaction progression was monitored using attenuated total reflectance‐Fourier transform infrared (ATR‐FT‐IR) spectroscopy, water contact angle goniometry, and atomic force microscopy (AFM). The PAA‐biotin conjugation reaction characterization using XPS confirmed the carbodiimide mediated amidation reaction. The resultant PLA film was then immersed into a solution of fluorescence‐conjugated streptavidin and examined under fluorescence microscopy to reveal various micropatterns magnified image
- 1 April 2009
- Published by SAGE Publications in Textile Research Journal
- Vol. 79 (6) , 534-547
Improving the Wettability of Deep-Groove Polypropylene Fibers by Photografting
This paper presented photografting as a surface modification method to provide permanent wettability improvement to deep-groove polypropylene (PP) fibers. We also evaluated their wettability by testing the dynamic contact angle (DCA) on single fibers and characterized the wicking performance of fiber bundles when polyacrylamide (PAAm) and polyacrylic acid (PAA) were grafted onto the fibers. In this study, the increase in monomer concentration was found more effective than longer UV exposure time in creating higher graft density on deep-groove PP fibers. Acrylic acid (AA) monomers penetrated into the fiber and polymerized inside, but acrylamide (AAm) did not. Fiber dimension changed slightly upon grafting of PAAm, and enlarged significantly after grafting with PAA. DCA results show that the advancing water contact angle on single fibers decreased from 100 to 55° by grafting of PAAm and PAA, and spontaneous wicking of water was observed after surface modification. The wicking amount of the vertically placed fiber bundles showed a linear relationship to the square root of time at early wicking times.
- 1 April 2009
- Published by SAGE Publications in Textile Research Journal
- Vol. 79 (6) , 534-547
Improving the Wettability of Deep-Groove Polypropylene Fibers by Photografting
This paper presented photografting as a surface modification method to provide permanent wettability improvement to deep-groove polypropylene (PP) fibers. We also evaluated their wettability by testing the dynamic contact angle (DCA) on single fibers and characterized the wicking performance of fiber bundles when polyacrylamide (PAAm) and polyacrylic acid (PAA) were grafted onto the fibers. In this study, the increase in monomer concentration was found more effective than longer UV exposure time in creating higher graft density on deep-groove PP fibers. Acrylic acid (AA) monomers penetrated into the fiber and polymerized inside, but acrylamide (AAm) did not. Fiber dimension changed slightly upon grafting of PAAm, and enlarged significantly after grafting with PAA. DCA results show that the advancing water contact angle on single fibers decreased from 100 to 55° by grafting of PAAm and PAA, and spontaneous wicking of water was observed after surface modification. The wicking amount of the vertically placed fiber bundles showed a linear relationship to the square root of time at early wicking times.
- 21 April 2008
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 88A (4) , 1079-1086
Toughness decrease of PLA‐PHBHHx blend films upon surface‐confined photopolymerization
The present research investigates the effect of photoinduced grafting reaction on the bulk properties of melt processed poly(L‐lactic acid) (PLA)‐poly[(3‐hydroxybutyrate)‐co‐(3‐hydroxyhexanoate)] (PHBHHx) blend films. PLA‐PHBHHx blend films, comprising 10 wt % PHBHHx showed a remarkable toughness improvement. From dynamic mechanical analysis of melt processed PLA‐PHBHHx blend films, the blend appears to be noncompatible. Unfortunately, PLA‐PHBHHx blend films underwent rapid physical aging as characterized using differential scanning calorimetry, resulting in a significant toughness loss. Physically aged films regained the original toughness on annealing at 60°C for 30 min. Annealed PLA‐PHBHHx blend films also underwent physical aging leading to a significant toughness loss. Hydrophilic monomers like acrylic acid and acrylamide were successfully photopolymerized from the film surface using a sequential, two‐step photografting approach. The resultant films were characterized using water contact angle goniometry, ATR‐FTIR spectroscopy, and mechanical testing. PLA‐PHBHHx blend films lost their toughness significantly on surface modification and this was assigned to UV‐assisted solvent induced crystallization as characterized using wide‐angle X‐ray diffraction analyses. © 2008 Wiley Periodicals, Inc. J Biomed Mater Res, 2009
- 21 April 2008
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 88A (4) , 1079-1086
Toughness decrease of PLA‐PHBHHx blend films upon surface‐confined photopolymerization
