T. A. Vompe
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
T. A. Vompe has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
I M Milyaev
A.A. Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Leninskii pr. 49, 119334, Moscow, Russia
3 shared publicationsI. M. Milyaev
A. A. Baikov Institute of Metallurgy and Materials Science of the Russian Academy of Sciences
2 shared publications- Milyaev Igor Matveevich
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Moscow, Russia
2 shared publications - V. S. Yusupov
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Moscow, Russia
2 shared publications A B Ankudinov
Baikov Institute of Metallurgy & Materials Science (IMET RAS), Moscow, Russia
1 shared publication- A. B. Ankudinov
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Moscow, Russia
1 shared publication
Latest Publications
- Open Access
- 1 May 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 848 (1)
Magnetic properties of the Fe-24%Cr-15%Co-3%Mo-1.5%Ti hard magnetic alloy in anisotropic and isotropic states
The magnetic properties of the Fe-24%Cr-15%Co-3%Mo-1.5%Ti (in wt. %) hard magnetic alloy in anisotropic and isotropic states after various heat treatments were studied. The alloy was prepared by the methods of powder metallurgy. The relative density was 98 %. The coefficient of thermal expansion of the alloy during heating and cooling was 17, 4*10 6 K−1 and 19, 0 *10− 6 K1 in the temperature range of 100 °C - 1300 °C. The kinetics of o-phase formation caused by an isothermal annealing at T = 750 ºC was investigated by means of the hardness measurements. The best magnetic properties of the alloy in anisotropic state were obtained after thermomagnetic treatment with cooling rate 200 ºC/h as Br = 1.22 T, Hc = 42.2 kAm-1 and (BH)max = 31.2 kJm- 3 and on the alloy in isotropic state with cooling rate 40 ºC/h.
- 1 May 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 848 (1)
Open AccessMagnetic properties of the Fe-24%Cr-15%Co-3%Mo-1.5%Ti hard magnetic alloy in anisotropic and isotropic states
The magnetic properties of the Fe-24%Cr-15%Co-3%Mo-1.5%Ti (in wt. %) hard magnetic alloy in anisotropic and isotropic states after various heat treatments were studied. The alloy was prepared by the methods of powder metallurgy. The relative density was 98 %. The coefficient of thermal expansion of the alloy during heating and cooling was 17, 4*10 6 K−1 and 19, 0 *10− 6 K1 in the temperature range of 100 °C - 1300 °C. The kinetics of o-phase formation caused by an isothermal annealing at T = 750 ºC was investigated by means of the hardness measurements. The best magnetic properties of the alloy in anisotropic state were obtained after thermomagnetic treatment with cooling rate 200 ºC/h as Br = 1.22 T, Hc = 42.2 kAm-1 and (BH)max = 31.2 kJm- 3 and on the alloy in isotropic state with cooling rate 40 ºC/h.
- Open Access
- 7 June 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 525 (1) , 012061
Effect of mixing duration and sintering temperature on the magnetic properties of hard magnetic powder alloy Fe-30Cr-8Co (wt.%)
Effect of mixing duration and sintering temperature on the magnetic properties of hard magnetic powder alloy Fe-30Cr-8Co (wt.%) was studied. The obtained magnetic hysteresis properties of the hard magnetic powder alloy are better than as for industrial Fe-Cr-Co alloy which cobalt content is twice bigger. The optimum sintering temperature was 1350-1400 °C. At a sintering temperature of 1400 °C for 2.5 hours the mixing duration does not affect on the magnetic hysteresis properties. This technological operation is not critical.
- 7 June 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 525 (1) , 012061
Open AccessEffect of mixing duration and sintering temperature on the magnetic properties of hard magnetic powder alloy Fe-30Cr-8Co (wt.%)
Effect of mixing duration and sintering temperature on the magnetic properties of hard magnetic powder alloy Fe-30Cr-8Co (wt.%) was studied. The obtained magnetic hysteresis properties of the hard magnetic powder alloy are better than as for industrial Fe-Cr-Co alloy which cobalt content is twice bigger. The optimum sintering temperature was 1350-1400 °C. At a sintering temperature of 1400 °C for 2.5 hours the mixing duration does not affect on the magnetic hysteresis properties. This technological operation is not critical.
- Open Access
- 7 June 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 525 (1) , 012011
Influence of heat treatment on the magnetic properties of Fe-28%Cr-7%Co-2%Mo-0.5%Si powder hard magnetic alloy
The hard magnetic alloy Fe-28%Cr-7%Co-2%Mo-0.5%Si (in wt. %) was prepared by the methods of powder metallurgy. The maximum magnetic properties on the alloy was received after the TMT temperature of 540 °C and was the following: residual induction Br up to 1.3 T, coercive force Hc up to 40 kAm−1 and maximum energy product (BH)max up to 31 kJm−3. The hardness of the alloy increases from 228 to 250 HV 30 in the temperature range of spinodal decomposition at 600 – 660 °C. The coefficient of thermal expansion of the alloy is 13,1*10−6 K−1. It was found that the additional annealing of the alloy till 460 °C can increase the coercive force approximately for 6 kAm−1.
