Xiao Peng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Xiao Peng has a total of 78 co-authors. Here are the top co-authors by number of shared publications:
F. Wang
Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 110016, China
18 shared publicationsC. Xu
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
5 shared publications- Liangfu Zheng
Center for Applied Energy Research, University of Kentucky, 2540 Research Park Drive, Lexington, Kentucky 40511, United States
5 shared publications J. Yan
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, (P.R. China)
4 shared publicationsJ. Zhao
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, 62 Wencui Road, Shenyang, 110016 Liaoning, China
3 shared publicationsXiaolan Wang
3 shared publications
Latest Publications
- Open Access
Integrated Laser Additive Manufacturing of α-Al2O3 Nanoparticle-Seeded β/γ’ Ni-Al Intermetallic Alloy with Enhanced High-Temperature Oxidation Performance
The oxidation of β-NiAl at high temperatures leads to the preferential formation of metastable alumina, such as θ-Al2O3, which exhibits a significantly faster growth rate compared to stable α-Al2O3. However, our recent research has shown that through the use of the surface-dispersing nanoparticles (NPs) of metal oxides with a hexagonal closed pack (hcp), such as α-Al2O3, the thermal growth of α-Al2O3 can be facilitated. The present study employed laser additive manufacturing (LAM) to develop an integrated α-Al2O3 NPs surface-seeded two-phase intermetallic alloy comprising brittle β-NiAl and tougher γ’-Ni3Al, which demonstrated better comprehensive mechanical properties. It was found that seeding the α-Al2O3 NPs promoted the early stage growth of α-Al2O3 on both β and γ’ phases during oxidation in air at 1000 °C. This led to a decrease in the oxidation rate but an enhancement in adhesion of the formed alumina scale in comparison to the naked β/γ’ two-phase alloy. The reasons for this result were interpreted.
Open AccessIntegrated Laser Additive Manufacturing of α-Al2O3 Nanoparticle-Seeded β/γ’ Ni-Al Intermetallic Alloy with Enhanced High-Temperature Oxidation Performance
The oxidation of β-NiAl at high temperatures leads to the preferential formation of metastable alumina, such as θ-Al2O3, which exhibits a significantly faster growth rate compared to stable α-Al2O3. However, our recent research has shown that through the use of the surface-dispersing nanoparticles (NPs) of metal oxides with a hexagonal closed pack (hcp), such as α-Al2O3, the thermal growth of α-Al2O3 can be facilitated. The present study employed laser additive manufacturing (LAM) to develop an integrated α-Al2O3 NPs surface-seeded two-phase intermetallic alloy comprising brittle β-NiAl and tougher γ’-Ni3Al, which demonstrated better comprehensive mechanical properties. It was found that seeding the α-Al2O3 NPs promoted the early stage growth of α-Al2O3 on both β and γ’ phases during oxidation in air at 1000 °C. This led to a decrease in the oxidation rate but an enhancement in adhesion of the formed alumina scale in comparison to the naked β/γ’ two-phase alloy. The reasons for this result were interpreted.