The present research investigates the effect of photoinduced grafting reaction on the bulk properties of melt processed poly(L‐lactic acid) (PLA)‐poly[(3‐hydroxybutyrate)‐co‐(3‐hydroxyhexanoate)] (PHBHHx) blend films. PLA‐PHBHHx blend films, comprising 10 wt % PHBHHx showed a remarkable toughness improvement. From dynamic mechanical analysis of melt processed PLA‐PHBHHx blend films, the blend appears to be noncompatible. Unfortunately, PLA‐PHBHHx blend films underwent rapid physical aging as characterized using differential scanning calorimetry, resulting in a significant toughness loss. Physically aged films regained the original toughness on annealing at 60°C for 30 min. Annealed PLA‐PHBHHx blend films also underwent physical aging leading to a significant toughness loss. Hydrophilic monomers like acrylic acid and acrylamide were successfully photopolymerized from the film surface using a sequential, two‐step photografting approach. The resultant films were characterized using water contact angle goniometry, ATR‐FTIR spectroscopy, and mechanical testing. PLA‐PHBHHx blend films lost their toughness significantly on surface modification and this was assigned to UV‐assisted solvent induced crystallization as characterized using wide‐angle X‐ray diffraction analyses. © 2008 Wiley Periodicals, Inc. J Biomed Mater Res, 2009
- 20 December 2007
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 85B (2) , 564-572
Effect of the photoreaction solvent on surface and bulk properties of poly(lactic acid) and poly(hydroxyalkanoate) films
The major objective of this research was to modify the surface properties of poly(lactic acid) (PLA) and poly(hydroxyalkanoate) (PHA) films by using a sequential two‐step photografting approach. In step 1, benzophenone was photografted on the film surface and in step 2, hydrophilic monomers acrylamide and acrylic acid were photopolymerized from the film surfaces. Another objective was to study the effect of the reaction solvent in step 2 on surface and bulk properties of these films. ATR‐FTIR spectroscopy and water contact angle goniometry were used to characterize the resultant film surfaces. When ethanol was used as the solvent in step 2, there was significant penetration of the monomers into the films, and bulk properties such as toughness and percent elongation at break were drastically affected. The penetration of these monomers into the bulk was characterized using transmission FTIR microspectroscopy. Microtomed sections of the surface‐modified films were placed in a diamond compression cell to perform the FTIR microspectroscopic analyses. The observed monomer penetration into the films was successfully reduced by using water instead of ethanol in step 2, and resultant films showed higher toughness and percent elongation at break than films surface‐modified using ethanol as a solvent in step 2. © 2007 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 2008
- 20 December 2007
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 85B (2) , 564-572
Effect of the photoreaction solvent on surface and bulk properties of poly(lactic acid) and poly(hydroxyalkanoate) films
The major objective of this research was to modify the surface properties of poly(lactic acid) (PLA) and poly(hydroxyalkanoate) (PHA) films by using a sequential two‐step photografting approach. In step 1, benzophenone was photografted on the film surface and in step 2, hydrophilic monomers acrylamide and acrylic acid were photopolymerized from the film surfaces. Another objective was to study the effect of the reaction solvent in step 2 on surface and bulk properties of these films. ATR‐FTIR spectroscopy and water contact angle goniometry were used to characterize the resultant film surfaces. When ethanol was used as the solvent in step 2, there was significant penetration of the monomers into the films, and bulk properties such as toughness and percent elongation at break were drastically affected. The penetration of these monomers into the bulk was characterized using transmission FTIR microspectroscopy. Microtomed sections of the surface‐modified films were placed in a diamond compression cell to perform the FTIR microspectroscopic analyses. The observed monomer penetration into the films was successfully reduced by using water instead of ethanol in step 2, and resultant films showed higher toughness and percent elongation at break than films surface‐modified using ethanol as a solvent in step 2. © 2007 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 2008
- 6 July 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 106 (2) , 1042-1047
Degradation of poly(L‐lactide) films under ultraviolet‐induced photografting and sterilization conditions