- 7 June 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 525 (1) , 012011
Open AccessInfluence of heat treatment on the magnetic properties of Fe-28%Cr-7%Co-2%Mo-0.5%Si powder hard magnetic alloy
The hard magnetic alloy Fe-28%Cr-7%Co-2%Mo-0.5%Si (in wt. %) was prepared by the methods of powder metallurgy. The maximum magnetic properties on the alloy was received after the TMT temperature of 540 °C and was the following: residual induction Br up to 1.3 T, coercive force Hc up to 40 kAm−1 and maximum energy product (BH)max up to 31 kJm−3. The hardness of the alloy increases from 228 to 250 HV 30 in the temperature range of spinodal decomposition at 600 – 660 °C. The coefficient of thermal expansion of the alloy is 13,1*10−6 K−1. It was found that the additional annealing of the alloy till 460 °C can increase the coercive force approximately for 6 kAm−1.
- 24 January 2017
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 58 (9-10) , 614-618
Magnetic Properties of Hard Magnetic Alloy Fe – 28% Cr – 13.4% Co – 2% Mo – 0.5% Si
- 24 January 2017
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 58 (9-10) , 614-618
Magnetic Properties of Hard Magnetic Alloy Fe – 28% Cr – 13.4% Co – 2% Mo – 0.5% Si
- 1 January 2015
- Published by Institute for Metals Superplasticity Problems of RAS in Letters on Materials
- Vol. 5 (4) , 424-427
Investigation of Magnetic Properties of Fe-25%Cr-10%Co-2%Mo-0,5%Si Powder Magnetic Alloy
- 1 January 2015
- Published by Institute for Metals Superplasticity Problems of RAS in Letters on Materials
- Vol. 5 (4) , 424-427
Investigation of Magnetic Properties of Fe-25%Cr-10%Co-2%Mo-0,5%Si Powder Magnetic Alloy
- 1 September 2014
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 5 (5) , 530-535
The effect of surfactant admixture during milling on pressing, sintering, and magnetic properties of FeCrCoMoW alloy
The effect of surfactant admixture (stearic and oleic acids) with a variety of milling (dry milling, milling in water and ethanol) on pressing and sintering and magnetic properties of the Fe-30Cr-20Co-2Mo-2W (wt %) hard magnetic powder alloy was studied. The addition of stearic and oleic acids in the amount of up to 2 wt % during dry or wet milling increases the density of pressed samples. The use of surfactants during milling in water and ethanol increases the density of sintered samples. X-ray diffraction shows that only accumulation of defects takes place in the crystal structure of the particles, and no additional phases form during dry or wet milling of powder mixtures containing a surfactant. The best magnetic hysteresis properties were obtained with samples milled in ethanol with 1% stearic acid.
- 1 September 2014
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 5 (5) , 530-535
The effect of surfactant admixture during milling on pressing, sintering, and magnetic properties of FeCrCoMoW alloy
The effect of surfactant admixture (stearic and oleic acids) with a variety of milling (dry milling, milling in water and ethanol) on pressing and sintering and magnetic properties of the Fe-30Cr-20Co-2Mo-2W (wt %) hard magnetic powder alloy was studied. The addition of stearic and oleic acids in the amount of up to 2 wt % during dry or wet milling increases the density of pressed samples. The use of surfactants during milling in water and ethanol increases the density of sintered samples. X-ray diffraction shows that only accumulation of defects takes place in the crystal structure of the particles, and no additional phases form during dry or wet milling of powder mixtures containing a surfactant. The best magnetic hysteresis properties were obtained with samples milled in ethanol with 1% stearic acid.
- 1 January 2012
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2012 (1) , 55-57
Kinetics of σ-phase formation in a strain aging hard magnetic Fe-33% Cr-12% Co-2% Cu alloy
The formation of σ-phase in aging hard magnet alloy Fe-33% Cr-12% Co-2% Cu, which was obtained by quenching from 1150°C into water and annealing in the temperature range 650–800°C, has been investigated. It was found that the maximum rate of the σ-phase formation was at 750°C.
- 1 January 2012
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2012 (1) , 55-57
Kinetics of σ-phase formation in a strain aging hard magnetic Fe-33% Cr-12% Co-2% Cu alloy
The formation of σ-phase in aging hard magnet alloy Fe-33% Cr-12% Co-2% Cu, which was obtained by quenching from 1150°C into water and annealing in the temperature range 650–800°C, has been investigated. It was found that the maximum rate of the σ-phase formation was at 750°C.