- 28 September 2023
- Published by Springer Nature in High Temperature Corrosion of Materials
- Vol. 100 (5-6) , 475-489
Development and High-Temperature Corrosion Performance of MCrAl(Y) Coatings Prepared by Electrochemical Deposition: A Brief Review
- 28 September 2023
- Published by Springer Nature in High Temperature Corrosion of Materials
- Vol. 100 (5-6) , 475-489
Development and High-Temperature Corrosion Performance of MCrAl(Y) Coatings Prepared by Electrochemical Deposition: A Brief Review
- 12 September 2023
- Published by Springer Nature in High Temperature Corrosion of Materials
- Vol. 100 (5-6) , 413-450
Nanoparticles Application in Promoting the Growth of a More Protective Oxide Scale at High Temperatures
- 12 September 2023
- Published by Springer Nature in High Temperature Corrosion of Materials
- Vol. 100 (5-6) , 413-450
Nanoparticles Application in Promoting the Growth of a More Protective Oxide Scale at High Temperatures
- Open Access
Study on the Microstructure and High-Temperature Oxidation Performance of β-NiAl/γ′-Ni3Al Intermetallic Compounds Fabricated by Laser Metal Deposition
Four Ni-Al intermetallic compounds with the Al concentrations in range of 28 to 35 (in atomic percentage) have been fabricated by laser metal deposition (LMD) through mixing appropriate contents of pure Ni powder with pre-alloyed high-Al nickel aluminide powder. Ni-35Al and Ni-32Al are both composed of more than 45 vol.% β-NiAl matrix phase dispersing γ′-Ni3Al, while Ni-30Al and Ni-28Al consisted of worm-like, needle-like γ′-Ni3Al mainly and less than 37 vol.% β-NiAl. After 20 h oxidation in air at 1000 °C, the results of thermobalance, X-ray diffraction and scanning electron microcopy, indicated that Ni-35Al and Ni-32Al are more oxidation-resistant than the Ni-30Al and Ni-28Al. Because the first two can thermally grow an external Al2O3 scale but the second two form a duplex oxide scale consisting of outer NiAl2O4 layer and inner Al2O3 layer.
Open AccessStudy on the Microstructure and High-Temperature Oxidation Performance of β-NiAl/γ′-Ni3Al Intermetallic Compounds Fabricated by Laser Metal Deposition
Four Ni-Al intermetallic compounds with the Al concentrations in range of 28 to 35 (in atomic percentage) have been fabricated by laser metal deposition (LMD) through mixing appropriate contents of pure Ni powder with pre-alloyed high-Al nickel aluminide powder. Ni-35Al and Ni-32Al are both composed of more than 45 vol.% β-NiAl matrix phase dispersing γ′-Ni3Al, while Ni-30Al and Ni-28Al consisted of worm-like, needle-like γ′-Ni3Al mainly and less than 37 vol.% β-NiAl. After 20 h oxidation in air at 1000 °C, the results of thermobalance, X-ray diffraction and scanning electron microcopy, indicated that Ni-35Al and Ni-32Al are more oxidation-resistant than the Ni-30Al and Ni-28Al. Because the first two can thermally grow an external Al2O3 scale but the second two form a duplex oxide scale consisting of outer NiAl2O4 layer and inner Al2O3 layer.
- 9 June 2023
- Published by Springer Nature in Journal of Materials Science
- Vol. 58 (24) , 10148-10165
Laser additively manufacturing of Al0.5CoCrFeNiTi0.5 high-entropy alloys with increased resistances to corrosion 3.5% NaCl and oxidation at 1000 °C
- 9 June 2023
- Published by Springer Nature in Journal of Materials Science
- Vol. 58 (24) , 10148-10165
Laser additively manufacturing of Al0.5CoCrFeNiTi0.5 high-entropy alloys with increased resistances to corrosion 3.5% NaCl and oxidation at 1000 °C
- 1 October 2018
- Published by Elsevier in Corrosion Science
- Vol. 143, 76-83
Thermal growth of exclusive alumina scale on a TiAl based alloy: Shot peening effect
- 1 October 2018
- Published by Elsevier in Corrosion Science
- Vol. 143, 76-83
Thermal growth of exclusive alumina scale on a TiAl based alloy: Shot peening effect
- 25 May 2018
- Published by Springer Nature in Metals and Materials International
- Vol. 24 (6) , 1293-1302
Temperature-Dependent Thermal and Chemical Stabilities as well as Mechanical Properties of Electrodeposited Nanocrystalline Ni
- 25 May 2018
- Published by Springer Nature in Metals and Materials International
- Vol. 24 (6) , 1293-1302
Temperature-Dependent Thermal and Chemical Stabilities as well as Mechanical Properties of Electrodeposited Nanocrystalline Ni