The degradation of polymers under ultraviolet (UV) irradiation has been a great concern for biomaterial and agricultural applications. The major objective of this research was to study the effect of UV irradiation on the representative bulk and surface properties of poly (L‐lactide) (PLA) films. Two UV sources with different spectral outputs and intensities were chosen so that one of them could be used for surface modification and the other could be used for UV sterilization of the PLA films. The results established that the molecular weight of PLA decreased significantly during irradiation from the photografting lamp under atmospheric conditions. Irradiation through a Pyrex container was shown to minimize polymer degradation during UV exposure from the photografting lamp. The PLA films UV‐irradiated under the sterilization lamp for 12 h revealed a similar reduction in the molecular weight and no change in the surface hydrophilicity. However, significantly less photodegradation was observed under the sterilization lamp when the samples were held in a Pyrex container. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2007
- 6 July 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 106 (2) , 1042-1047
Degradation of poly(L‐lactide) films under ultraviolet‐induced photografting and sterilization conditions
The degradation of polymers under ultraviolet (UV) irradiation has been a great concern for biomaterial and agricultural applications. The major objective of this research was to study the effect of UV irradiation on the representative bulk and surface properties of poly (L‐lactide) (PLA) films. Two UV sources with different spectral outputs and intensities were chosen so that one of them could be used for surface modification and the other could be used for UV sterilization of the PLA films. The results established that the molecular weight of PLA decreased significantly during irradiation from the photografting lamp under atmospheric conditions. Irradiation through a Pyrex container was shown to minimize polymer degradation during UV exposure from the photografting lamp. The PLA films UV‐irradiated under the sterilization lamp for 12 h revealed a similar reduction in the molecular weight and no change in the surface hydrophilicity. However, significantly less photodegradation was observed under the sterilization lamp when the samples were held in a Pyrex container. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2007
- 26 April 2007
- Published by Wiley in Journal of Vinyl and Additive Technology
- Vol. 13 (2) , 57-64
Hydrophilization of polypropylene films by using migratory additives
Linear and branched hydrophilic additives of various molecular weights (MWs) were extruded with polypropylene (PP) to make blend films. The surface‐modifying additives included polyethylene glycol (PEG), hydroxyl‐terminated four‐arm polyethylene oxide (PEO), and a commercial hydrophilic additive, Irgasurf HL560. Films were extruded by using a twin‐screw microcompounder at 200°C, and the resulting film thickness was 100 μm. Attenuated total reflectance (ATR)‐FTIR spectrometry and water contact angle measurements were performed on the film surfaces over time to investigate the additive migration behavior. Although ATR‐FTIR detected concentration increases for all additives in the subsurface region, there was no significant improvement in surface hydrophilicity for the PEGs and four‐arm PEOs in the same period of time as water contact angles were measured on the surfaces. Among the linear additives, low MW PEG (1 kDa) was found to migrate faster than the high MW varieties. The linear PEG and four‐arm PEO with MW higher than 2 kDa did not exhibit significant migration to the surface within a month. Irgasurf was found to change the surface wettability effectively in a relatively short time. J. VINYL ADDIT. TECHNOL., 13:57–64, 2007. © 2007 Society of Plastics Engineers.
- 26 April 2007
- Published by Wiley in Journal of Vinyl and Additive Technology
- Vol. 13 (2) , 57-64
Hydrophilization of polypropylene films by using migratory additives
Linear and branched hydrophilic additives of various molecular weights (MWs) were extruded with polypropylene (PP) to make blend films. The surface‐modifying additives included polyethylene glycol (PEG), hydroxyl‐terminated four‐arm polyethylene oxide (PEO), and a commercial hydrophilic additive, Irgasurf HL560. Films were extruded by using a twin‐screw microcompounder at 200°C, and the resulting film thickness was 100 μm. Attenuated total reflectance (ATR)‐FTIR spectrometry and water contact angle measurements were performed on the film surfaces over time to investigate the additive migration behavior. Although ATR‐FTIR detected concentration increases for all additives in the subsurface region, there was no significant improvement in surface hydrophilicity for the PEGs and four‐arm PEOs in the same period of time as water contact angles were measured on the surfaces. Among the linear additives, low MW PEG (1 kDa) was found to migrate faster than the high MW varieties. The linear PEG and four‐arm PEO with MW higher than 2 kDa did not exhibit significant migration to the surface within a month. Irgasurf was found to change the surface wettability effectively in a relatively short time. J. VINYL ADDIT. TECHNOL., 13:57–64, 2007. © 2007 Society of Plastics Engineers.